C04B35/62868
Method to produce a ceramic matrix composite with controlled surface characteristics
A method to produce a ceramic matrix composite with controlled surface characteristics includes: applying a scrim ply to a surface of a fiber preform, where the fiber preform includes silicon carbide fibers coated with boron nitride; infiltrating the fiber preform and the scrim ply with a slurry, thereby forming an impregnated ply on an impregnated fiber preform; infiltrating the impregnated fiber preform and the impregnated ply with a melt comprising silicon, and then cooling, thereby forming a ceramic matrix composite having a ceramic surface layer thereon, where the ceramic surface layer has a predetermined thickness and is devoid of boron; machining or grit blasting the ceramic surface layer to form an intermediate layer suitable for coating; and depositing an environmental barrier coating on the intermediate layer. Thus, a ceramic matrix composite coated with the environmental barrier coating is formed with the intermediate layer in between.
Ceramic matrix composite and method of manufacturing the same
A ceramic matrix composite includes a substrate which contains a fibrous body made of silicon carbide fiber, and a matrix which is formed in the substrate, and which contains silicon carbide and a silicon material made of silicon or a binary silicon alloy.
Fiber having integral weak interface coating, method of making and composite incorporating the fiber
Disclosed is a method of coating a high temperature fiber including depositing a base material on the high temperature fiber using atomic layer deposition, depositing an intermediate material precursor on the base material using molecular layer deposition, depositing a top material on the intermediate material precursor or the intermediate layer using atomic layer deposition, and heat treating the intermediate precursor. The intermediate material in the final coating includes a structural defect, has lower density than the top material or a combination thereof. Also disclosed are the coated high temperature fiber and a composite including the high temperature fiber.
THROUGH THICKNESS REINFORCEMENT
A method for making a ceramic matrix composite component includes densifying a fibrous preform of the component with a ceramic matrix to form an intermediate component; infiltrating a hole in the intermediate component with an infiltrate material comprising a solid and a metallic alloy whose reaction forms a carbide, silicide, boride or combination thereof, heating the infiltrate material to a temperature in excess of a melting point of the metallic alloy; and sequentially cooling regions of the hole starting from an interior end of the hole to the outer surface of the intermediate component to form a solidified through-thickness reinforcement element. The hole extends in a through-thickness direction and is open to an exterior surface of the intermediate component.
Automated preparation method of a SiC.SUB.f./SiC composite flame tube
An automated preparation method of a SiC.sub.f/SiC composite flame tube, comprising the following steps: preparing an interface layer for a SiC fiber by a chemical vapor infiltration process, and obtaining the SiC fiber with a continuous interface layer; laying a unidirectional tape on the SiC fiber with the continuous interface layer and winding the SiC fiber with the continuous interface layer to form and obtaining a preform of a net size molding according to a fiber volume and a fiber orientation obtained in a simulation calculation; and adopting a reactive melt infiltration process and the chemical vapor infiltration process successively for a densification and obtaining a high-density SiC.sub.f/SiC composite flame tube in a full intelligent way. The SiC.sub.f/SiC composite flame tube prepared by the present disclosure not only has a high temperature resistance, but also has a low thermal expansion coefficient, high thermal conductivity and high thermal shock resistance.
Doped silicon carbide ceramic matrix composite
A method for forming ceramic matrix composite (CMC) component includes forming a fiber preform, positioning the fiber preform into a chemical vapor infiltration reactor chamber, and densifying the fiber preform. Densification includes infiltrating the fiber preform with a first gas comprising precursors of silicon carbide and infiltrating the fiber preform with a second gas comprising a first rare earth element, wherein the steps of infiltrating the fiber preform with the first gas and infiltrating the fiber preform with the second gas are conducted simultaneously to produce a first rare earth-doped silicon carbide matrix in a first region of the component.
Method for treating silicon carbide fibres
A method of treating at least one silicon carbide fibre, the method including a) formation of a silica layer at the surface of a silicon carbide fibre having an oxygen content less than or equal to 1% in atomic percentage, the silica layer being formed by contacting this fibre with an oxidizing medium having a temperature greater than or equal to 50° C. and pressure greater than or equal to 1 MPa, and b) removal of the silica layer formed by hydrothermal treatment of the fibre obtained after implementation of step a) in which the fibre is treated with water at a pressure between saturating vapour pressure and 30 MPa and at a temperature less than or equal to 400° C.
CONSTANT CROSS SECTION MANDREL FOR CMC COMPONENTS
A mandrel for a molding process includes a first portion and a second portion that form a mandrel having a channel between the first and second portions. At least one locking pin is configured to urge the first and second portions away from each other to establish a gap in response to inserting the locking pin into the channel along a respective end of the mandrel. A molding apparatus and method of forming a matrix composite component are also disclosed.
CERAMIC MATRIX COMPOSITE WITH INTERFACIAL COATING SYSTEM
A ceramic matrix composite includes a ceramic matrix, fibers embedded in the ceramic matrix, and an interfacial coating system on each of the fibers. The interfacial coating system includes alternating layers of boron nitride layers of individual thicknesses of about 50 nanometers to 200 nanometers and carbon layers of individual thicknesses of less than 5 nanometers.
Method for producing a hollow part made of a ceramic matrix composite material
A method for producing a hollow part made of a ceramic matrix composite material. The method includes shaping a hollow fibrous preform. A core of oxidizable material is housed or inserted into the preform. The method also includes consolidating the preform and extracting the core by oxidising the core.