C03B37/01473

Optical fiber

One of embodiments relates to an optical fiber in which an alkali metal element is efficiently doped to its core to suppress transmission loss from increasing. A mean concentration or a concentration distribution of the alkali metal element is adjusted such that 0.48 or less is obtained as an weighted value obtained by weighting a distribution of field intensity of guided light at a wavelength of 1550 nm, with respect to a radial direction distribution of a ratio I.sub.D2/I.sub.3 of an intensity I.sub.D2 of Raman scattering light by a silica three-membered ring structure and an intensity I.sub.3 of Raman scattering light by a SiO stretching vibration, in a cross-sectional region having a diameter of 20 m.

Method for producing optical fiber base material, and optical fiber base material

A method for manufacturing an optical fiber preform includes: adding an alkali metal element or an alkaline earth metal element to an inner surface of a glass pipe made of silica-based glass; reducing a diameter of the glass pipe after the adding; etching an inner surface of a continuous section of the glass pipe in a longitudinal direction after the reducing; and collapsing the glass pipe after the etching. At least one of the adding, the reducing, the etching, and the collapsing includes performing a local etching on an inner surface of a section of the glass pipe that is shorter than the continuous section.