D21H11/18
WIPING SHEET AND METHOD FOR MANUFACTURING WIPING SHEET
A wiping sheet includes a patterned part of a fiber assembling base material and a non-patterned part of the fiber assembling base material. The patterned part includes cellulose nanofiber; and the non-patterned part does not include the cellulose nanofiber.
Cellulose Microfiber-Reinforced Polyamide Resin Molded Article
Provided is a polyamide resin molded article having high mechanical properties and dimensional accuracy as well as low friction coefficient, low wear, and/or low abrasion property. The present invention provides a polyamide resin molded article composed of a polyamide resin composition including (A) a polyamide resin, (B) chemically modified cellulose microfibers having a weight average molecular weight (Mw) of 100,000 or more, a ratio (Mw/Mn) of the weight average molecular weight (Mw) and the number average molecular weight (Mn) of 6 or less, an alkali-soluble polysaccharides average content of 12 mass percent or less, and a degree of crystallization of 60% or more, and (C) a dispersant having a melting point of 80° C. or less and a number average molecular weight of 1000-50,000, wherein the melting point (Tm) and the crystallization temperature (Tc) of the polyamide resin molded article satisfy formula (1): Tm−Tc≥30° C. . . . (1).
ARTICLES OF MANUFACTURE COMPRISING NANOCELLULOSE ELEMENTS
The present invention provides formulations comprising a suspension of nanocellulose (NC) elements and a drying/dispersal additive selected from the group consisting of temperature-responsive polymers, small molecule additives in volatile systems, and blocking agents and methods of preparing such formulations, and further provides NC-containing materials, composite materials and useful articles of manufacture made therefrom.
Composition of matter in a pre-refiner blend zone
A composition is contained a blend zone prior to refining containing non-fibrillated virgin cellulose fibers, waste/recycle cellulose fibers or both; cellulose ester fibers, water, and one or more additives comprising fillers, internal sizing agents, biocides, process anti-foaming agents, colorants, optical modifiers, or a combination thereof. An in-line mixer can be used for adding the additives, and the consistency of the composition is lowered relative to a feed of material from a hydropulper.
SULFONATED PULP FIBERS, DERIVATIVE PULP, SULFONATED FINE CELLULOSE FIBERS, METHOD FOR PRODUCING SULFONATED FINE CELLULOSE FIBERS, AND METHOD FOR PRODUCING SULFONATED PULP FIBERS
[Object] An object is to provide a sulfonated fine cellulose fiber having excellent transparency a sulfonated pulp fiber suitable for the sulfonated fine cellulose fiber, a method for producing these fibers, and a derivative pulp containing the sulfonated pulp fiber.
[Means for achieving the object] The sulfonated pulp fiber of the present invention is a pulp fiber comprising a plurality of cellulose fibers, wherein a part of hydroxyl groups of the cellulose fibers of the pulp fiber is substituted with sulfo groups, an introduction amount of sulfur attributable to the sulfo groups is adjusted to be higher than 0.42 mmol/g while maintaining a fiber shape, and a water retention value of the pulp fiber is adjusted to 150% or more. Since the sulfonated pulp fiber has a predetermined water retaining property or more while maintaining the fiber shape, the degree of flexibility in handling can be improved.
Pulp Treating Apparatus and Method
A pulp treating arrangement (10) has a pulp treating apparatus (100), which receives a first pulp (150) which including at least one of virgin pulp (152) and recycled pulp (154). The arrangement performs a processing of fines of the first pulp (150), and outputs a second pulp (160) having a modified percentage of fines on the basis of the processing and provides a micro-/nanocellulose process arrangement (104) with the second pulp (160).
Pulp Treating Apparatus and Method
A pulp treating arrangement (10) has a pulp treating apparatus (100), which receives a first pulp (150) which including at least one of virgin pulp (152) and recycled pulp (154). The arrangement performs a processing of fines of the first pulp (150), and outputs a second pulp (160) having a modified percentage of fines on the basis of the processing and provides a micro-/nanocellulose process arrangement (104) with the second pulp (160).
Method of manufacturing cellulose nanofiber compact
A method of manufacturing a cellulose nanofiber compact includes a supporting step of supporting a plate-like first precursor containing cellulose nanofibers in a heating vessel, a preliminary molding step of heating the first precursor supported in the heating vessel with infrared rays to obtain a plate-like second precursor and a molding step of molding the second precursor, with heating and pressurizing the second precursor in a mold.
Method of manufacturing cellulose nanofiber compact
A method of manufacturing a cellulose nanofiber compact includes a supporting step of supporting a plate-like first precursor containing cellulose nanofibers in a heating vessel, a preliminary molding step of heating the first precursor supported in the heating vessel with infrared rays to obtain a plate-like second precursor and a molding step of molding the second precursor, with heating and pressurizing the second precursor in a mold.
MICROFIBRILLATED CELLULOSE-LOADED FOAM, METHOD OF PRODUCING SUCH FOAM AND USE OF SUCH A FOAM
A microfibrillated cellulose-loaded foam is indicated, comprising microfibrillated cellulose, at least one thickening agent and/or at least one adhesive biopolymer. Furthermore, a method for producing such a microfibrillated cellulose-loaded foam and a use of such a foam are provided.