C04B41/5059

Barrier coating with calcium aluminosilicate additive

A gas turbine engine article includes a substrate and a silicate-resistant barrier coating disposed on the substrate. The silicate-resistant barrier coating is composed of a refractory matrix and a calcium aluminosilicate additive (CAS additive) dispersed in the refractory matrix.

Barrier coating with calcium aluminosilicate additive

A gas turbine engine article includes a substrate and a silicate-resistant barrier coating disposed on the substrate. The silicate-resistant barrier coating is composed of a refractory matrix and a calcium aluminosilicate additive (CAS additive) dispersed in the refractory matrix.

Method to produce a ceramic matrix composite with controlled surface characteristics
11697623 · 2023-07-11 · ·

A method to produce a ceramic matrix composite with controlled surface characteristics includes: applying a scrim ply to a surface of a fiber preform, where the fiber preform includes silicon carbide fibers coated with boron nitride; infiltrating the fiber preform and the scrim ply with a slurry, thereby forming an impregnated ply on an impregnated fiber preform; infiltrating the impregnated fiber preform and the impregnated ply with a melt comprising silicon, and then cooling, thereby forming a ceramic matrix composite having a ceramic surface layer thereon, where the ceramic surface layer has a predetermined thickness and is devoid of boron; machining or grit blasting the ceramic surface layer to form an intermediate layer suitable for coating; and depositing an environmental barrier coating on the intermediate layer. Thus, a ceramic matrix composite coated with the environmental barrier coating is formed with the intermediate layer in between.

Method to produce a ceramic matrix composite with controlled surface characteristics
11697623 · 2023-07-11 · ·

A method to produce a ceramic matrix composite with controlled surface characteristics includes: applying a scrim ply to a surface of a fiber preform, where the fiber preform includes silicon carbide fibers coated with boron nitride; infiltrating the fiber preform and the scrim ply with a slurry, thereby forming an impregnated ply on an impregnated fiber preform; infiltrating the impregnated fiber preform and the impregnated ply with a melt comprising silicon, and then cooling, thereby forming a ceramic matrix composite having a ceramic surface layer thereon, where the ceramic surface layer has a predetermined thickness and is devoid of boron; machining or grit blasting the ceramic surface layer to form an intermediate layer suitable for coating; and depositing an environmental barrier coating on the intermediate layer. Thus, a ceramic matrix composite coated with the environmental barrier coating is formed with the intermediate layer in between.

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES

An oxidation protection system disposed on a substrate is provided, which may comprise a boron layer comprising a boron compound disposed on the substrate; a silicon layer comprising a silicon compound disposed on the boron layer; and at least one sealing layer comprising monoaluminum phosphate and phosphoric acid disposed on the silicon layer.

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES

An oxidation protection system disposed on a substrate is provided, which may comprise a boron layer comprising a boron compound disposed on the substrate; a silicon layer comprising a silicon compound disposed on the boron layer; and at least one sealing layer comprising monoaluminum phosphate and phosphoric acid disposed on the silicon layer.

Coating fabrication method for producing engineered microstructure of silicate-resistant barrier coating

A coating fabrication method includes providing engineered granules and thermally consolidating the engineered granules on a substrate to form a silicate-resistant barrier coating. Each of the engineered granules is an aggregate of at least one refractory matrix region and at least one calcium aluminosilicate additive region (CAS additive region) attached with the at least one refractory matrix region. In the thermal consolidation, the refractory matrix region from the engineered granules form grains of a refractory matrix of the silicate-resistant barrier coating and the CAS additive region from the engineered granules form CAS additives that are dispersed in grain boundaries between the grains.

Coating fabrication method for producing engineered microstructure of silicate-resistant barrier coating

A coating fabrication method includes providing engineered granules and thermally consolidating the engineered granules on a substrate to form a silicate-resistant barrier coating. Each of the engineered granules is an aggregate of at least one refractory matrix region and at least one calcium aluminosilicate additive region (CAS additive region) attached with the at least one refractory matrix region. In the thermal consolidation, the refractory matrix region from the engineered granules form grains of a refractory matrix of the silicate-resistant barrier coating and the CAS additive region from the engineered granules form CAS additives that are dispersed in grain boundaries between the grains.

Environmental barrier coating

An article includes a ceramic-based substrate and a barrier layer on the ceramic-based substrate. The barrier layer includes a matrix phase and gettering particles in the matrix phase. The gettering particles with an aspect ratio greater than one are aligned such that a maximum dimension of the gettering particles extends along an axis that is generally parallel to the substrate. The barrier layer includes a dispersion of diffusive particles in the matrix phase. A composite material and a method of applying a barrier layer to a substrate are also disclosed.

Environmental barrier coating

An article includes a ceramic-based substrate and a barrier layer on the ceramic-based substrate. The barrier layer includes a matrix phase and gettering particles in the matrix phase. The gettering particles with an aspect ratio greater than one are aligned such that a maximum dimension of the gettering particles extends along an axis that is generally parallel to the substrate. The barrier layer includes a dispersion of diffusive particles in the matrix phase. A composite material and a method of applying a barrier layer to a substrate are also disclosed.