C08G18/797
Two-component polyurethane composition
A two-component polyurethane composition including a polyol component and a polyisocyanate component, wherein the polyol component comprises at least one polyester polyol A1 based on dimer fatty acids and/or dimer fatty alcohols having an OH number of 65-350 mg KOH/g, at least one polybutadiene polyol A2 and at least one alkoxylated alkylenediamine A3. The polyurethane composition has high strength and only a minor dependence of the mechanical properties, especially strength, on temperature, especially in the range from −40° C. to +100° C.
Hydroformylated triglycerides and uses thereof
This disclosure provides methods for the chemical modification of triglycerides that are highly enriched in specific fatty acids and subsequent use thereof for producing functionally versatile polymers.
EPOXY PHOSPHATE ESTER
Provided is a composition comprising one or more epoxy phosphate esters wherein the structure comprises two or more polyester linkages. Also provided is a method of making the epoxy phosphate esters that comprises reacting one or more epoxy-terminated polyesters with one or more phosphoric acids. Further provided is an adhesive composition that comprises one or more epoxy phosphate esters, one or more multifunctional isocyanate prepolymers, and one or more multifunctional isocyanate-reactive compounds.
Binders containing secondary amine groups, based on cyclic ethers
The present invention relates to a process for producing polyaspartic ester compositions by reacting cyclic ethers bearing primary amino and/or primary aminoalkyl groups with fumaric and/or maleic esters, to the polyaspartic ester compositions thus obtainable, and to the use thereof in two-component coating compositions.
AQUEOUS COMPOSITION FOR SURFACE COATING AND AUTOMOTIVE SHEET USING THE COMPOSITION
Disclosed is an aqueous composition for surface coating, including: a main ingredient comprising a first compound having at least two functional groups selected from the group consisting of a carboxyl group, a hydroxyl group, an amino group and combinations thereof, per molecule; a curing agent comprising a second compound having at least two functional groups selected from the group consisting of an aziridine group, an isocyanate group, a carbodiimide group and combinations thereof, per molecule; and an aqueous solvent. Further, an automotive sheet using the aqueous composition for surface coating is disclosed.
ASPHALT COMPOSITION COMPRISING MONOMERIC MDI AS THERMOSETTING REACTIVE COMPOUND
An asphalt composition comprising 0.1 to 10.0 wt.-% monomeric MDI based on the total weight of the composition.
POLYESTER-MODIFIED POLYBUTADIENOLS FOR PRODUCING POLYURETHANE ELASTOMERS AND THERMOPLASTIC POLYURETHANES
The invention relates to polyurethanes obtainable by reaction of (a) polyisocyanates A selected from modified or unmodified 4,4′-methanediphenyl diisocyanate, higher nuclear homologs of 4,4′-methanediphenyl diisocyanate, isocyanated groups containing prepolymers based on 4,4′methandiphenyl diisocyanate, and mixtures thereof, with (b) compounds having at least two isocyanate-reactive hydrogen atoms, comprising (b1) block copolymers formed from a polybutadienol and a cyclic ester as component B1, and (b2) low molecular weight extenders or crosslinkers each having a molecular weight of 62 to 500 g/mol as component B2.
POLYUREA COMPOSITION
The invention relates to compositions comprising at least one first and one second component; —the first component K1 comprising at least one di(aminobenzoate) ester A1 of formula (I) with an average molecular weight of 500 g/mol to 2000 g/mol, preferably 600 g/mol to 1500 g/mol and particularly preferred between 650 g/mol and 1300 g/mol, G being a divalent group derived from poly(tetramethylene oxide) diol, and —the second component K2 comprising at least one aromatic polyisocyanate B1 with an average molecular weight of 160 g/mol to 1100 g/mol, preferably 500 g/mol to 800 g/mol.
SPRAYABLE POLYURETHANE COATING
Provided is a sprayable polyurethane coating, comprising the reaction product of an isocyanate component and an isocyanate-reactive component, wherein the isocyanate component includes an isocyanate, and the isocyanate-reactive component includes a cardanol-modified epoxy polyol. The cardanol-modified epoxy polyol is a reaction product of an epoxy component and an epoxy-reactive component at a ratio of epoxy groups to epoxy reactive groups from 1:0.95 to 1:5, and the epoxy-reactive component includes a cardanol component. A sprayable polyurethane based reaction system comprising the sprayable polyurethane coating and a process for forming the sprayable polyurethane coating are also provided.
SOFT SOLVENT-FREE FLAME-RETARDANT POLYURETHANE SYNTHETIC LEATHER AND PREPARATION METHOD THEREFOR
Disclosed are a soft solvent-free flame-retardant polyurethane synthetic leather and a preparation method therefor. The soft solvent-free flame-retardant polyurethane synthetic leather comprises an antifouling layer, a surface layer, an intermediate layer, a bonding layer and a base cloth in sequence from top to bottom, wherein the bonding layer is prepared from component A and an isocyanate; the molar ratio of —NCO in the isocyanate to —OH in the component A is 0.85-0.93; and the component A is composed of a polyhydric alcohol, an inhibition-type catalyst, a flame retardant, a filler and a viscosity modifier in parts by weight.
Disclosed are a soft solvent-free flame-retardant polyurethane synthetic leather and a preparation method therefor. The soft solvent-free flame-retardant polyurethane synthetic leather comprises an antifouling layer, a surface layer, an intermediate layer, a bonding layer and a base cloth in sequence from top to bottom, wherein the bonding layer is prepared from component A and an isocyanate; the molar ratio of —NCO in the isocyanate to —OH in the component A is 0.85-0.93; and the component A is composed of a polyhydric alcohol, an inhibition-type catalyst, a flame retardant, a filler and a viscosity modifier in parts by weight. The polyurethane synthetic leather prepared by the present invention has daily life antifouling properties, a good durability, is soft to the touch, is strongly skin-friendly, and has a very superior flame-retardant performance, and also has excellent antifouling, scratch resistance and flexure resistance properties; the production process is simple, efficient and environmentally friendly and same can satisfy market demands.