Patent classifications
D21H11/14
METHOD FOR SPRAYING CHEMICAL SOLUTION
A chemical solution spraying method for spraying a chemical solution onto a canvas K1 has a loop shape in a side view while reciprocating two nozzle devices S at the same speed along rail L extending in a width direction of canvas K1 with respect to canvas K1, in which time period Tc during which canvas K1 is in contact with wet paper X is 0.03 seconds or more, time period Tn required for nozzle devices S to each one-way move is 0.5 to 10 minutes, traveling speed Vp of canvas K1 is 500 m/min or more, length K of canvas K1 is 20 to 80 m, a number of times of contact N of any point on a surface of canvas K1 with wet paper X during time period Tn, time period Tn, traveling speed Vp, and length K satisfy a relationship of N=(Tn.Math.Vp)/K, under predetermined conditions.
METHOD FOR SPRAYING CHEMICAL SOLUTION
A chemical solution spraying method for spraying a chemical solution onto a canvas K1 has a loop shape in a side view while reciprocating two nozzle devices S at the same speed along rail L extending in a width direction of canvas K1 with respect to canvas K1, in which time period Tc during which canvas K1 is in contact with wet paper X is 0.03 seconds or more, time period Tn required for nozzle devices S to each one-way move is 0.5 to 10 minutes, traveling speed Vp of canvas K1 is 500 m/min or more, length K of canvas K1 is 20 to 80 m, a number of times of contact N of any point on a surface of canvas K1 with wet paper X during time period Tn, time period Tn, traveling speed Vp, and length K satisfy a relationship of N=(Tn.Math.Vp)/K, under predetermined conditions.
BARRIER RECYCLED PAPERBOARD AND METHOD FOR MANUFACTURING THEREOF
A coated paperboard includes a recycled paperboard substrate having a first side and a second side, a first aqueous barrier coating applied over the first side, and a second aqueous barrier coating applied over the first aqueous barrier coating. The first aqueous barrier coating is formed from a mixture of binder and pigment. The second aqueous barrier coating is formed from a mixture of binder and pigment.
BARRIER RECYCLED PAPERBOARD AND METHOD FOR MANUFACTURING THEREOF
A coated paperboard includes a recycled paperboard substrate having a first side and a second side, a first aqueous barrier coating applied over the first side, and a second aqueous barrier coating applied over the first aqueous barrier coating. The first aqueous barrier coating is formed from a mixture of binder and pigment. The second aqueous barrier coating is formed from a mixture of binder and pigment.
MOISTURE RESISTANT BIODEGRADABLE COMPOSITION
A biodegradable composition having resistance to moisture and organic waste is provided.
MOISTURE RESISTANT BIODEGRADABLE COMPOSITION
A biodegradable composition having resistance to moisture and organic waste is provided.
High Efficiency Fiber Bleaching Process
A high efficiency bleaching method for cellulosic pulp includes: (a) providing a charge of aqueous cellulosic pulp to a bleaching vessel at a consistency of from 10% to 30% along with a peroxy bleaching agent and an alkaline agent effective to adjust pH of the charge to 9.5 to 12.5; and (b) bleaching the aqueous cellulosic pulp in the bleaching vessel while maintaining a bleaching temperature of from 110° F. (43° C.) to 135° F. (57° C.) and a pH of the charge from 9.5 to 12.5 for an extended bleaching retention time. The bleaching method is advantageously used to bleach low brightness recycle pulp, and/or as part of a multistage process with bleaching stages of lesser duration, and/or as a high peroxy efficiency, low dose bleaching process or in connection with concurrently storing and bleaching pulp.
High Efficiency Fiber Bleaching Process
A high efficiency bleaching method for cellulosic pulp includes: (a) providing a charge of aqueous cellulosic pulp to a bleaching vessel at a consistency of from 10% to 30% along with a peroxy bleaching agent and an alkaline agent effective to adjust pH of the charge to 9.5 to 12.5; and (b) bleaching the aqueous cellulosic pulp in the bleaching vessel while maintaining a bleaching temperature of from 110° F. (43° C.) to 135° F. (57° C.) and a pH of the charge from 9.5 to 12.5 for an extended bleaching retention time. The bleaching method is advantageously used to bleach low brightness recycle pulp, and/or as part of a multistage process with bleaching stages of lesser duration, and/or as a high peroxy efficiency, low dose bleaching process or in connection with concurrently storing and bleaching pulp.
METHOD FOR THE PRODUCTION OF PAPER PRODUCTS
A method for the production of paper products, such as paper and cardboard, by recycling cellulose-based raw materials containing starch. The method includes the steps of pulping in water cellulose-based raw materials containing starch, particularly recycled paper products, obtaining a pulped mass; adding to the pulped mass of the previous step under agitation a mineral acid in a quantity that is suitable to obtain a pH of the pulped mass not lower than 4, and obtaining a pulped mass treated with acid. The method further includes the step of subjecting the pulped mass treated with acid obtained in the second step, optionally treated with other chemical additives, in succession, to filtration, pressing and drying, and obtaining a paper product. Paper products obtainable by this method are also related.
FAN-FOLDED PAPER WEB STACK
In a zig-zag folded stack of paper web, particularly a stack of recycling paper web, wherein at least one fold of the zag folded stack of paper web is provided with a perforation-tie-row, wherein the ties of the fold coupled to folding-web-she folded above one another, wherein the fold tie in the perforation, each, comprise a maximal longitudinal direction [respective] in the longitudinal fold direction, it is provided that at least one section of a fold comprises a perforation-fold-row of at least five alternatingly arranged ties and perforations, wherein a ratio of a summed up combined longitudinal extension of the folding ties within the section in relation to a summed up combined longitudinal extension of the perforations of the same number within the folding section is larger than or equal to 0.8, preferably larger than or equal to 1.