Patent classifications
D07B2201/2082
METHOD FOR MANUFACTURING AN INDIVIDUALLY SHEATHED STRAND, STRAND THUS OBTAINED AND STRAND MANUFACTURING INSTALLATION
The method for manufacturing an individually sheathed strand comprises: conveying a group of metal wires through a die; upstream of the die, applying a first filler product to at least a first portion of the strand; upstream of the die, applying a second filler product to at least a second portion of the strand distinct from the first portion; and extruding a plastic around the group of metal wires passing through the die, so as to envelop the group of metal wires covered with the first and second filler products in a continuous sheath formed of the extruded plastic. The second filler product has greater adhesion to the group of metal wires than the first filler product.
SELF HEALING ELEVATOR LOAD BEARING MEMBER
An elevator load bearing member includes a plurality of load bearing cords and a jacket at least partially surrounding the cords. The jacket includes a layer received against the cords, and a self-healing component. A method of making an elevator load bearing member is also disclosed.
TIRE
Provided is a tire in which a steel cord applied to a carcass ply has improved corrosion resistance to water penetration, fretting resistance, and cord untwisting resistance. Provided is a tire including a carcass ply (1) as a skeleton, the carcass ply is reinforced by a steel cord including no wrapping filament. The steel cord is composed of a plurality of steel filaments having 3 or more core filaments, at least a part of the surface of each of the plurality of steel filaments is coated with a resin material containing at least an ionomer, and when a resin component contained in the resin material is composed of a single resin, the melting point of the resin material is 150 C. or less, and when the resin component is composed of a composition containing two or more resins, the softening point of the resin material is 150 C. or less.
Method for Producing a Tension Member, Tension Member, and Use Thereof
The invention relates to a method for filling in a tension member in particular for conveyor belts, in particular a tension member which is configured as a steel cable. The method is intended to allow the full penetration of the tension member structure. Here, the method contains at least the following method steps: introducing the individual wires (2, 2, 2, 2, 2) of the strand (5) into the stranding head (1) of a stranding machine (10) and partially or fully applying at least one coating agent to at least 50% of the individual wires (2, 2, 2, 2, 2) of the strand (5) prior to the twisting of the individual wires (2, 2, 2, 2, 2) to form a strand (5) or simultaneously with the twisting of the individual wires (2, 2, 2, 2, 2) to form a strand (5) and twisting the individual wires (2, 2, 2, 2, 2) to form a strand (5), wherein at least 50% of the individual wires (2, 2, 2, 2, 2) have been provided with at least one coating agent, and making a cable from at least one strand (5).
Cable rubberized in situ comprising a rubberizing composition comprising a corrosion inhibitor
A cord rubberized in situ (C) comprising: an internal layer of the cord (CT1), an external layer of the cord (CT3), a rubber composition (20) positioned between the internal layer of the cord and the external layer of the cord. The rubber composition (20) comprises a compound of formula (I): ##STR00001##
in which X and Y represent, independently of each other, an alkali metal or alkaline earth metal cation.
HIGH-STRENGTH FIBER COMPOSITE CABLE
A high-strength fiber bundle sufficiently impregnated with a thermoplastic resin, without impairing mechanical strength. A high-strength fiber composite cable is produced by impregnating a bundle of carbon fibers with a matrix resin. The matrix resin is obtained by mixing, with a thermoplastic resin, such as polyphenylene sulfide, an oligomer having a weight-average molecular weight of less than 10,000, obtained by causing a reaction between an organic compound having a phenolic hydroxyl group and an organic compound having a glycidyl ether group. The matrix resin, which has a viscosity low in comparison with that of the thermoplastic resin serving as a base material, readily impregnates the bundle of carbon fibers with certainty.
Method for producing a tension member, tension member, and use thereof
The invention relates to a method for filling in a tension member in particular for conveyor belts, in particular a tension member which is configured as a steel cable. The method is intended to allow the full penetration of the tension member structure. Here, the method contains at least the following method steps: introducing the individual wires (2, 2, 2, 2, 2) of the strand (5) into the stranding head (1) of a stranding machine (10) andpartially or fully applying at least one coating agent to at least 50% of the individual wires (2, 2, 2, 2, 2) of the strand (5) prior to the twisting of the individual wires (2, 2, 2, 2, 2) to form a strand (5) or simultaneously with the twisting of the individual wires (2, 2, 2, 2, 2) to form a strand (5) andtwisting the individual wires (2, 2, 2, 2, 2) to form a strand (5), wherein at least 50% of the individual wires (2, 2, 2, 2, 2) have been provided with at least one coating agent, andmaking a cable from at least one strand (5).
HYBRID COMPENSATION MEMBER
A compensation and tie-down member for an elevator system includes one or more lightweight compensation tension elements having a first tensile strength/unit mass/unit length, and one or more heavier weight compensation tension elements having a second tensile strength/unit mass/unit length less than the first tensile strength/unit mass/unit length.
METHOD FOR MANUFACTURING TIRE
Provided is a method for manufacturing a tire using a steel cord which can be manufactured without reducing productivity and can prevent propagation of moisture inside. The method for manufacturing a tire includes a vulcanization step of vulcanizing a green tire provided with a belt having at least one belt layer, in which the belt layer includes a steel cord 10 formed by twisting a steel filament 2 together with a resin filament 1 having a softening point of 125 C. or lower, and the resin filament 1 includes at least an ionomer.
Cable and method for manufacturing cable
In a method for manufacturing a cable, a filling step S5 of filling a tube hole of a socket main body which is formed in a tubular shape and in which first end portions of wire rods are disposed with a mixture obtained by mixing a thermosetting resin into a preliminary mixture obtained by mixing ceramic particles and fly ash in advance is carried out.