C08L33/064
FOAMED ACRYLIC-RESIN OBJECT, PROCESS FOR PRODUCING SAME, AND FIBER-REINFORCED COMPOSITE
Provided is a foamed acrylic-resin object, in which a heat-resistant temperature in thermomechanical analysis is 170 C. or higher, and the number of bubbles respectively having a major diameter of 2 mm or greater is 2.0 or less per area of 10 cm10 cm.
PREPARATION OF RETORT PACKAGING INK THROUGH CROSS-LINKING OF POLYURETHANE RESINS
A method of preparing a retort packaging article includes: providing a sealable packaging; applying an ink to an outer surface of the sealable packaging; and overlaying a substantially transparent lamination layer over the ink and enveloping at least a portion of the sealable packaging. The ink contains a styrene-acrylic resin, which has anhydride functionality, and a polyurethane resin.
PREPARATION OF RETORT PACKAGING INK THROUGH CROSS-LINKING OF POLYURETHANE RESINS
A method of preparing a retort packaging article includes: providing a sealable packaging; applying an ink to an outer surface of the sealable packaging; and overlaying a substantially transparent lamination layer over the ink and enveloping at least a portion of the sealable packaging. The ink contains a styrene-acrylic resin, which has anhydride functionality, and a polyurethane resin.
SHALE SWELLING INHIBITORS
The present invention provides amidic polymers, which exhibit shale swelling inhibitor activity having improved bio-degradability. The amidic polymers of the invention may be employed in a wide variety of compositions, particularly in subterranean drilling operations. Non-limiting generic structures of the amidic polymers are set out below: (1) wherein R.sub.1-R.sub.3 and integers m and n are defined herein.
##STR00001##
FILM TOUCH SENSOR AND METHOD FOR FABRICATING THE SAME
A film touch sensor includes a separation layer; a protective layer disposed on the separation layer, and an electrode pattern layer which is disposed on the protective layer and includes an insulation layer that is a cured layer of a binder resin including (a-1) a resin in which at least a part of a phenolic hydroxyl group or a carboxyl group is protected with an acid decomposable group, (a-2) an acrylic resin containing an epoxy group, and (a-3) an acrylic resin containing an oxetane group, such that it is possible to suppress thermal damage such as wrinkles, or cracks of the insulation layer, which may occur in high-temperature deposition and annealing processes, and significantly reduce an occurrence rate of cracks during peeling-off the same from a carrier substrate.
FILM TOUCH SENSOR AND METHOD FOR FABRICATING THE SAME
A film touch sensor includes a separation layer; a protective layer disposed on the separation layer, and an electrode pattern layer which is disposed on the protective layer and includes an insulation layer that is a cured layer of a binder resin including (a-1) a resin in which at least a part of a phenolic hydroxyl group or a carboxyl group is protected with an acid decomposable group, (a-2) an acrylic resin containing an epoxy group, and (a-3) an acrylic resin containing an oxetane group, such that it is possible to suppress thermal damage such as wrinkles, or cracks of the insulation layer, which may occur in high-temperature deposition and annealing processes, and significantly reduce an occurrence rate of cracks during peeling-off the same from a carrier substrate.
PROTECTIVE WATER REVERSIBLE CLEAR COATING FOR SUBSTRATES
A protective, sacrificial, water-reversible, coating composition for the protection of substrates comprised of water, a volatile base, a film-forming acrylic polymer in a water dispersion form, a compatabilizing polymer, specifically poly (2-ethyl-2-oxazoline), a poly acidic polymer (pH specific in terms of its solubility), wherein said coating is both water applied and water reversible or re-soluble under specific pH conditions.
Slurry composition for lithium ion secondary battery and electrode for lithium ion secondary battery
Provided is a slurry composition for a lithium ion secondary battery that can cause an electrode for a lithium ion secondary battery to display excellent adhesiveness (peel strength) and flexibility (pliability) and that can cause a lithium ion secondary battery to display excellent rate characteristics and cycle characteristics. The slurry composition for a lithium ion secondary battery contains a silicon compound and a binder. The silicon compound includes either or both of Li.sub.2SiO.sub.3 and Li.sub.4SiO.sub.4. The binder includes a water-soluble polymer that includes either or both of an ethylenically unsaturated carboxylic acid monomer unit (A) and an alkali metal salt thereof, and that includes a cross-linkable monomer unit (B). A 1 mass % aqueous solution of the water-soluble polymer has a viscosity of 1,000 mPa.Math.s or less. The slurry composition for a lithium ion secondary battery has a pH of not lower than 9 and not higher than 12.
Shale swelling inhibitors
The present invention provides amidic polymers, which exhibit shale swelling inhibitor activity having improved biodegradability. The amidic polymers of the invention may be employed in a wide variety of compositions, particularly in subterranean drilling operations. Non-limiting generic structures of the amidic polymers are set out below: formula (1) wherein R.sub.1-R.sub.3 and integers m and n are defined herein. ##STR00001##
COPOLYMER, PROCESS FOR PRODUCING COPOLYMER, RESIN COMPOSITION, SHAPED ARTICLE AND VEHICLE
The present invention provides a copolymer demonstrating superior heat resistance, fluidity, mechanical properties, appearance, low water absorbency and moldability. In addition, the present invention provides a process for producing a copolymer that enables the resulting copolymer to demonstrate superior heat resistance, fluidity, mechanical properties, appearance, low water absorbency and moldability. The copolymer of the present invention is a copolymer containing 80 mol % or more of a methyl (meth)acrylate unit (A), wherein the Vicat softening temperature thereof is 115 C. or higher, the saturated water absorption rate thereof at 60 C. is 4% by weight or less, and the yellow index thereof is 1 or less. In addition, the process for producing a copolymer of the present invention comprises the obtaining of a precursor by suspension polymerizing a monomer mixture containing 80 mol % or more of methyl (meth)acrylate (a) and 0.7 mol % to 7 mol % of (meth)acrylic acid (b), followed by melting and kneading the resulting precursor with an extruder to obtain a copolymer containing 80 mol % or more of a methyl (meth)acrylate unit (A), 0.45 mol % to 7 mol % of a (meth)acrylic acid unit (B), and 0.001 mol % to 0.25 mol % of a glutaric anhydride unit (C).