C08L2555/72

Reducing crumb rubber modified bitumen odors
11274208 · 2022-03-15 · ·

A method for reducing odors including the steps of admixing active agents and a diluting agent to liquid crumb rubber modified bitumen, wherein the active agents comprise 20 to 60 wt.-% of an aldehyde selected from alpha-hexyl cinnamaldehyde, 2-(4-tert.-butylbenzyl) propionaldehyde, 2-benzylidenheptanal, or mixtures thereof, and 10 to 40 wt.-% of one or more alcohols having a boiling point of at least 150° C., calculated on the total weight of active agents. A crumb rubber modified bitumen composition as obtained by the method above. The use of a crumb rubber modified bitumen composition as obtained by the method above in road surfacing and road base materials, in insulating layers for buildings, in roofing materials and/or in sealing sheeting.

Culture medium protective liquid material and embryo culture method
11299707 · 2022-04-12 · ·

A culture medium protective liquid material of the present invention covers a culture medium when a living cell is cultured. The culture medium protective liquid material contains liquid paraffin which is liquid at room temperature as a main component thereof and an antioxidative substance for restraining the liquid paraffin from being oxidized.

NANOSTRUCTURED ALUMINOSILICATE WAX CARRIER FOR ASPHALT

A modified bitumen includes bitumen and a bitumen modifier. The bitumen modifier includes composite particles. The composite particles include aluminosilicate nanostructures defining nanopores and micropores and paraffin wax adhered to surfaces of the aluminosilicate nanostructures. Modifying bitumen includes combining bitumen and the bitumen modifier.

REDUCING CRUMB RUBBER MODIFIED BITUMEN ODORS
20210284844 · 2021-09-16 ·

A method for reducing odors including the steps of admixing active agents and a diluting agent to liquid crumb rubber modified bitumen, wherein the active agents comprise 20 to 60 wt.-% of an aldehyde selected from alpha-hexyl cinnamaldehyde, 2-(4-tert.-butylbenzyl) propionaldehyde, 2-benzylidenheptanal, or mixtures thereof, and 10 to 40 wt.-% of one or more alcohols having a boiling point of at least 150° C., calculated on the total weight of active agents. A crumb rubber modified bitumen composition as obtained by the method above. The use of a crumb rubber modified bitumen composition as obtained by the method above in road surfacing and road base materials, in insulating layers for buildings, in roofing materials and/or in sealing sheeting.

Polymer modified asphalt roofing material

A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity reducing agent, a wax, a salt of a fatty acid ester, and an amide of a fatty acid. The shingle coating asphalt coating composition is used to make a shingle. The shingle includes a substrate, the asphalt, and roofing granules.

Polymer modified asphalt roofing material

A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity reducing agent, a wax, a salt of a fatty acid ester, and an amide of a fatty acid. The shingle coating asphalt coating composition is used to make a shingle. The shingle includes a substrate, the asphalt, and roofing granules.

Polymer modified asphalt roofing material

A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity reducing agent, a wax, a salt of a fatty acid ester, and an amide of a fatty acid. The shingle coating asphalt coating composition is used to make a shingle. The shingle includes a substrate, the asphalt, and roofing granules.

POLYMER MODIFIED ASPHALT ROOFING MATERIAL

A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity reducing agent, a wax, a salt of a fatty acid ester, and an amide of a fatty acid. The shingle coating asphalt coating composition is used to make a shingle. The shingle includes a substrate, the asphalt, and roofing granules.

Polymer modified asphalt roofing material

A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity reducing agent, a wax, a salt of a fatty acid ester, and an amide of a fatty acid. The shingle coating asphalt coating composition is used to make a shingle. The shingle includes a substrate, the asphalt, and roofing granules.

Polymer modified asphalt roofing material

A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity reducing agent, a wax, a salt of a fatty acid ester, and an amide of a fatty acid. The shingle coating asphalt coating composition is used to make a shingle. The shingle includes a substrate, the asphalt, and roofing granules.