G02B1/043

OPHTHALMIC DEVICES

An ophthalmic device for slowing, inhibiting or preventing myopia progression which is a polymerization product of a monomeric mixture comprising (a) greater than 50 wt. %, based on the total weight of the monomeric mixture, of one or more non-silicone-containing hydrophilic monomers; (b) one or more crosslinking agents; and (c) one or more red-light blocking compounds blocking greater than 5% to about 25% of red-light transmission through the ophthalmic device at a wavelength of from about 550 nm to about 800 nm, wherein the one or more red-light blocking compounds have one or more ethylenically unsaturated reactive end groups.

OPHTHALMIC DEVICES

An ophthalmic device for slowing, inhibiting or preventing myopia progression which is a polymerization product of a monomeric mixture comprising (a) greater than 50 wt. %, based on the total weight of the monomeric mixture, of one or more non-silicone-containing hydrophilic monomers; (b) one or more crosslinking agents; and (c) one or more red-light blocking compounds blocking greater than 5% to about 25% of red-light transmission through the ophthalmic device at a wavelength of from about 550 nm to about 800 nm, wherein the one or more red-light blocking compounds have one or more ethylenically unsaturated reactive end groups.

WS12-RELEASING CONTACT LENS

A WS12-releasing contact lens is described as well as method of manufacturing the same. The WS12-releasing contact lens comprises a polymeric lens body and WS12 releasably adhered to the polymeric lens body, and releases from 0.05 μg to 0.5 μg WS12 after 1 hour in a release media or when worn by a human subject. The WS12-releasing contact lens can be comfortably worn by a symptomatic contact lens wearer and can increase the duration of comfortable lens wearing time and/or reduce lens awareness events and/or reduce contact lens dryness in a symptomatic contact lens wearer.

WS12-RELEASING CONTACT LENS

A WS12-releasing contact lens is described as well as method of manufacturing the same. The WS12-releasing contact lens comprises a polymeric lens body and WS12 releasably adhered to the polymeric lens body, and releases from 0.05 μg to 0.5 μg WS12 after 1 hour in a release media or when worn by a human subject. The WS12-releasing contact lens can be comfortably worn by a symptomatic contact lens wearer and can increase the duration of comfortable lens wearing time and/or reduce lens awareness events and/or reduce contact lens dryness in a symptomatic contact lens wearer.

CONTACT LENS WITH IMPROVED VISION BREAK-UP TIME

Described are polymerizable high energy light absorbing compounds. The compounds absorb various wavelengths of ultraviolet and/or high energy visible light and are suitable for incorporation in various products, such as biomedical devices and ophthalmic devices. Such devices exhibit a number of desirable properties, including favorable vision break-up times.

OPTICAL MATERIAL, OPTICAL PRODUCT, AND MANUFACTURING METHOD THEREOF

An optical material for making an optical product is provided. The optical material includes a light-resistant material undergone surface modification by titanium dioxide, so that the optical product is at least resistant to light having a wavelength between 280 nm and 380 nm. The optical product and a manufacturing method thereof are also provided.

METHOD FOR MAKING PHOTOCHROMIC CONTACT LENSES

Described herein is a method for producing a contact lens comprising a central photochromic zone that has a diameter of about 13 mm or less and is concentric with the central axis of the contact lens. The method comprises: applying, in the center of the molding surface of a male mold half, a drop (having a volume of about 5 μL or less) of a first polymerizable fluid composition containing at least one photochromic compound and a relatively-high molecular weight polysiloxane vinylic crosslinker for increasing the viscosity and adhesion on the molding surface of the male mold half; dosing a second polymerizable fluid composition in a female mold hald; closing the female mold hald with the male mold half with the drop thereon to form a molding assembly; and curing the second polymerizable fluid composition and the drop of the first polymerizable fluid composition in the molding assembly.

METHOD FOR MAKING PHOTOCHROMIC CONTACT LENSES

Described herein is a method for producing a contact lens comprising a central photochromic zone that has a diameter of about 13 mm or less and is concentric with the central axis of the contact lens. The method comprises: applying, in the center of the molding surface of a male mold half, a drop (having a volume of about 5 μL or less) of a first polymerizable fluid composition containing at least one photochromic compound and a relatively-high molecular weight polysiloxane vinylic crosslinker for increasing the viscosity and adhesion on the molding surface of the male mold half; dosing a second polymerizable fluid composition in a female mold hald; closing the female mold hald with the male mold half with the drop thereon to form a molding assembly; and curing the second polymerizable fluid composition and the drop of the first polymerizable fluid composition in the molding assembly.

POLYMERIZABLE ABSORBERS OF UV AND HIGH ENERGY VISIBLE LIGHT
20220340760 · 2022-10-27 ·

Described are polymerizable high energy light absorbing compounds. The compounds absorb various wavelengths of ultraviolet and/or high energy visible light and are suitable for incorporation in various products, such as biomedical devices and ophthalmic devices.

POLYMERIZABLE ABSORBERS OF UV AND HIGH ENERGY VISIBLE LIGHT
20220340760 · 2022-10-27 ·