Patent classifications
D21H21/50
DRY POLYMER APPLICATION METHOD
A method of incorporating a low molecular weight polymer (e.g., polymer strength aid) into an industrial process (e.g., papermaking process) is provided. The method comprises treating an industrial process (e.g., paper sheet precursor) with a powder or wetted powder, wherein the powder comprises a polymer dry polymer (e.g., polymer strength aid), wherein the polymer dry polymer (e.g., polymer strength aid) has a weight average molecular weight of from about 10 kDa to about 2,000 kDa.
RECORDING MEDIUM MANUFACTURING APPARATUS
A recording medium manufacturing apparatus includes at least one material supplying section which includes a storage unit which stores a fiber-containing material containing cellulose fibers and a resin, at least one carrying body which carries the fiber-containing material which is supplied from the material supplying section, a transfer-target body onto which the fiber-containing material which is carried by the carrying body is electrostatically transferred, and an after-treatment unit which performs an after-treatment on the fiber-containing material which is electrostatically transferred onto the transfer-target body.
Coating composition and coated paper and coated paperboard
A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate, wherein less than about 90% by weight and greater than about 60% by weight of particles of the calcium carbonate have an equivalent spherical diameter (esd) less than 2 microns. The coating composition may include a thickener present in an amount ranging from about 0.1% to about 0.9% by active dry weight of the composition. A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate having a mean particle size (d50) of at least about 2.4 microns and a steepness factor of at least about 30. The coating composition may be a paper basecoat composition or a paperboard basecoat composition. A paper or paperboard product may include the coating composition on at least one surface of the paper product or paperboard product.
Coating composition and coated paper and coated paperboard
A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate, wherein less than about 90% by weight and greater than about 60% by weight of particles of the calcium carbonate have an equivalent spherical diameter (esd) less than 2 microns. The coating composition may include a thickener present in an amount ranging from about 0.1% to about 0.9% by active dry weight of the composition. A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate having a mean particle size (d50) of at least about 2.4 microns and a steepness factor of at least about 30. The coating composition may be a paper basecoat composition or a paperboard basecoat composition. A paper or paperboard product may include the coating composition on at least one surface of the paper product or paperboard product.
FIBROUS STRUCTURE CONTAINING ARTICLES
Articles, such as sanitary tissue products, including fibrous structures, and more particularly articles including fibrous structures having a plurality of fibrous elements wherein the article exhibits differential cellulose content throughout the thickness of the article and methods for making same are provided.
FIBROUS STRUCTURE CONTAINING ARTICLES
Articles, such as sanitary tissue products, including fibrous structures, and more particularly articles including fibrous structures having a plurality of fibrous elements wherein the article exhibits differential cellulose content throughout the thickness of the article and methods for making same are provided.
Coating composition and coated paper and coated paperboard
A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate, wherein less than about 90% by weight and greater than about 60% by weight of particles of the calcium carbonate have an equivalent spherical diameter (esd) less than 2 microns. The coating composition may include a thickener present in an amount ranging from about 0.1% to about 0.9% by active dry weight of the composition. A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate having a mean particle size (d.sub.50) of at least about 2.4 microns and a steepness factor of at least about 30. The coating composition may be a paper basecoat composition or a paperboard basecoat composition. A paper or paperboard product may include the coating composition on at least one surface of the paper product or paperboard product.
Coating composition and coated paper and coated paperboard
A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate, wherein less than about 90% by weight and greater than about 60% by weight of particles of the calcium carbonate have an equivalent spherical diameter (esd) less than 2 microns. The coating composition may include a thickener present in an amount ranging from about 0.1% to about 0.9% by active dry weight of the composition. A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate having a mean particle size (d.sub.50) of at least about 2.4 microns and a steepness factor of at least about 30. The coating composition may be a paper basecoat composition or a paperboard basecoat composition. A paper or paperboard product may include the coating composition on at least one surface of the paper product or paperboard product.
COATING COMPOSITION AND COATED PAPER AND COATED PAPERBOARD
A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate, wherein less than about 90% by weight and greater than about 60% by weight of particles of the calcium carbonate have an equivalent spherical diameter (esd) less than 2 microns. The coating composition may include a thickener present in an amount ranging from about 0.1% to about 0.9% by active dry weight of the composition. A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate having a mean particle size (d50) of at least about 2.4 microns and a steepness factor of at least about 30. The coating composition may be a paper basecoat composition or a paperboard basecoat composition. A paper or paperboard product may include the coating composition on at least one surface of the paper product or paperboard product.
COATING COMPOSITION AND COATED PAPER AND COATED PAPERBOARD
A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate, wherein less than about 90% by weight and greater than about 60% by weight of particles of the calcium carbonate have an equivalent spherical diameter (esd) less than 2 microns. The coating composition may include a thickener present in an amount ranging from about 0.1% to about 0.9% by active dry weight of the composition. A coating composition may include kaolin having a shape factor less than about 70 and calcium carbonate having a mean particle size (d50) of at least about 2.4 microns and a steepness factor of at least about 30. The coating composition may be a paper basecoat composition or a paperboard basecoat composition. A paper or paperboard product may include the coating composition on at least one surface of the paper product or paperboard product.