Patent classifications
C03B37/02781
Hollow core photonic bandgap optical fibres and methods of fabrication
A hollow core photonic bandgap optical fibre comprises: a cladding comprising capillaries in a hexagonal array and a hollow core formed by excluding a hexagonal group of nineteen capillaries from the centre of the hexagonal array. The core is inflated. A core size ratio is 1.26 or above, defined as a ratio of the core diameter to the cladding diameter normalized to the ratio of the core diameter to the cladding diameter in an undistorted hexagonal array; a first ring ratio is between 0.55 and 2.50, defined as a ratio of the length of radially aligned struts separating the capillaries of the first ring to the length of a strut in an undistorted hexagonal array; and a core node spacing is between 0.60 and 1.90, where defined as a ratio of a strut length around the core of a largest corner capillary and a strut length around the core of a smallest side capillary. The fabrication method comprises four different pressures for the core, corner capillary, side capillary and cladding.
METHODS FOR PRODUCING A HOLLOW-CORE FIBER AND FOR PRODUCING A PREFORM FOR A HOLLOW-CORE FIBER
Methods are known for producing an anti-resonant hollow-core fiber which has a hollow core extending along a fiber longitudinal axis and an inner jacket region that surrounds the hollow core, said jacket region comprising multiple anti-resonant elements. The known methods have the steps of: providing a cladding tube that has a cladding tube inner bore and a cladding tube longitudinal axis along which a cladding tube wall extends that is delimited by an interior and an exterior; providing a number of tubular anti-resonant element preforms; arranging the anti-resonant element preforms at target positions of the interior of the cladding tube wall, thereby forming a primary preform which has a hollow core region and an inner jacket region; and elongating the primary preform in order to form the hollow-core fiber or further processing the primary preform in order to form a secondary preform. The aim of the invention is to achieve a high degree of precision and an exact positioning of the anti-resonant elements in a sufficiently stable and reproducible manner on the basis of the aforementioned methods. This is achieved in that a cladding tube is provided with an outer diameter ranging from 90 to 250 mm and a length of at least 1 m; tubular structural elements are provided, at least some of which have a wall thickness ranging from 0.2 to 2 mm and a length of at least 1 m; and the structural elements are arranged in the cladding tube inner bore while the cladding tube longitudinal axis is vertically oriented, the upper end face of each structural element being positioned at the target position.
METHODS FOR PRODUCING A HOLLOW-CORE FIBER AND FOR PRODUCING A PREFORM FOR A HOLLOW-CORE FIBER
Methods are known for producing an anti-resonant hollow-core fiber which has a hollow core extending along a fiber longitudinal axis and an inner jacket region that surrounds the hollow core, said jacket region comprising multiple anti-resonant elements. The known methods have the steps of: providing a cladding tube that has a cladding tube inner bore and a cladding tube longitudinal axis along which a cladding tube wall extends that is delimited by an interior and an exterior; providing a number of tubular anti-resonant element preforms; arranging the anti-resonant element preforms at target positions of the interior of the cladding tube wall, thereby forming a primary preform which has a hollow core region and an inner jacket region; and elongating the primary preform in order to form the hollow-core fiber or further processing the primary preform in order to form a secondary preform. The aim of the invention is to achieve a high degree of precision and an exact positioning of the anti-resonant elements in a sufficiently stable and reproducible manner on the basis of the aforementioned methods. This is achieved in that while carrying out a process according to step (c), components of the primary preform made of quartz glass and/or parts surrounding the primary preform made of quartz glass are heated and softened together, wherein the quartz glass of at least one of the preform components and/or the quartz glass of at least one of the parts surrounding the preform contains at least one dopant which decreases or increases the viscosity of quartz glass.
Optical fiber manufacturing method using relative bulk densities
An optical fiber manufacturing method includes setting a first holding member and a rod inside a glass pipe, the first holding member made of glass and having plural holes formed, so that the rod is supported by the first holding member; filling glass particles between the rod and a glass pipe inner wall; holding the rod such that the rod and the filled glass particles are enclosed by the glass pipe inner wall and the first and second holding members, and sealing one end of the glass pipe and manufacturing an intermediate; and manufacturing an optical fiber from the intermediate, wherein a bulk density of the first and second holding members is set with reference to a bulk density of a filling portion made from the glass particles, and the predetermined range is determined according to a core diameter permissible variation range in its longitudinal direction.
Hollow core optical fibre
A hollow core optical fibre comprises a tubular jacket; a cladding comprising a plurality of primary capillaries spaced apart from one another in a ring and each bonded to an inner surface of the jacket at a peripheral location around the circumference of the jacket; and a hollow core formed by a central void within the ring of primary capillaries; wherein the cladding further comprises, within each primary capillary, two secondary capillaries and no more, the two secondary capillaries spaced apart from one another and each bonded to an inner surface of the primary capillary at an azimuthal location around the circumference of the primary capillary which is displaced from the peripheral location of the primary capillary.
