Patent classifications
C08K2003/2265
POLYCRYSTALLINE 18H HEXAFERRITE, METHOD OF MANUFACTURE, AND USES THEREOF
A polycrystalline ferrite composition comprises a formula of M.sub.5Me.sub.2Ti.sub.3Fe.sub.12O.sub.31, wherein M is Ba.sup.2+, Se.sup.+, or a combination thereof; and Me is Mg.sup.2+, Zn.sup.2+, Cu.sup.2+, Co.sup.2+, or a combination thereof; and has an average grain size of 1 micrometer to 100 micrometers. A composite comprises a polymer matrix; and the polycrystalline ferrite composition. Methods of making the polycrystalline ferrite composition and the composite are also disclosed.
Y-TYPE HEXAFERRITE, METHOD OF MANUFACTURE, AND USES THEREOF
In an aspect, a Co.sub.2Y-type ferrite includes oxides of at least Ba, La, Co, Me, Fe, and optionally Ca; wherein Me is at least Ni and optionally one or more of Zn, Cu, Mn, or Mg. A composite can include the Co.sub.2Y-type ferrite and a polymer. An article can include the Co.sub.2Y-type ferrite.
Method of producing an elastic coating and an elastic coating
The present invention relates to a method of producing an elastic coating which is suitable for waterproofing, by using film forming onto a solid surface, textile or mesh. In this method, a dispersion which comprises i) one or more adhesives and/or coagulating aggregates, mainly in solid form, ii) one or more polymers, and iii) one or more surface-active agents, is brought into contact with a coagulator of the surface-active agent of the dispersion. The present invention also relates to a coating which is prepared by using the present method.
HIGH FIDELITY SHEET EXPLOSIVE SIMULANTS
An explosive sheet simulant that uses an ethylene vinyl acetate polymer combined with a mixture of a boron carbide and iron oxide for X-ray attenuating properties, and components of the mixture selected for predetermined flexural modulus combined with particle density, effective atomic number, X-ray transmission properties, or millimeter wave properties.
HYDROPHOBIC, LOW GLASS TRANSITION TEMPERATURE OLIGOMER WITH HIGH LEVEL OF CHAIN TRANSFER AGENT
Disclosed herein is an additive for a paint or stain composition or for a colorant composition. The additive is polymerized from at least one acrylate monomer and a chain transfer agent. The additive has a weight molecular weight from about 2,000 Daltons to about 5,000 Daltons, and the chain transfer agent comprises a hydrogen-sulfur functionality and is present from about 8 to about 20 parts per hundred parts of monomers. The additive's glass transition temperature ranges from about −50° C. to about −10° C. and the additive is hydrophobic. The additive is added to the colorant composition to minimize tip drying at the colorant canisters, and is added to paint or stain composition as an open time extender.
Z-TYPE HEXAFERRITE HAVING A NANOCRYSTALLINE STRUCTURE
In an aspect, a Co.sub.2Z ferrite has the formula: (Ba.sub.1−xSr.sub.x).sub.3Co.sub.2+yM.sub.yFe.sub.24−2y−zO.sub.41. M is at least one of Mo, Ir, or Ru. The variable x can be 0 to 0.8, or 0.1 to 0.8. The variable y can be 0 to 0.8, or 0.01 to 0.8. The variable z can be −2 to 2. The Co.sub.2Z ferrite can have an average grain size of 5 to 100 nanometers, or 30 to 80, or 10 to 40 nanometers as measured using at least one of transmission electron microscopy, field emission scanning electron microscopy, or x-ray diffraction.
Products by Upcycling Landfill Waste Streams
Fossil-fuel and rubber-derived waste stream conversion to composite lumber substitutes or barrier members; the composites having material properties and uses of greater value than the solid waste stream components separately or together. Preferred combinations including waste materials derived from waste carpet, waste tires, and waste bituminous roofing shingles, all enormous problems for landfill disposal. In a range of formulation ratios, when combined with a binder, new and marketable products are made from solid waste. Improved resistance to rot, to water, and to weathering is exhibited in synergy with improved compressive and flexural strength, enabling production of a wide variety of useful and environmentally-friendly structural products, for example. Product weight and strength can be engineered to suit and may be structural members for architectural, engineering or agricultural use. Advantageously, the new products themselves can be re-used—by an end-of-life process for making more new products, achieving the capacity to make and remake multigenerational products from solid wastes and to reduce loading of landfills. Production by profile extrusion and by RIM molding are described.
THERMOPLASTIC RESIN COMPOSITION WITH IMPROVED UV RESISTANCE
Thermoplastic resin composition comprising: (a1) at least one styrene-acrylonitrile copolymer component A1, (a2) at least one acrylonitrile styrene acrylate graft copolymer A2 as impact modifier, (a3) optionally at least one thermoplastic polymer A3 other than components A1 and A2, (b) at least one pigment B, (c) at least one hindered amine UV light stabilizer C, and (d) optionally further polymer additives D, other than components B and C, wherein the UV stabilizing component(s) present in the thermoplastic resin are only hindered amine UV light stabilizer(s) C.
THERMOPLASTIC RESIN COMPOSITION WITH IMPROVED UV RESISTANCE
Thermoplastic resin composition comprising: (a1) at least one styrene-acrylonitrile copolymer component A1, (a2) at least one acrylonitrile styrene acrylate graft copolymer A2 as impact modifier, (a3) optionally at least one thermoplastic polymer A3 other than components A1 and A2, (b) at least one pigment B, (c) at least one hindered amine UV light stabilizer C, and (d) optionally further polymer additives D, other than components B and C, wherein the UV stabilizing component(s) present in the thermoplastic resin are only hindered amine UV light stabilizer(s) C.
THERMOPLASTIC STYRENE COPOLYMER RESIN COMPOSITION WITH IMPROVED UV RESISTANCE
Thermoplastic styrene copolymer resin composition comprising: (a1) at least one styrene-acrylonitrile copolymer component A1, (a2) at least one acrylonitrile styrene acrylate graft copolymer A2 as impact modifier, (a3) optionally at least one thermoplastic polymer A3 other than components A1 and A2, (b) at least one transition metal oxide pigment B, (cl) at least one hindered amine UV light stabilizer C1, (c2) optionally at least one UV absorber C2 different from Cl, (d) optionally further polymer additives D, other than components B, C1, C2, and E, and (e) optionally one metal scavenger component E, wherein at least 99.0 wt.-% of the transition metal oxide pigment B consist of transition metal atoms and oxygen atoms.