Patent classifications
C03B37/0122
ANTIRESONANT HOLLOW CORE FIBRE, PREFORM THEREFOR AND METHOD OF FABRICATION
A shaped tube (50,51) for use as a component in the fabrication of an antiresonant hollow core optical fibre, the shaped tube having a side wall with a transverse cross-sectional shape comprising a number of major curved portions (52) alternating with the same number of minor substantially straight portions (54), each curved portion (52) having an inwardly curving shape, and each straight portion (54) being equidistant from a central longitudinal axis of the shaped tube (50,51).
HOLLOW CORE OPTICAL FIBER AND A LASER SYSTEM
A hollow core photonic crystal fiber (PCF) including an outer cladding region and seven hollow tubes surrounded by the outer cladding region. Each of the hollow tubes is fused to the outer cladding to form a ring defining an inner cladding region and a hollow core region surrounded by the inner cladding region. The hollow tubes are not touching each other but are arranged with distance to adjacent hollow tubes. The hollow tubes each have an average outer diameter d2 and an average inner diameter d1, wherein d1/d2 is equal to or larger than about 0.8, such as equal to or larger than about 0.85, such as equal to or larger than about 0.9. Also, a laser system.
Method of manufacture of a capillary for a hollow-core photonic crystal fiber
A method for manufacturing a capillary usable as part of a hollow-core photonic crystal fiber. The method includes obtaining a capillary having capillary wall including a first wall thickness; and chemically etching the capillary wall to reduce the wall thickness of the capillary wall. During performance of the etching, a control parameter is locally varied along the length of the capillary, the control parameter relating to reactivity of an etchant used in the etching, so as to control the etched wall thickness of the capillary wall along the capillary length. Also disclosed is a capillary manufactured by such a method and various devices including such a capillary.
Hollow-core fibre and method of manufacturing thereof
A hollow-core anti-resonant-reflecting fibre (HC-AF) includes a hollow-core region, an inner cladding region, and an outer cladding region. The hollow-core region axially extends along the HC-AF. The inner cladding region includes a plurality of anti-resonant elements (AREs) and surrounds the hollow-core region. The outer cladding region surrounds the inner cladding region. The hollow-core region and the plurality of AREs are configured to provide phase matching of higher order hollow-core modes and ARE modes in a broadband wavelength range.
HOLLOW-CORE FIBRE AND METHOD OF MANUFACTURING THEREOF
A hollow-core anti-resonant-reflecting fibre (HC-AF) includes a hollow-core region, an inner cladding region, and an outer cladding region. The hollow-core region axially extends along the HC-AF. The inner cladding region includes a plurality of anti-resonant elements (AREs) and surrounds the hollow-core region. The outer cladding region surrounds the inner cladding region. The hollow-core region and the plurality of AREs are configured to provide phase matching of higher order hollow-core modes and ARE modes in a broadband wavelength range.
HOLLOW CORE OPTICAL FIBER AND A LASER SYSTEM
A hollow core photonic crystal fiber (PCF) including an outer cladding region and seven hollow tubes surrounded by the outer cladding region. Each of the hollow tubes is fused to the outer cladding to form a ring defining an inner cladding region and a hollow core region surrounded by the inner cladding region. The hollow tubes are not touching each other, but are arranged with distance to adjacent hollow tubes. The hollow tubes each have an average outer diameter d2 and an average inner diameter d1, wherein d1/d2 is equal to or larger than about 0.8, such as equal to or larger than about 0.85, such as equal to or larger than about 0.9. Also, a laser system.
OPTICAL FIBERS, METHODS OF THEIR FORMATION, AND METHODS OF THEIR USE
An example of an optical fiber includes an attenuating cladding disposed around a first waveguide (e.g., a core) and a waveguide (e.g., a waveguide cladding) disposed around the attenuating cladding. An attenuating cladding may be a doped layer that may be doped with, for example, a dopant comprising metal. A first waveguide and a second waveguide may each transmit light for a distinct sample characterization technique. An example of an optical fiber includes a core, a first intermediate cladding disposed around the core, an attenuating cladding disposed around the first intermediate cladding, an attenuating cladding disposed around the first intermediate cladding, a second intermediate cladding disposed around the attenuating cladding, a waveguide cladding disposed around the second intermediate cladding, and outer cladding disposed around the waveguide cladding, and an outer coating around the outer cladding. An optical fiber may be formed using a rod-in-tube process.
Hollow core optical fiber and method of making the same
The selection of starting materials used in the process of forming an MCR is controlled to specifically define the physical properties of the core tube and/or the capillary tubes in the local vicinity of the core tube. The physical properties are considered to include, but are not limited to, the diameter of a given tube/capillary, its wall thickness, and its geometry (e.g., circular, non-circular). A goal is to select starting materials with physical properties that yield a final hollow core optical fiber with a “uniform” core region (for the purposes of the present invention, a “uniform” core region is one where the struts of cladding periodic array surrounding the central core are uniform in length and thickness (with the nodes between the struts thus being uniformly spaced apart), which yields a core wall of essentially uniform thickness and circularity.
Antiresonant hollow core preforms and optical fibres and methods of fabrication
A preform (10) for an antiresonant hollow core optical fibre comprises an outer jacket tube (12) having an inner surface and a central longitudinal axis (24); a plurality of antiresonant cladding tubes (14) spaced apart at predefined peripheral locations around the inner surface of the outer jacket tube (12), each antiresonant cladding tube (14) in contact with the inner surface such that a central longitudinal axis (26) of each antiresonant cladding tube (14) is at a first radial distance from the central longitudinal axis (24) of the outer jacket tube (12); and a plurality of spacing elements (22) disposed alternately with the antiresonant cladding tubes (14) and each in contact with an outer surface of each of two adjacent antiresonant cladding tubes (14) at one or more contact points (28), the contact points (28) at a second radial distance from the central longitudinal axis (24) of the outer jacket tube (12), the second radial distance being greater than the first radial distance.
Method for fabrication of sleeveless photonic crystal canes with an arbitrary shape
The fabrication of sleeveless canes utilizes a preform with an array of glass canes in the preform. At least one tube-sleeve encircles the array of glass canes and is secured to the array of glass canes. The array of glass canes is moved into a furnace wherein the array of glass canes is heated. The furnace is maintained at a furnace temperature within the range of 2000° C. to 1700° C. and the array of glass canes is drawn from the furnace. The drawing of the array of glass canes both scales down the glass canes and elongates the glass canes. Maintaining the furnace at a furnace temperature within the range of 2000° C. to 1700° C. assures that the array of glass canes and the glass canes maintain their original shape.