Optogenetic probe
An optogenetic probe, an optogenetic system, and a method for fabricating an optogenetic probe are provided. The optogenetic probe has a proximal and a distal end, and includes an elongated body made of a body glass material and extending longitudinally between the proximal and distal ends. The optogenetic probe also includes at least one optical channel, each including an optical channel glass material having a refractive index larger than a refractive index of the body glass material, so as to guide light therealong. The optogenetic probes also includes at least one electrical channel, each including an electrical channel structure having an electrical conductivity larger than the electrical conductivity of the body glass material, so as to conduct electricity therealong. The optogenetic probe further includes at least one fluidic channel, each adapted for transporting fluid therealong. Each optical, electrical and fluidic channel extends longitudinally within the elongated body.
METHODS FOR PRODUCING A HOLLOW-CORE FIBER AND FOR PRODUCING A PREFORM FOR A HOLLOW-CORE FIBER
Methods are known for producing an anti-resonant hollow-core fiber which has a hollow core extending along a fiber longitudinal axis and an inner jacket region that surrounds the hollow core, said jacket region comprising multiple anti-resonant elements. The known methods have the steps of: providing a cladding tube that has a cladding tube inner bore and a cladding tube longitudinal axis along which a cladding tube wall extends that is delimited by an interior and an exterior; providing a number of tubular anti-resonant element preforms; arranging the anti-resonant element preforms at target positions of the interior of the cladding tube wall, thereby forming a primary preform which has a hollow core region and an inner jacket region; and elongating the primary preform in order to form the hollow-core fiber or further processing the primary preform in order to form a secondary preform. The aim of the invention is to achieve a high degree of precision and an exact positioning of the anti-resonant elements in a sufficiently stable and reproducible manner on the basis of the aforementioned methods. This is achieved in that the step of providing and/or arranging the anti-resonant element preforms and/or the process of carrying out a hot-forming process includes a fixation measure and/or a sealing measure using an amorphous SiO.sub.2 particle-containing sealing or joining compound.
METHODS FOR PRODUCING A HOLLOW-CORE FIBER AND FOR PRODUCING A PREFORM FOR A HOLLOW-CORE FIBER
Methods are known for producing an anti-resonant hollow-core fiber which has a hollow core extending along a fiber longitudinal axis and an inner jacket region that surrounds the hollow core, said jacket region comprising multiple anti-resonant elements. The known methods have the steps of: providing a cladding tube that has a cladding tube inner bore and a cladding tube longitudinal axis along which a cladding tube wall extends that is delimited by an interior and an exterior; providing a number of tubular anti-resonant element preforms; arranging the anti-resonant element preforms at target positions of the interior of the cladding tube wall, thereby forming a primary preform which has a hollow core region and an inner jacket region; and elongating the primary preform in order to form the hollow-core fiber or further processing the primary preform in order to form a secondary preform. The aim of the invention is to achieve a high degree of precision and an exact positioning of the anti-resonant elements in a sufficiently stable and reproducible manner on the basis of the aforementioned methods. This is achieved in that the step of providing the cladding tube includes a processing measure, in which the cladding tube wall is machined with a longitudinal structure extending in the direction of the cladding tube longitudinal axis in the region of the target positions.
METHODS FOR PRODUCING A HOLLOW-CORE FIBER AND FOR PRODUCING A PREFORM FOR A HOLLOW-CORE FIBER
Methods are known for producing an anti-resonant hollow-core fiber which has a hollow core extending along a fiber longitudinal axis and an inner jacket region that surrounds the hollow core, said jacket region comprising multiple anti-resonant elements. The known methods have the steps of: providing a cladding tube that has a cladding tube inner bore and a cladding tube longitudinal axis along which a cladding tube wall extends that is delimited by an interior and an exterior; forming a number of precursors for anti-resonant elements at target positions of the cladding tube wall; and elongating the primary preform in order to form the hollow-core fiber or further processing the primary preform in order to form a secondary preform from which the hollow-core fiber is drawn. The aim of the invention is to achieve a high degree of precision and an exact positioning of the anti-resonant elements in a sufficiently stable and reproducible manner on the basis of the aforementioned methods. This is achieved in that the formation of the anti-resonant element precursors includes the formation of elongated pressure chambers, each of which adjoins a wall that can be deformed under pressure and heat in the region of the target positions of the anti-resonant elements and which cause a section of the deformable wall to protrude in the direction of the cladding tube inner bore under the effect of pressure and heat, thereby forming an anti-resonant element or a precursor for same, while carrying out a process according to step (c).
Hollow core optical fiber with controlled diameter hollow regions and method of making the same
A technique for fabricating a hollow core optical fiber with a controllable core region (in terms of diameter) is based upon regulating conditions (gas flow, volume, and/or temperature) within the hollow core region during the fiber draw process. The introduction of a gas, or any change in volume or temperature of the hollow core region, allows for the diameter of the hollow core region to self-regulate as a multistructured core rod (MCR) is drawn down into the final hollow core optical fiber structure. This self-regulation provides a core region having a diameter that selected and then stabilized for the duration of the draw process. The inventive process is also useful in controlling the diameter of any selected hollow region of an MCR including, but not limited to, shunts and corner capillaries disposed around the core region.