C04B41/5064

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES
20210276924 · 2021-09-09 · ·

An oxidation protection system disposed on a substrate is provided, which may comprise a base layer comprising a first pre-slurry composition comprising a first phosphate glass composition, and/or a sealing layer comprising a second pre-slurry composition comprising a second phosphate glass composition and a strengthening compound comprising boron nitride, a metal oxide, and/or silicon carbide.

CUTTING INSERT AND METHOD FOR MANUFACTURING THE SAME
20210268589 · 2021-09-02 ·

A cutting insert comprises: a body; and a blade fixed to the body and made of a polycrystalline cubic boron nitride including 98.5% by volume or more of cubic boron nitride, the blade having a rake face and a flank face, the rake face and the flank face meeting each other and thus forming a ridge line which serves as a cutting edge, the rake face being provided with a land surface extending along the cutting edge, and a chip breaker disposed on a side opposite to the cutting edge with the land surface therebetween and also having a recess contiguous to the land surface.

CUTTING INSERT AND METHOD FOR MANUFACTURING THE SAME
20210268589 · 2021-09-02 ·

A cutting insert comprises: a body; and a blade fixed to the body and made of a polycrystalline cubic boron nitride including 98.5% by volume or more of cubic boron nitride, the blade having a rake face and a flank face, the rake face and the flank face meeting each other and thus forming a ridge line which serves as a cutting edge, the rake face being provided with a land surface extending along the cutting edge, and a chip breaker disposed on a side opposite to the cutting edge with the land surface therebetween and also having a recess contiguous to the land surface.

High temperature oxidation protection for composites
11091402 · 2021-08-17 · ·

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition comprising a first phosphate glass composition, with a primary flow modifier and a first carrier fluid, wherein the primary flow modifier comprises at least one of cellulose or calcium silicate; applying the first slurry on a surface of the composite structure to form a base layer; and heating the composite structure to a temperature sufficient to adhere the base layer to the composite structure.

High temperature oxidation protection for composites
11091402 · 2021-08-17 · ·

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition comprising a first phosphate glass composition, with a primary flow modifier and a first carrier fluid, wherein the primary flow modifier comprises at least one of cellulose or calcium silicate; applying the first slurry on a surface of the composite structure to form a base layer; and heating the composite structure to a temperature sufficient to adhere the base layer to the composite structure.

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES
20210179503 · 2021-06-17 · ·

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition with a first carrier fluid, applying the first slurry on a surface of the composite structure, and heating the composite structure to a temperature sufficient to form a base layer on the composite structure. The first pre-slurry composition may comprise a first phosphate glass composition and a low coefficient of thermal expansion material, wherein the low coefficient of thermal expansion material is a material with a coefficient of thermal expansion of less than 10×10.sup.−6° C.

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES
20210179503 · 2021-06-17 · ·

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition with a first carrier fluid, applying the first slurry on a surface of the composite structure, and heating the composite structure to a temperature sufficient to form a base layer on the composite structure. The first pre-slurry composition may comprise a first phosphate glass composition and a low coefficient of thermal expansion material, wherein the low coefficient of thermal expansion material is a material with a coefficient of thermal expansion of less than 10×10.sup.−6° C.

High temperature oxidation protection for composites
11046619 · 2021-06-29 · ·

An oxidation protection system disposed on a substrate is provided, which may comprise a base layer comprising a first pre-slurry composition comprising a first phosphate glass composition, and/or a sealing layer comprising a second pre-slurry composition comprising a second phosphate glass composition and a strengthening compound comprising boron nitride, a metal oxide, and/or silicon carbide.

High temperature oxidation protection for composites

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition with a first carrier fluid, applying the first slurry on a surface of the composite structure, and heating the composite structure to a temperature sufficient to form a base layer on the composite structure. The first pre-slurry composition may comprise a first phosphate glass composition and a low coefficient of thermal expansion material, wherein the low coefficient of thermal expansion material is a material with a coefficient of thermal expansion of less than 10×10.sup.−6° C.

High temperature oxidation protection for composites

The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition with a first carrier fluid, applying the first slurry on a surface of the composite structure, and heating the composite structure to a temperature sufficient to form a base layer on the composite structure. The first pre-slurry composition may comprise a first phosphate glass composition and a low coefficient of thermal expansion material, wherein the low coefficient of thermal expansion material is a material with a coefficient of thermal expansion of less than 10×10.sup.−6° C.