D01D1/04
Composite fabric and method for making the same
A method for manufacturing a composite fabric includes the steps of feeding, mixing and stirring, first drying, hot melt extrusion, first cooling, stretch extension, second cooling, winding-strands-into-roll, second drying, and weaving. The composite fabric is composed of multiple first threads and multiple second threads which are woven to the first threads. The first threads and the second threads are respectively reflective threads and glowing threads so that the composite fabric includes both features of light reflection and glowing in dark.
Wire drawing process of light storage wire
A wire drawing process of a light storage wire includes a feeding step, a mixing step, a first drying step, a hot melt extrusion step, a first cooling step, a shaping/organizing wire step, a hot-temperature remodeling step, a stretching step, a second cooling step, a strand winding/rolling step, and a second drying step.
Wire drawing process of light storage wire
A wire drawing process of a light storage wire includes a feeding step, a mixing step, a first drying step, a hot melt extrusion step, a first cooling step, a shaping/organizing wire step, a hot-temperature remodeling step, a stretching step, a second cooling step, a strand winding/rolling step, and a second drying step.
Preparation method of chitin-modified polypropylene spunbond non-woven fabric
A chitin-modified polypropylene spunbond non-woven fabric and a preparation method of the chitin-modified polypropylene spunbond non-woven fabric are provided. The chitin-modified polypropylene spunbond non-woven fabric contains a modified chitin in a weight percentage range of approximately 0.2%-1.5%. The modified chitin includes chitin modified by a modifier including 2-hydroxybenzimidazole, cellulose acetate butyrate, and adipic acid dihydrazide. The chitin-modified polypropylene spunbond non-woven fabric has an anti-mold grade less than 1, and an antibacterial rate greater than 9.5%.
Efficient fiber manufacturing
Various embodiments of the present disclosure can include at least one of a method, apparatus and system for the efficient melting of a feedstock to at least one of a molten and vitrified state to be used in a manufacturing system comprised of: a melter to which the feedstock is provided; and a heat recovery system configured to capture exhaust waste heat produced by the melter, wherein the heat recovery system transfers an energy recovered from the exhaust waste heat to pre-heat the feedstock provided to the melter.
Efficient fiber manufacturing
Various embodiments of the present disclosure can include at least one of a method, apparatus and system for the efficient melting of a feedstock to at least one of a molten and vitrified state to be used in a manufacturing system comprised of: a melter to which the feedstock is provided; and a heat recovery system configured to capture exhaust waste heat produced by the melter, wherein the heat recovery system transfers an energy recovered from the exhaust waste heat to pre-heat the feedstock provided to the melter.
MELT ELECTROSPINNING DEVICE AND METHOD
The present disclosure provides a melt electrospinning device. The melt electrospinning device includes a melting unit, a spinning unit, an electrostatic generating unit, a collection unit, and a sealed cavity. A lining of the melting unit is made of a material having a melting point greater than 500° C. The spinning unit is connected to the bottom of the melting unit and includes a spinneret made from a conductive material having a melting point greater than 500° C. The melt electrospinning process is performed in the sealed cavity. The present disclosure further provides a melt electrospinning method.
MELT ELECTROSPINNING DEVICE AND METHOD
The present disclosure provides a melt electrospinning device. The melt electrospinning device includes a melting unit, a spinning unit, an electrostatic generating unit, a collection unit, and a sealed cavity. A lining of the melting unit is made of a material having a melting point greater than 500° C. The spinning unit is connected to the bottom of the melting unit and includes a spinneret made from a conductive material having a melting point greater than 500° C. The melt electrospinning process is performed in the sealed cavity. The present disclosure further provides a melt electrospinning method.
SYSTEMS FOR MANUFACTURING BULKED CONTINUOUS CARPET FILAMENT
Systems for manufacturing bulked continuous carpet filament from polymer, where the systems are configured for: (1) passing polymer flakes through a crystalliers; (2) melting the polymer to create a first single stream of polymer melt; (3) separating the first single stream of polymer melt into multiple streams of polymer melt; (4) exposing the multiple streams of polymer melt to a pressure of between about 0 millibars and about 25 millibars in a chamber; (5) recombining the multiple streams of polymer melt into a second single stream of polymer melt; and (6) providing the second single stream of polymer melt to one or more spinning machines that are configured to form the second single stream of polymer melt into bulked continuous carpet filament.
Preparation method of a fabric
The present disclosure provides a fabric, a preparation method thereof and clothing formed therefrom. The preparation method includes the following steps: obtaining bio-based synthetic fiber chips from textile waste materials; obtaining extruded filaments from the bio-based synthetic fiber chips by adopting a spinning solution; and weaving and interlocking the extruded filaments with bio-based elastic fibers to obtain the fabric. The prepared fabric is obtained from the textile waste materials, so that waste recycling is realized, and the pollution of the textile wastes to the environment is avoided. The spinning solution is adopted in the preparation process of the fabric, so that the opacity and hydrophilicity of the fabric can be enhanced.