Patent classifications
C04B41/5058
METHOD OF REPAIRING CERAMIC COMPOSITE ARTICLES
A method of repairing an article including cleaning a repair area, wherein the repair area comprises a ceramic matrix composite; and depositing a ceramic material in the cleaned repair area using laser assisted chemical vapor deposition. Also disclosed is a repaired ceramic composite produced by this method.
Oxidation protection systems and methods
A method of forming a B.sub.4C layer as a component of an oxidation protection system as component of oxidation protection system on a carbon-carbon composite material may include forming a liquid mixture comprising a boron-compound and a carbon-compound. The method may further include applying the liquid mixture on the carbon-carbon composite material. The boron compound may comprise boric acid (H.sub.3BO.sub.3). In various embodiments, the carbon-compound comprises phenolic resin. In various embodiments, the method further includes heating the carbon-carbon composite material after applying the liquid mixture on the carbon-carbon composite material to from a boron carbide (B.sub.4C) layer.
Oxidation protection systems and methods
A method of forming a B.sub.4C layer as a component of an oxidation protection system as component of oxidation protection system on a carbon-carbon composite material may include forming a liquid mixture comprising a boron-compound and a carbon-compound. The method may further include applying the liquid mixture on the carbon-carbon composite material. The boron compound may comprise boric acid (H.sub.3BO.sub.3). In various embodiments, the carbon-compound comprises phenolic resin. In various embodiments, the method further includes heating the carbon-carbon composite material after applying the liquid mixture on the carbon-carbon composite material to from a boron carbide (B.sub.4C) layer.
OXIDATION PROTECTION WITH IMPROVED WATER RESISTANCE FOR COMPOSITES
Systems and methods for forming an oxidation protection system on a composite structure are provided. In various embodiments, the oxidation protection system comprises a boron-glass layer formed on the composite substrate and a silicon-glass layer formed over the boron-glass layer. Each of the boron-glass layer and the silicon-glass layer include a glass former and a glass modifier.
OXIDATION PROTECTION WITH IMPROVED WATER RESISTANCE FOR COMPOSITES
Systems and methods for forming an oxidation protection system on a composite structure are provided. In various embodiments, the oxidation protection system comprises a boron-glass layer formed on the composite substrate and a silicon-glass layer formed over the boron-glass layer. Each of the boron-glass layer and the silicon-glass layer include a glass former and a glass modifier.
OXIDATION PROTECTION SYSTEMS AND METHODS
A method of forming a B.sub.4C layer as a component of an oxidation protection system as component of oxidation protection system on a carbon-carbon composite material may include forming a liquid mixture comprising a boron-compound and a carbon-compound. The method may further include applying the liquid mixture on the carbon-carbon composite material. The boron compound may comprise boric acid (H.sub.3BO.sub.3). In various embodiments, the carbon-compound comprises phenolic resin. In various embodiments, the method further includes heating the carbon-carbon composite material after applying the liquid mixture on the carbon-carbon composite material to from a boron carbide (B.sub.4C) layer.
OXIDATION PROTECTION SYSTEMS AND METHODS
A method of forming a B.sub.4C layer as a component of an oxidation protection system as component of oxidation protection system on a carbon-carbon composite material may include forming a liquid mixture comprising a boron-compound and a carbon-compound. The method may further include applying the liquid mixture on the carbon-carbon composite material. The boron compound may comprise boric acid (H.sub.3BO.sub.3). In various embodiments, the carbon-compound comprises phenolic resin. In various embodiments, the method further includes heating the carbon-carbon composite material after applying the liquid mixture on the carbon-carbon composite material to from a boron carbide (B.sub.4C) layer.
Method for coating a ceramic matrix composite part with an environmental barrier
A method for coating a ceramic matrix composite part with an environmental barrier, the method including a) applying, to a surface of the part, a coating composition including a first powder of a rare earth silicate and a second powder including boron, the coating composition having a ratio R=[mass of the second powder]/[mass of the first powder] of between 0.1% and 5%, and b) sintering the first and second powders to obtain the environmental barrier on the part.
Method for coating a ceramic matrix composite part with an environmental barrier
A method for coating a ceramic matrix composite part with an environmental barrier, the method including a) applying, to a surface of the part, a coating composition including a first powder of a rare earth silicate and a second powder including boron, the coating composition having a ratio R=[mass of the second powder]/[mass of the first powder] of between 0.1% and 5%, and b) sintering the first and second powders to obtain the environmental barrier on the part.
COMPOSITE COMPONENT VOID REPAIR
Methods for repairing composite component voids are provided. For example, one method comprises locating a void in a composite component and subjecting the composite component to a process for repair. The process for repair includes creating a flow path through the void, applying a filler material to the composite component at the flow path, and processing the composite component having the filler material. In some embodiments, the flow path has a first opening on a first side of the composite component and a second opening on a second, opposite side of the composite component. In other embodiments, at least one portion of the flow path extends at a first angle with respect to a lateral direction defined by the CMC component, and at least another portion extends at a second angle with respect to the lateral direction.