Patent classifications
C04B35/62873
AUTOMATED PREPARATION METHOD OF A SICF/SIC COMPOSITE FLAME TUBE
An automated preparation method of a SiC.sub.f/SiC composite flame tube, comprising the following steps: preparing an interface layer for a SiC fiber by a chemical vapor infiltration process, and obtaining the SiC fiber with a continuous interface layer; laying a unidirectional tape on the SiC fiber with the continuous interface layer and winding the SiC fiber with the continuous interface layer to form and obtaining a preform of a net size molding according to a fiber volume and a fiber orientation obtained in a simulation calculation; and adopting a reactive melt infiltration process and the chemical vapor infiltration process successively for a densification and obtaining a high-density SiC.sub.f/SiC composite flame tube in a full intelligent way. The SiC.sub.f/SiC composite flame tube prepared by the present disclosure not only has a high temperature resistance, but also has a low thermal expansion coefficient, high thermal conductivity and high thermal shock resistance.
Method of treating ceramic fibers by phosphating
A method of treating silicon carbide fibers comprises phosphating heat treatment in a reactive gas so as to form a coating around each fiber for protection against oxidation. The coating comprises a surface layer of silicon pyrophosphate crystals and at least one underlying bilayer system comprising a layer of a phosphosilicate glass and a layer of microporous carbon.
Method for manufacturing an oxide/oxide composite material turbomachine blade provided with internal channels
An oxide/oxide composite material turbomachine blade including a fiber reinforcement obtained by weaving a first plurality of threads and a second plurality of threads, with the threads of said first plurality of threads being arranged in successive layers and extending in the longitudinal direction of the fiber blank corresponding to the longitudinal direction of the blade is disclosed. The reinforcement is densified by a matrix, with the blade further including one or several internal channels having a coiled shape extending in the longitudinal direction of the blade.
METHOD OF MAKING A CERAMIC MATRIX COMPOSITE THAT EXHIBITS CHEMICAL RESISTANCE
A method of making a ceramic matrix composite that exhibits chemical resistance has been developed. The method comprises depositing a compliant layer comprising boron nitride, silicon-doped boron nitride, and/or pyrolytic carbon on silicon carbide fibers, depositing a barrier layer having a high contact angle with molten silicon on the compliant layer, and depositing a wetting layer comprising silicon carbide, boron carbide, and/or pyrolytic carbon on the barrier layer. After depositing the wetting layer, a fiber preform comprising the silicon carbide fibers is infiltrated with a slurry. After slurry infiltration, the fiber preform is infiltrated with a melt comprising silicon, and then the melt is cooled, thereby forming a ceramic matrix composite.
METHOD OF MAKING A CERAMIC MATRIX COMPOSITE THAT EXHIBITS MOISTURE AND ENVIRONMENTAL RESISTANCE
A method of making a ceramic matrix composite that exhibits moisture and environmental resistance has been developed. The method includes depositing a diffusion barrier layer comprising boron nitride on silicon carbide fibers and depositing a moisture-tolerant layer comprising silicon-doped boron nitride on the diffusion barrier layer, where a thickness of the moisture-tolerant layer is from about 3 to about 300 times a thickness of the diffusion barrier layer. Thus, a compliant multilayer including the moisture-tolerant layer and the diffusion barrier layer is formed. A wetting layer comprising silicon carbide, boron carbide, and/or pyrolytic carbon is deposited on the compliant multilayer layer. After depositing the wetting layer, a fiber preform comprising the silicon carbide fibers is infiltrated with a slurry. After slurry infiltration, the fiber preform is infiltrated with a melt comprising silicon and then the melt is cooled, thereby forming a ceramic matrix composite.
Method for producing a surface layer on a ceramic matrix composite
A method is provided in which a resin coating is applied to a surface of a preform. The resin coating includes a carbonaceous resin and a particulate. The preform is added to a tooling. The preform, which is positioned in the tooling, is cured. The tooling is removed. The resin coating on the surface of the preform is pyrolyzed to form a resin carbon-char layer on the surface of the preform. The preform and the resin carbon-char layer are infiltrated with silicon to form a ceramic matrix composite (CMC) component including a layer of silicon carbide. During the infiltration, the silicon reacts with carbon in the resin carbon-char layer to form the layer of silicon carbide on the preform.
Low-thickness thermostructural composite material part, and manufacture method
A thermostructural composite material part including carbon or ceramic fiber reinforcement densified by a matrix having at least one thin portion in which: the thickness of the part is less than 2 mm, or indeed less than 1 mm; the fiber reinforcement is made as a single thickness of multilayer fabric made of spread yarns having a weight of not less than 200 tex; the fiber volume ratio lies in the range 25% to 45%; and the ratio between the number of layers of the multilayer fabric and the thickness in millimeters of the part is not less than four.
Method of fabricating a turbine or compressor guide vane sector made of composite material for a turbine engine, and a turbine or a compressor incorporating such guide vane sectors
Single-airfoil vanes each having an inner platform, an outer platform, and an airfoil are obtained by three-dimensionally weaving a fiber blank in a single piece, by shaping the fiber blank to obtain a single-piece fiber preform, and by densifying the preform with a matrix to obtain a vane of composite material forming a single piece with inner and outer platforms incorporated therein. A plurality of vanes is assembled together at an intermediate stage of densification to form a multi-airfoil composite material guide vane sector for a turbine nozzle or a compressor diffuser and the assembled-together vanes are bonded together.
ARTICLES FOR CREATING HOLLOW STRUCTURES IN CERAMIC MATRIX COMPOSITES
The present disclosure relates to a method of fabricating a ceramic composite components. The method may include providing at least a first layer of reinforcing fiber material which may be a pre-impregnated fiber. An additively manufactured component may be provided on or near the first layer. A second layer of reinforcing fiber, which may be a pre-impregnated fiber may be formed on top the additively manufactured component. A precursor is densified to consolidates at least the first and second layer into a densified composite, wherein the additively manufactured material defines at least one cooling passage in the densified composite component.
METHOD FOR PRODUCING CERAMIC MATRIX COMPOSITE
A production method for a ceramic matrix composite is comprised of: compounding an aggregate powder including a ceramic and a binder including at least one of thermoplastic resins and waxes to form a composition of the aggregate powder and the binder; pressing the composition to form sheets; accumulating fabrics of reinforcement fibers including the ceramic and the sheets alternately; pressing an accumulated body of the fabrics and the sheets; and generating a matrix combining the reinforcement fibers together.