H01L2924/01044

Semiconductor device and method of forming the same

A device includes an interconnect structure, a barrier multi-layer structure, an oxide layer, a pad metal layer, and a passivation layer. The barrier multi-layer structure is over the interconnect structure, the barrier multi-layer structure includes a first metal nitride layer and a second metal nitride layer over the first metal nitride layer. The oxide layer is over the barrier multi-layer structure, in which the oxide layer is an oxide of the second metal nitride layer of the barrier multi-layer structure. The pad metal layer is over the oxide layer. The passivation layer is in contact with the barrier multi-layer structure, the oxide layer, and the pad metal layer.

Protective surface layer on under bump metallurgy for solder joining

A method of fabricating an under-bump metallurgy (UBM) structure that is free of gold processing includes forming a titanium layer on top of a far back of line (FBEOL) of a semiconductor. A first copper layer is formed on top of the titanium layer. A photoresist (PR) layer is formed on top of the first copper layer between traces of the FBEOL to provide a cavity to the FBEOL traces. A top copper layer is formed on top of the first copper layer. A protective surface layer (PSL) is formed on top of the top copper layer.

ADVANCED THROUGH SUBSTRATE VIA METALLIZATION IN THREE DIMENSIONAL SEMICONDUCTOR INTEGRATION
20170345739 · 2017-11-30 ·

An advanced through silicon via structure for is described. The device includes a substrate including integrated circuit devices. A high aspect ratio through substrate via is disposed in the substrate. The through substrate via has vertical sidewalls and a horizontal bottom. The substrate has a horizontal field area surrounding the through substrate via. A metallic barrier layer is disposed on the sidewalls of the through substrate via. A surface portion of the metallic barrier layer has been converted to a nitride surface layer by a nitridation process. The nitride surface layer enhances the nucleation of subsequent depositions. A first metal layer fills the through substrate via and has a recess in an upper portion. A second barrier layer is disposed over the recess. A second metal layer is disposed over the second barrier layer and creates a contact.

ADVANCED THROUGH SUBSTRATE VIA METALLIZATION IN THREE DIMENSIONAL SEMICONDUCTOR INTEGRATION
20170345739 · 2017-11-30 ·

An advanced through silicon via structure for is described. The device includes a substrate including integrated circuit devices. A high aspect ratio through substrate via is disposed in the substrate. The through substrate via has vertical sidewalls and a horizontal bottom. The substrate has a horizontal field area surrounding the through substrate via. A metallic barrier layer is disposed on the sidewalls of the through substrate via. A surface portion of the metallic barrier layer has been converted to a nitride surface layer by a nitridation process. The nitride surface layer enhances the nucleation of subsequent depositions. A first metal layer fills the through substrate via and has a recess in an upper portion. A second barrier layer is disposed over the recess. A second metal layer is disposed over the second barrier layer and creates a contact.

DESIGNS AND METHODS FOR CONDUCTIVE BUMPS
20220059484 · 2022-02-24 ·

Methods, techniques, and structures relating to die packaging. In one exemplary implementation, a die package interconnect structure includes a semiconductor substrate and a first conducting layer in contact with the semiconductor substrate. The first conducting layer may include a base layer metal. The base layer metal may include Cu. The exemplary implementation may also include a diffusion barrier in contact with the first conducting layer and a wetting layer on top of the diffusion barrier. A bump layer may reside on top of the wetting layer, in which the bump layer may include Sn, and Sn may be electroplated. The diffusion barrier may be electroless and may be adapted to prevent Cu and Sn from diffusing through the diffusion barrier. Furthermore, the diffusion barrier may be further adapted to suppress a whisker-type formation in the bump layer.

Final passivation for wafer level warpage and ULK stress reduction

Embodiments are directed to a method of forming a semiconductor chip package and resulting structures having an annular PSPI region formed under a BLM pad. An annular region is formed under a barrier layer metallurgy (BLM) pad. The annular region includes a photosensitive polyimide (PSPI). A conductive pedestal is formed on a surface of the BLM pad and a solder bump is formed on a surface of the conductive pedestal. The annular PSPI region reduces wafer warpage and ULK peeling stress.

Final passivation for wafer level warpage and ULK stress reduction

Embodiments are directed to a method of forming a semiconductor chip package and resulting structures having an annular PSPI region formed under a BLM pad. An annular region is formed under a barrier layer metallurgy (BLM) pad. The annular region includes a photosensitive polyimide (PSPI). A conductive pedestal is formed on a surface of the BLM pad and a solder bump is formed on a surface of the conductive pedestal. The annular PSPI region reduces wafer warpage and ULK peeling stress.

PROCESS FOR ELECTRICALLY CONNECTING CONTACT SURFACES OF ELECTRONIC COMPONENTS

A process for electrically connecting contact surfaces of electronic components by capillary wedge bonding a round wire of 8 to 80 μm to the contact surface of a first electronic component, forming a wire loop, and stitch bonding the wire to the contact surface of a second electronic component, wherein the wire comprises a wire core having a silver or silver-based wire core with a double-layered coating comprised of a 1 to 50 nm thick inner layer of nickel or palladium and an adjacent 5 to 200 nm thick outer layer of gold.

PROCESS FOR ELECTRICALLY CONNECTING CONTACT SURFACES OF ELECTRONIC COMPONENTS

A process for electrically connecting contact surfaces of electronic components by capillary wedge bonding a round wire of 8 to 80 μm to the contact surface of a first electronic component, forming a wire loop, and stitch bonding the wire to the contact surface of a second electronic component, wherein the wire comprises a wire core having a silver or silver-based wire core with a double-layered coating comprised of a 1 to 50 nm thick inner layer of nickel or palladium and an adjacent 5 to 200 nm thick outer layer of gold.

Epoxy resin composition for encapsulating semiconductor device and semiconductor device encapsulated by the same
09735076 · 2017-08-15 · ·

An epoxy resin composition for encapsulating a semiconductor device and a semiconductor device encapsulated by the epoxy resin composition, the composition including a base resin; a filler; a colorant; and a thermochromic pigment, wherein a color of the thermochromic pigment is irreversibly changed when a temperature thereof exceeds a predetermined temperature.