D06M13/292
TREATMENT AGENT FOR ELASTIC FIBERS, AND ELASTIC FIBER
Disclosed is an elastic fiber treatment agent that contains a smoothing agent and an alkyl phosphate ester compound. The alkyl phosphate ester compound contains specific phosphate ester Q1 and at least one or more selected from specific phosphate esters Q2 and Q3. In a P nucleus NMR measurement of the alkyl phosphate ester compound upon an alkali over-neutralization pretreatment, a P nucleus NMR integral ratio attributed to the phosphate ester Q1 is 15% to 60% if the sum of P nucleus NMR integral ratios attributed to the phosphate esters Q1 to Q3 and phosphoric acid and its salt is taken as 100%.
TREATMENT AGENT FOR ELASTIC FIBERS, AND ELASTIC FIBER
Disclosed is an elastic fiber treatment agent that contains a smoothing agent and an alkyl phosphate ester compound. The alkyl phosphate ester compound contains specific phosphate ester Q1 and at least one or more selected from specific phosphate esters Q2 and Q3. In a P nucleus NMR measurement of the alkyl phosphate ester compound upon an alkali over-neutralization pretreatment, a P nucleus NMR integral ratio attributed to the phosphate ester Q1 is 15% to 60% if the sum of P nucleus NMR integral ratios attributed to the phosphate esters Q1 to Q3 and phosphoric acid and its salt is taken as 100%.
ELASTIC FIBER TREATING AGENT AND ELASTIC FIBERS
An elastic fiber treatment agent that contains a smoothing agent, water and an organic phosphoric acid ester salt. The smoothing agent contains a mineral oil with an aniline point of not more than 110° C., a silicone oil, and optionally an ester oil. Assuming that the sum of the content ratios of the smoothing agent, the water, and the organic phosphoric acid ester salt in the elastic fiber treatment agent is 100 parts by mass, the elastic fiber treatment agent contains the mineral oil at a ratio of 20 to 90 parts by mass and the water at a ratio of 0.01 to 2 parts by mass.
ELASTIC FIBER TREATING AGENT AND ELASTIC FIBERS
An elastic fiber treatment agent that contains a smoothing agent, water and an organic phosphoric acid ester salt. The smoothing agent contains a mineral oil with an aniline point of not more than 110° C., a silicone oil, and optionally an ester oil. Assuming that the sum of the content ratios of the smoothing agent, the water, and the organic phosphoric acid ester salt in the elastic fiber treatment agent is 100 parts by mass, the elastic fiber treatment agent contains the mineral oil at a ratio of 20 to 90 parts by mass and the water at a ratio of 0.01 to 2 parts by mass.
Durable Thermoregulating Textile Structures and Methods of Manufacture
A textile structure including one or more layers of warp yarns interwoven with one or more layers of weft yarns, a durable thermoregulating coating, and a binder that chemically bonds the durable thermoregulating coating to the textile structure. The warp yarns and/or weft yarns include polyester yarns. A method for manufacturing a textile structure includes weaving one or more layers of warp yarns with one or more layers or weft yarns to form a woven textile structure, brushing the textile structure at least two times, applying a binder to the textile structure, and applying a durable thermoregulating coating to the textile structure such that the binder chemically bonds the durable thermoregulating coating to the textile structure. The method may also include heat setting and curing the textile structure to fix the durable thermoregulating coating permanently onto the textile structure.
ELASTIC FIBER PROCESSING AGENT AND ELASTIC FIBER
An elastic fiber treatment agent that contains, as a smoothing agent, a mineral oil with a content ratio of an aromatic component of less than 1% by mass and an aniline point of 70° C. to 110° C. The mineral oil has a mass ratio between the content of a naphthene component and the content of a paraffin component of such that naphthene component/paraffin component=30 to 50/70 to 50.
ELASTIC FIBER PROCESSING AGENT AND ELASTIC FIBER
An elastic fiber treatment agent that contains, as a smoothing agent, a mineral oil with a content ratio of an aromatic component of less than 1% by mass and an aniline point of 70° C. to 110° C. The mineral oil has a mass ratio between the content of a naphthene component and the content of a paraffin component of such that naphthene component/paraffin component=30 to 50/70 to 50.
Wettable SMS material for personal protective equipment applications
A wettable SMS material for personal protective equipment, such as a SMS fabric that has been treated to improve the wettability and absorbency properties of the SMS fabric is provided. A treated SMS fabric for personal protective equipment can retain its durability, breathability, and comfort, and may also provide the fabric with wettability and absorption properties. An article for personal protective equipment formed from a wettable SMS fabric is also provided.
Wettable SMS material for personal protective equipment applications
A wettable SMS material for personal protective equipment, such as a SMS fabric that has been treated to improve the wettability and absorbency properties of the SMS fabric is provided. A treated SMS fabric for personal protective equipment can retain its durability, breathability, and comfort, and may also provide the fabric with wettability and absorption properties. An article for personal protective equipment formed from a wettable SMS fabric is also provided.
COMPOSITIONS AND METHODS FOR THERMAL MANAGEMENT OF TEXTILES AND FOAMS
Described herein are compositions that include microencapsulated phase change materials and thermal conductivity additives and methods for applying the compositions to substrates, including fibers, textile, and foams, to impart beneficial thermal management properties to the substrates. The treated substrates feel cool to the touch for an extended period of time.