Patent classifications
C08K2003/2224
Flame retardant fiber optic cable with halogen free sheath for blowing applications
Embodiments of the disclosure relate to an optical fiber cable. The optical fiber cable includes a subunit having a first interior surface and a first exterior surface. The first interior surface defines a central bore along a longitudinal axis of the optical fiber cable. At least one optical fiber is disposed within the central bore of the subunit, and a plurality of strengthening yarns is disposed around the subunit. A cable sheath disposed around the plurality of strengthening yarns. The cable sheath has a second interior surface and a second exterior surface. The second exterior surface defines an outermost surface of the optical fiber cable. The cable sheath includes from 55% to 68% by weight of a mineral-based flame retardant additive and from 35% to 45% by weight of a polymer blend. The polymer blend includes a co-polyester or co-polyether and a polyolefin or a polyolefin elastomer.
LOW SMOKE HALOGEN FREE FLAME RETARDANT THERMOPLASTIC ELASTOMER COMPOSITIONS
Halogen-free flame retardant compositions comprising thermoplastic elastomers, which exhibit flame retardance and low-smoke emission. The flame retardant compositions comprise (a) one or more thermoplastic elastomers; and (b) a flame retardant mixture comprising: magnesium hydroxide, aluminium trihydrate, melamine cyanurate, and optionally a phosphate ester flame retardant.
Epoxy resin composition for neutron shielding, and method for preparing the same
Provided is an epoxy resin composition including a nano-sized radioactive radiation shielding material which has superior shielding effects for against radiation, and to a method for preparing same. In particular, the method for preparing the epoxy resin composition for neutron shielding, includes the steps of: a step of mixing a boron compound powder for absorbing neutrons, optionally a high density metal powder for shielding from against gamma rays and a flame retardant powder, respectively separately or in combination, with an amine-based curing agent to obtain a mixture of a curing agent and a powder; an ultrasonic wave treating step of applying ultrasonic waves to the mixture to coat the surface of the powder with the amine-based curing agent and to disperse the powder in the curing agent; and a dispersing step of mixing and dispersing the amine-based curing agent, that was dispersed and includes the powder treated with ultrasonic waves, in an epoxy resin.
Flame retardant polymeric composition
The invention disclose halogen free thermoplastic or cross linked polymers compositions comprising a polyolefin and/or a polyolefin containing polar co-monomers and a combination of metal hydroxides and inorganic hypophosphite as a synergic, and optionally other ingredients. These compositions show a superior balance of flame retardant properties compared to already known corresponding halogen free formulations. Molded items obtained using the polymer composition according to the present invention are useful in a wide range of injection molding and extrusion applications, especially cables.
Flame retardant polymeric composition
The invention disclose halogen free thermoplastic or cross linked polymers compositions comprising a polyolefin and/or a polyolefin containing polar co-monomers and a combination of metal hydroxides and inorganic hypophosphite as a synergic, and optionally other ingredients. These compositions show a superior balance of flame retardant properties compared to already known corresponding halogen free formulations. Molded items obtained using the polymer composition according to the present invention are useful in a wide range of injection molding and extrusion applications, especially cables.
Heat-resistant chlorine-containing crosslinked resin formed body and method for producing the same, silane master batch, master batch mixture and formed body thereof, and heat-resistant product
A production method comprising: (a) a step of melt-mixing a base resin containing a chlorinated polyethylene; an organic peroxide, an inorganic filler, and a silane coupling agent, in specific ratios, at a temperature equal to or higher than a decomposition temperature of the organic peroxide, to prepare a silane master batch; (b) a step of mixing the silane master batch obtained in the step (a) with a silanol condensation catalyst, and then forming the resultant mixture; and conducting at least one of the melt-mixing in the step (a) and the mixing in the step (b) is performed in the coexistence of a chloroprene rubber or a polyvinyl chloride; a heat-resistant chlorine-containing crosslinked resin formed body produced by the method, a silane master batch, a mixture and formed body thereof, and a heat-resistant product.
Rubber composition, processing method thereof, and flame-retardant product using the same
The present invention discloses a rubber composition, a processing method for obtaining the rubber composition, and application of the composition in processing of flame-retardant products. The rubber composition includes a rubber matrix and essential components. The rubber matrix includes a branched polyethylene with a content represented as A, in which 0<A≤100, and an EPM and an EPDM with a total content represented as B, in which 0≤B<100. The essential components include 1.5 to 10 parts of a crosslinking agent and 40 to 300 parts of a flame-retardant agent. The rubber composition can be applied to production of flame-retardant products, such as flame-retardant cable, flame-retardant cool air hose for automobile, flame-retardant sealing strip, high-temperature-resistant flame-retardant conveyor belt, and flame-retardant waterproof coil. The products have good flame-retardant effects and mechanical properties.
INSULATING TAPE
Provided is an insulating tape to be used in a nonaqueous secondary battery, the insulating tape being capable of maintaining its insulating property even under a severe environment, e.g., even when being heated, and being capable of improving the safety of the nonaqueous secondary battery. Specifically, provided is an insulating tape for a nonaqueous battery, including a base material, and a pressure-sensitive adhesive layer arranged on one side, or each of both sides, of the base material, in which the base material and/or the pressure-sensitive adhesive layer each contain/contains an insulating inorganic filler. Also provided is an insulating tape for a nonaqueous battery, including a base material with an insulating layer, and a pressure-sensitive adhesive layer arranged on one side, or each of both sides, of the base material with the insulating layer, in which the insulating layer contains an insulating inorganic filler.
Flame-retardant and fire-resistant polymer compositions made from lime
A mineral filler in a flame-retardant organic polymer composition comprising a calcium compound for a fire-resistant effect characterized in that said calcium compound comprises at least calcium hydroxide, use of same and the combustion residue obtained therefrom, and polymer sheaths for electrical cables containing the mineral filler in the flame-retardant polymer composition.
COLLOIDAL SILICA COATED MAGNESIUM HYDROXIDE
Magnesium hydroxide having low glossiness and acid resistance which is required for coatability. The magnesium hydroxide is coated magnesium hydroxide comprising magnesium hydroxide and colloidal silica coating the surface thereof, wherein (A) the coating amount of colloidal silica is 0.1 to 20.0 wt % in terms of SiO.sub.2 based on 100 wt % of magnesium hydroxide; and (B) the coated magnesium hydroxide has a long diameter (width) of 0.5 to 20 μm, a thickness of 0.01 to 0.5 μm and an aspect ratio of not less than 10.