D07B2207/4059
CORD FOR ELASTOMER REINFORCEMENT USE
Provided is an elastomer reinforcement cord with improved rust inhibition. An elastomer reinforcement cord (10) includes metal filaments and a polymer material. The elastomer reinforcement cord (10) has a multi-strand structure which includes: at least one core strand (21) formed by twisting plural metal filaments (1a) and (1b) together; and two or more sheath strands (22) each formed by twisting plural metal filaments (11a) and (11b) together, and in which the sheath strands are twisted together around the core strand. In a region surrounded by a line connecting the centers of the metal filaments constituting the outermost sheath layer of the core strand at a cross-section in a direction orthogonal to an axial direction after vulcanization of the core strand, when a region occupied by other than the metal filaments is defined as a gap region, a filling rate, which is a ratio of the area of the polymer material with respect to the gap region, is 52% to 120%.
CORD FOR ELASTOMER REINFORCEMENT USE
Provided is an elastomer reinforcement cord with improved rust inhibition. An elastomer reinforcement cord (10) includes metal filaments and a polymer material. The elastomer reinforcement cord (10) has a multi-strand structure which includes: at least one core strand (21) formed by twisting plural metal filaments (1a) and (1b) together; and two or more sheath strands (22) each formed by twisting plural metal filaments (11a) and (11b) together, and in which the sheath strands are twisted together around the core strand. In a region surrounded by a line connecting the centers of the metal filaments constituting the outermost sheath layer of the core strand at a cross-section in a direction orthogonal to an axial direction after vulcanization of the core strand, when a region occupied by other than the metal filaments is defined as a gap region, a filling rate, which is a ratio of the area of the polymer material with respect to the gap region, is 52% to 120%.
ELASTOMER REINFORCEMENT CORD
Provided is an elastomer reinforcement cord in which the problem of stress concentration at an interface between an elastomer and a metal cord is solved and the durability is thereby improved. The elastomer reinforcement cord includes metal filaments (1a) and (1b), and a polymer material (3) having a melting point or softening point of 80° C. to 160° C. The elastomer reinforcement cord has a core (11) and at least one sheath layer (12). In a region surrounded by a line connecting the centers of the metal filaments constituting the outermost sheath layer at a cross-section in a direction orthogonal to an axial direction after vulcanization, when a region occupied by other than the metal filaments is defined as a gap region, the polymer material is contained in this gap region, and a filling rate, which is a ratio of the area of the polymer material, is higher than 120%, taking the area of the gap region as 100%.
ELASTOMER REINFORCEMENT CORD
Provided is an elastomer reinforcement cord in which the problem of stress concentration at an interface between an elastomer and a metal cord is solved and the durability is thereby improved. The elastomer reinforcement cord includes metal filaments (1a) and (1b), and a polymer material (3) having a melting point or softening point of 80° C. to 160° C. The elastomer reinforcement cord has a core (11) and at least one sheath layer (12). In a region surrounded by a line connecting the centers of the metal filaments constituting the outermost sheath layer at a cross-section in a direction orthogonal to an axial direction after vulcanization, when a region occupied by other than the metal filaments is defined as a gap region, the polymer material is contained in this gap region, and a filling rate, which is a ratio of the area of the polymer material, is higher than 120%, taking the area of the gap region as 100%.
ELASTOMER REINFORCEMENT CORD
Provided is an elastomer reinforcement cord with improved rust resistance. An elastomer reinforcement cord 10 includes metal filaments and a polymer material. The elastomer reinforcement cord 10 has a multi-strand structure which includes: at least one core strand 21 formed by twisting plural metal filaments 1a and 1b together; and two or more sheath strands 22 each formed by twisting plural metal filaments 11a and 11b together, the sheath strands being twisted together around the core strand. An intra-sheath-strand filling rate a, which is a ratio of the area of the polymer material with respect to an intra-sheath-strand gap region A, is 52% or higher, and an inter-strand filling rate b, which is a ratio of the area of the polymer material with respect to an inter-strand gap region B, is 75% or higher.
ELASTOMER REINFORCEMENT CORD
Provided is an elastomer reinforcement cord with improved rust resistance. An elastomer reinforcement cord 10 includes metal filaments and a polymer material. The elastomer reinforcement cord 10 has a multi-strand structure which includes: at least one core strand 21 formed by twisting plural metal filaments 1a and 1b together; and two or more sheath strands 22 each formed by twisting plural metal filaments 11a and 11b together, the sheath strands being twisted together around the core strand. An intra-sheath-strand filling rate a, which is a ratio of the area of the polymer material with respect to an intra-sheath-strand gap region A, is 52% or higher, and an inter-strand filling rate b, which is a ratio of the area of the polymer material with respect to an inter-strand gap region B, is 75% or higher.
HIGH STRENGTH DATA TRANSMISSION CABLE
Disclosed is a non-steel high strength data transmission cable having a strength member (5) and a core (1). The high strength data transmission cable includes a length of a core-cable (10), the length of core-cable (10) includes core (1) plus at least. one. fiber-optic conductor (2) that is: (i) disposed in a helical shape; and (ii) completely encased in a solid, flexible material.
Also disclosed is a process for making a high strength data transmission cable. The high strength data transmission cable is capable of being wound on a winch under tensions and surging shocks experienced by a fishing trawler, and provides high quality data signal transmission and resolution so as to permit use for transmitting data during fish trawl operation from high-resolution sonars used to monitor fish caught.
IMPROVED HIGH RESOLUTION HEADLINE SONAR CABLE
Disclosed is a non-steel headline sonar cable having a strength member [5] and a core [1], the headline sonar cable comprising a length of a core-cable [10], the length of core-cable (10] comprising core [1] as well as comprising at least one fiber-optic conductor [2] that is: [i] disposed in a helical shape; and [ii] completely encased in a solid, flexible material. Also disclosed is a process for making a headline sonar cable. The headline sonar cable is capable of being wound on a winch under tensions and surging shocks experienced by a fishing trawler and provides high quality data signal transmission and resolution so as to permit use for transmitting data from high resolution sonars used to monitor fish caught in a fish trawl during operation.
Tire
Provided is a tire in which a steel cord applied to a carcass ply has improved corrosion resistance to water penetration, fretting resistance, and cord untwisting resistance. Provided is a tire including a carcass ply (1) as a skeleton. The carcass ply is reinforced by a steel cord including no wrapping filament. The steel cord is composed of a plurality of steel filaments having 3 or more core filaments, at least a part of the surface of each of the plurality of steel filaments is coated with a resin material containing at least an ionomer, and when a resin component contained in the resin material is composed of a single resin, the melting point of the resin material is 150° C. or less, and when the resin component is composed of a composition containing two or more resins, the softening point of the resin material is 150° C. or less.
Tire
Provided is a tire in which a steel cord applied to a carcass ply has improved corrosion resistance to water penetration, fretting resistance, and cord untwisting resistance. Provided is a tire including a carcass ply (1) as a skeleton. The carcass ply is reinforced by a steel cord including no wrapping filament. The steel cord is composed of a plurality of steel filaments having 3 or more core filaments, at least a part of the surface of each of the plurality of steel filaments is coated with a resin material containing at least an ionomer, and when a resin component contained in the resin material is composed of a single resin, the melting point of the resin material is 150° C. or less, and when the resin component is composed of a composition containing two or more resins, the softening point of the resin material is 150° C. or less.