C07C4/18
Catalyst for Producing C8 Aromatic Hydrocarbon Having Reduced Ethylbenzene Content and Preparation Method Therefor
Disclosed are a catalyst and a preparation method therefor, the catalyst being able to maintain a high production yield of C8 aromatic hydrocarbons in the process of converting a feedstock containing alkyl aromatics to C8 aromatic hydrocarbons such as mixed xylene through disproportionation/transalkylation/dealkylation while reducing a content of ethylbenzene in the products.
Catalyst for Producing C8 Aromatic Hydrocarbon Having Reduced Ethylbenzene Content and Preparation Method Therefor
Disclosed are a catalyst and a preparation method therefor, the catalyst being able to maintain a high production yield of C8 aromatic hydrocarbons in the process of converting a feedstock containing alkyl aromatics to C8 aromatic hydrocarbons such as mixed xylene through disproportionation/transalkylation/dealkylation while reducing a content of ethylbenzene in the products.
PROCESS FOR INTERCONVERSION OF OLEFINS WITH MODIFIED BETA ZEOLITE
Methods for interconverting olefins in an olefin-rich hydrocarbon stream include contacting the olefin-rich hydrocarbon stream with a catalyst system in an olefin interconversion unit to produce an interconverted effluent comprising ethylene and propylene. The contacting may be conducted at a reaction temperature from 450° C. to 750° C., a reaction pressure from 1 bar to 5 bar, and a residence time from 0.5 seconds to 1000 seconds. The catalyst system includes a framework-substituted beta zeolite. The framework-substituted beta zeolite has a *BEA aluminosilicate framework that has been modified by substituting a portion of framework aluminum atoms of the *BEA aluminosilicate framework with beta-zeolite Al-substitution atoms independently selected from the group consisting of titanium atoms, zirconium atoms, hafnium atoms, and combinations thereof.
PROCESS FOR INTERCONVERSION OF OLEFINS WITH MODIFIED BETA ZEOLITE
Methods for interconverting olefins in an olefin-rich hydrocarbon stream include contacting the olefin-rich hydrocarbon stream with a catalyst system in an olefin interconversion unit to produce an interconverted effluent comprising ethylene and propylene. The contacting may be conducted at a reaction temperature from 450° C. to 750° C., a reaction pressure from 1 bar to 5 bar, and a residence time from 0.5 seconds to 1000 seconds. The catalyst system includes a framework-substituted beta zeolite. The framework-substituted beta zeolite has a *BEA aluminosilicate framework that has been modified by substituting a portion of framework aluminum atoms of the *BEA aluminosilicate framework with beta-zeolite Al-substitution atoms independently selected from the group consisting of titanium atoms, zirconium atoms, hafnium atoms, and combinations thereof.
METHODS OF HEAVY REFORMATE CONVERSION INTO AROMATIC COMPOUNDS
Method of making BTX compounds including benzene, toluene, and xylene, including feeding heavy reformate to a reactor containing a composite zeolite catalyst. The composite zeolite catalyst includes a mixture of layered mordenite (MOR-L) comprising a layered or rod-type morphology with a layer thickness less than 30 nm and ZSM-5. The MOR-L, the ZSM-5, or both include one or more impregnated metals. The method further includes producing the BTX compounds by simultaneously performing transalkylation and dealkylation of the heavy reformate in the reactor. The composite zeolite catalyst is able to simultaneously catalyze both the transalkylation and dealkylation reactions.
METHODS OF HEAVY REFORMATE CONVERSION INTO AROMATIC COMPOUNDS
Method of making BTX compounds including benzene, toluene, and xylene, including feeding heavy reformate to a reactor containing a composite zeolite catalyst. The composite zeolite catalyst includes a mixture of layered mordenite (MOR-L) comprising a layered or rod-type morphology with a layer thickness less than 30 nm and ZSM-5. The MOR-L, the ZSM-5, or both include one or more impregnated metals. The method further includes producing the BTX compounds by simultaneously performing transalkylation and dealkylation of the heavy reformate in the reactor. The composite zeolite catalyst is able to simultaneously catalyze both the transalkylation and dealkylation reactions.
METHODS OF HEAVY REFORMATE CONVERSION INTO AROMATIC COMPOUNDS
Method of making BTX compounds including benzene, toluene, and xylene, including feeding heavy reformate to a reactor containing a composite zeolite catalyst. The composite zeolite catalyst includes a mixture of layered mordenite (MOR-L) comprising a layered or rod-type morphology with a layer thickness less than 30 nm and ZSM-5. The MOR-L, the ZSM-5, or both include one or more impregnated metals. The method further includes producing the BTX compounds by simultaneously performing transalkylation and dealkylation of the heavy reformate in the reactor. The composite zeolite catalyst is able to simultaneously catalyze both the transalkylation and dealkylation reactions.
PROCESS FOR CATALYTIC UPCYCLING OF HYDROCARBON POLYMERS TO ALKYLAROMATIC COMPOUNDS
Process for upcycling a waste material to form alkylaromatic compounds is described herein. The process typically includes the steps of feeding a waste material containing hydrocarbon polymer(s) into a reactor containing a catalyst therein, and operating the reactor at a sufficient temperature for a sufficient period of time to convert the hydrocarbon polymer(s) to a liquid and/or wax product containing alkylaromatic compound(s). Each of the alkylaromatic compound(s) contains at least 10 carbon atoms. The catalyst contains a transition metal or a mixture of a transition metal and another metal. Optionally, the catalyst is dispersed on the surface of a support. The product may contain other unsaturated compounds, such as olefins. Typically, the reactor operates at a temperature in the range between 250° C. and 350° C. The total selectivity of the process to form the one or more alkylaromatic compounds is typically between 50 mol % and 95 mol %.
PROCESS FOR CATALYTIC UPCYCLING OF HYDROCARBON POLYMERS TO ALKYLAROMATIC COMPOUNDS
Process for upcycling a waste material to form alkylaromatic compounds is described herein. The process typically includes the steps of feeding a waste material containing hydrocarbon polymer(s) into a reactor containing a catalyst therein, and operating the reactor at a sufficient temperature for a sufficient period of time to convert the hydrocarbon polymer(s) to a liquid and/or wax product containing alkylaromatic compound(s). Each of the alkylaromatic compound(s) contains at least 10 carbon atoms. The catalyst contains a transition metal or a mixture of a transition metal and another metal. Optionally, the catalyst is dispersed on the surface of a support. The product may contain other unsaturated compounds, such as olefins. Typically, the reactor operates at a temperature in the range between 250° C. and 350° C. The total selectivity of the process to form the one or more alkylaromatic compounds is typically between 50 mol % and 95 mol %.
Catalyst for Converting Alkylaromatic Hydrocarbon and Preparation Method Thereof
Disclosed are a bifunctional catalyst and a preparation method therefor, the bifunctional catalyst being suitable to produce high-value aromatic hydrocarbons by subjecting alkylaromatic hydrocarbons to a disproportionation/transalkylation/dealkylation reaction while suppressing aromatic loss or subjecting C8 aromatic hydrocarbons to an isomerization reaction while suppressing xylene loss.