Patent classifications
E01C7/185
VOID REDUCING ASPHALT MEMBRANE COMPOSITION, METHOD AND APPARATUS FOR ASPHALT PAVING APPLICATIONS
A method of forming a pavement construction joint that involves dispensing a band of a void reducing joint composition on a substrate using at least one spray application vehicle, wherein the band comprises a width of about 4 to about 24 inches. A paving pass is applied over the band of joint composition, wherein the paving pass is positioned against an edge of a previously laid portion of pavement to form a pavement construction joint having a volume of air voids. At least a portion of the joint composition migrates upward to reduce the volume of air voids. The composition is resistant to flow when applied and migrates into hot mix asphalt in the area of the longitudinal joint to reduce air voids to 7% or less and reduce water permeability. The composition becomes tack-free quickly after application. The composition bonds to asphalt, concrete, brick, stone and metal.
Hot applied tack coat
A method of applying building a pavement structure using a polymer modified hot-applied tack coat is disclosed. This polymer modified tack coat is non-adhesive at ambient temperatures, and, thus, also non tracking. The tack is applied while hot, but cools quickly. The subsequent application of hot mix asphalt results in a superior bond between the asphalt layer and the tack layer. It is particularly well suited to bonded friction course applications since it removes the necessity of specialized spray paving machinery and allows the use of conventional asphalt distributors and pavers.
Concrete based reinforced road structure covered by asphalt
Concrete based reinforced road structure covered by asphalt that comprises a basic layer (1) made of concrete with a substantially horizontal upper surface and placed directly or through a subconstruction on the ground and at least one mould cover layer (2) thereon made of asphalt, and support elements (3) positioned between the basic layer (1) and the cover layer (2), wherein the support elements (3) are inserted in a predetermined depth in the basic layer (1) prior to the setting thereof so that they are partially projecting out of the basic layer (1) in normal direction to the upper surface, and the projecting portion provides protection to the cover layer (2) against being displaced relative to the basic layer (1) under loads to which the road is exposed, and the support elements (3) are flat stripes with walls being substantially normal to the surface of the basic layer (1) and comprising subsequent sections with differing directions to form respective meandering lines.
LOW RESIDUAL SPRAY PAVING COATING AND METHOD
A paving mixture for application to a surface and a method for the same are provided. The mixture comprises a binding material layer applied to the surface to form a base layer on the surface, and an aggregate material layer applied on top of the binding material layer. The binding material layer can be applied in an amount of at most 0.125 gallons/yd.sup.2. The aggregate material layer contains an asphalt mixture that provides a road surface. The aggregate material layer and the binding material layer can be combined on the surface within 30 seconds of application of the binding material layer. Additionally, multiple paving mixtures may be applied to the surface.
CONSTRUCTION REINFORCEMENT WITH PROTRUDING REINFORCEMENTS
A fabric (10, 20, 30) adapted for the reinforcement of constructions such as of roads or pavements has a fabric width W2 in a transverse direction. The fabric (10, 20, 30) comprises a carrier (12, 22, 32). The fabric further comprises reinforcement elements (14, 24, 24, 34) extending over the fabric width and being fixed or bound to the carrier (12, 22, 32). The carrier (12, 22, 32) has a carrier width W1 that is smaller than the fabric width W2 so that the reinforcement elements (14, 24, 24, 34) protrude out of the carrier (12, 22, 32). The advantage is that when two neighbouring fabrics (40, 44) overlap, it is possible to avoid a double layer of carriers.
Binder composition for improved tack coat and stress absorbing membrane interlayer application for road construction
A method of installing an asphalt pavement, which method involves: identifying a surface to be paved; applying a non-tracking layer of binder composition to the surface; and permitting the application of an asphalt layer over the non-tracking layer of binder composition. The binder composition consists essentially of: at least one asphalt binder; at least one elastomer; and ethylene bis stearamide. In a further embodiment the binder composition consists essentially of: at least one asphalt binder; at least one elastomer; sulfur; and ethylene bis stearamide. The composition is applied as a tack coat and/or a stress absorbing membrane interlayer and is non-tracking.
Void reducing asphalt membrane composition, method and apparatus for asphalt paving applications
A void reducing asphalt membrane composition for asphalt pavements that includes: an asphalt binder; an elastomeric polymer; a wax modifier; and at least one of: i) fumed silica or fumed alumina; and ii) a saponified fatty acid and a resin acid gelling compound. The composition is resistant to flow when applied and migrates into hot mix asphalt in the area of the longitudinal joint to reduce air voids to 7% or less and reduce water permeability. The composition becomes tack-free quickly after application. The composition bonds to asphalt, concrete, brick, stone and metal.
VOID REDUCING ASPHALT MEMBRANE COMPOSITION, METHOD AND APPARATUS FOR ASPHALT PAVING APPLICATIONS
A method of forming a pavement construction joint that involves dispensing a band of a void reducing joint composition on a substrate using at least one spray application vehicle, wherein the band comprises a width of about 4 to about 24 inches. A paving pass is applied over the band of joint composition, wherein the paving pass is positioned against an edge of a previously laid portion of pavement to form a pavement construction joint having a volume of air voids. At least a portion of the joint composition migrates upward to reduce the volume of air voids. The composition is resistant to flow when applied and migrates into hot mix asphalt in the area of the longitudinal joint to reduce air voids to 7% or less and reduce water permeability. The composition becomes tack-free quickly after application. The composition bonds to asphalt, concrete, brick, stone and metal.
Void reducing asphalt membrane composition, method and apparatus for asphalt paving applications
A roadway structure that includes: a substrate; a hot mix application portion positioned over the substrate, wherein said hot mix application portion comprises first and second adjacent paving passes defining a longitudinal joint, and wherein the first and second adjacent paving passes contain air voids along the longitudinal joint; and a spray-applied band of void reducing joint composition positioned between the substrate and the hot mix application portion, wherein the band is below the longitudinal joint, and wherein at least at portion of the void reducing joint composition fills at least some of the air voids.