Patent classifications
C04B2237/343
Zirconia layered body
There is provided at least any of a layered body which has a change in color tone and in which it is unnecessary to select a colorant and the content of the colorant in consideration of a difference in the sintering behavior between layers, a precursor thereof, or a method for producing these. Provided is a layered body which has a structure, in which two or more layers containing stabilizer-containing zirconia and a colorant are layered, and in which types and contents of the colorants contained in the layers are equal to each other, the layered body including at least: a first layer containing a colorant and zirconia which has a stabilizer content of higher than or equal to 3.3 mol %; and a second layer containing a colorant and zirconia which has a stabilizer content different from that of the zirconia contained in the first layer.
METHOD FOR PRODUCING A METAL-CERAMIC SUBSTRATE AND FURNACE
The invention relates to a method for producing a metal-ceramic substrate and to a furnace suitable for carrying out the method. With the method, a metal-ceramic substrate with increased thermal and current conductivity can be obtained. The method comprises the steps of providing a stack containing a ceramic body, a metal foil, and a solder material in contact with the ceramic body and the metal foil, the solder material comprising a metal having a melting point of at least 700° C., a metal having a melting point of less than 700° C., and an active metal, and heating the stack, the stack passing through a heating zone for heating.
METHOD FOR PRODUCING A METAL-CERAMIC SUBSTRATE
The present invention relates to a method for producing a metal-ceramic substrate. The method has the following steps: providing a stack containing a ceramic body, a metal foil, and a solder material in contact with the ceramic body and the metal foil, wherein the solder material has: a metal having a melting point of at least 700° C., a metal having a melting point of less than 700° C., and an active metal; and heating the stack, wherein at least one of the following conditions is satisfied: the high temperature heating duration is no more than 60 min; the peak temperature heating duration is no more than 30 min; the heating duration is no more than 60 min.
HONEYCOMB STRUCTURE, EXHAUST GAS PURIFICATION CATALYST, AND EXHAUST GAS PURIFICATION SYSTEM
A pillar shaped honeycomb structure for induction heating, the honeycomb structure being made of ceramics and including: an outer peripheral wall; and a partition wall disposed on an inner side of the outer peripheral wall, the partition wall defining a plurality of cells, each of the cells penetrating from one end face to other end face to form a flow path, wherein a composite material containing a conductor and a non-conductor is provided in the cells in a region of 50% or less of the total length of the honeycomb structure from one end face, and wherein the conductor is a conductor that generates heat in response to a change in a magnetic field.
Method for manufacturing sensor element
A method for manufacturing a sensor element that includes: a pair of electrodes; a ceramic layer having a hollow space that is to be an air introduction hole; and a first layer and a second layer stacked at both surfaces of the ceramic layer, One of the electrodes is in communication with the hollow space, The method includes: preparing an unsintered ceramic sheet, and a burn-out material sheet having a thickness different from that of the unsintered ceramic sheet, the burn-out material sheet having, in a plane orthogonal to the direction of an axial line O, a cross-sectional area substantially identical to a cross-sectional area of the pre-sintering hollow space; placing the burn-out material sheet in the pre-sintering hollow space; pressing the sheets so as to have an identical thickness; and burning out the burn-out material sheet.
COPPER/CERAMIC JOINED BODY AND INSULATING CIRCUIT SUBSTRATE
A copper/ceramic bonded body is provided, including: a copper member made of copper or a copper alloy; and a ceramic member, the copper member and the ceramic member being bonded to each other, in which a total concentration of Al, Si, Zn, and Mn is 3 atom % or less when concentration measurement is performed by an energy dispersive X-ray analysis method at a position 1000 nm away from a bonded interface between the copper member and the ceramic member to a copper member side, assuming that a total value of Cu, Mg, Ti, Zr, Nb, Hf, Al, Si, Zn, and Mn is 100 atom %.
MEMBER FOR POWER STORAGE DEVICE, ALL-SOLID-STATE BATTERY, AND METHOD FOR MANUFACTURING MEMBER FOR POWER STORAGE DEVICE
Provided is a member for a power storage device that, even when the amount of electrode active material supported is increased, enables charge and discharge and thus achieves a high capacity. A member 6 for a power storage device includes: a solid electrolyte layer 1; and an electrode layer 2 provided on the solid electrolyte layer 1 and made of a sintered body of an electrode material layer 2A containing an electrode active material precursor powder having an average particle diameter of not less than 0.01 μm and less than 0.7 μm.
SEMICONDUCTOR DEVICE
A semiconductor device includes: an insulated circuit substrate including first and second conductive layers on a top surface side; a first semiconductor chip mounted on the first conductive layer; a second semiconductor chip mounted on the second conductive layer; a printed circuit board including a first lower-side wiring layer arranged to be opposed to the first semiconductor chip, and a second lower-side wiring layer arranged to be opposed to the second semiconductor chip, the printed circuit board being provided with a curved part curved toward the insulated circuit substrate; a first connection member arranged to connect the first semiconductor chip with the first lower-side wiring layer; a second connection member arranged to connect the second semiconductor chip with the second lower-side wiring layer; and a third connection member arranged to connect the first conductive layer with the second lower-side wiring layer at the curved part.
CERAMIC JOINED BODY, ELECTROSTATIC CHUCK DEVICE, AND METHOD FOR PRODUCING CERAMIC JOINED BODY
A ceramic joined body (1) includes: a pair of ceramic plates (2,3) that include a conductive material; and a conductive layer (4) and an insulating layer (5) that are interposed between the pair of ceramic plates (2, 3), a porosity at an interface between the pair of ceramic plates (2, 3) and the insulating layer (5) is 4% or less, and a ratio of an average primary particle diameter of an insulating material which forms the insulating layer (5) to an average primary particle diameter of an insulating material which forms the ceramic plates (2, 3) is more than 1.
YAG CERAMIC JOINED BODY AND PRODUCTION METHOD THEREFOR
A YAG ceramic bonded body in which a YAG ceramic and a YAG ceramic or optical glass are bonded, wherein the YAG ceramic bonded body comprises glass as a bonding layer, and has a rate of change of transmittance that is within 7%. An object of this invention is to provide a bonded body in which a YAG ceramic and a YAG ceramic are bonded, or a bonded body in which a YAG ceramic and optical glass are bonded, and which is capable of suppressing the reflection of light at the bonded interface, as well as the production method thereof.