H10N30/04

Method for adjusting the stress state of a piezoelectric film and acoustic wave device employing such a film
11462676 · 2022-10-04 · ·

A method for adjusting the stress state of a piezoelectric film having a first stress state at room temperature includes a step of forming an assembly including a carrier having a thermal expansion coefficient, a compliant layer placed on the carrier, and the piezoelectric film placed on the compliant layer, the piezoelectric film having a thermal expansion coefficient different from that of the carrier. The method also includes a step of heat treating the assembly, in which the assembly is heated to a treatment temperature above the glass transition temperature of the compliant layer. The present disclosure also relates to a process for fabricating an acoustic wave device comprising the piezoelectric layer the stress state of which was adjusted as described herein.

Nanovoided graded-index optical elements, optical arrays, and methods of forming the same

A graded-index optical element may include a nanovoided material including a first surface and a second surface opposite the first surface. The nanovoided material may be transparent between the first surface and the second surface. Additionally, the nanovoided material may have a predefined change in effective refractive index in at least one axis due to a change in at least one of nanovoid size or nanovoid distribution along the at least one axis. Various other elements, devices, systems, materials, and methods are also disclosed.

METHODS AND MECHANISMS FOR MAINTAINING AN ELECTRO-ACTIVE POLYMER IN A PRE-STRETCH STATE AND USES THEREOF
20220248539 · 2022-08-04 ·

In some embodiments, the present invention is directed to an actuator which includes at least the following: a pre-stretched electro-active polymer film being pre-stretched in a single or biaxial planar directions; at least one first semi-stiff conductor attached to a first surface of the pre-stretched electro-active polymer film, wherein the first surface is parallel to the single or biaxial planar stretch directions; at least one second semi-stiff conductor attached to a second surface of the pre-stretched electro-active polymer film, wherein the second surface is opposite to the first surface; where the semi-stiff conductors are configured to: fix the pre-stretched electro-active polymer film in a pre-stretched state and allow the pre-stretched electro-active polymer film to expand; a pair of mechanical connectors coupled to each end of an active region of the pre-stretched electro-active polymer film.

COMPOSITIONS FOR ACTIVE COMPRESSION DEVICES AND RELATED METHODS
20220246829 · 2022-08-04 ·

Some embodiments relate to compositions for active compression devices and related methods. In some embodiments, a composition for an active compression device comprises an electro-active polymer film. In some embodiments, the electro-active polymer film comprises at least one polymer and at least one additive.

Polymer materials including coated nanovoids and methods and systems for forming the same

A nanovoided polymer-based material may include a bulk polymer material defining a plurality of nanovoids and an interfacial film disposed at an interface between each of the plurality of nanovoids and the bulk polymer material. The interfacial film may include one or more layers of material. A method of forming a nanovoided polymer-based material may include (1) forming a bulk polymer material defining a plurality of nanovoids and (2) forming an interfacial film at an interface between each of the plurality of nanovoids and the bulk polymer material. Various other methods, systems, and materials are also disclosed.

Fabrication of shaped voids

In some examples, a method includes forming a material layer on a substrate, partially polymerizing a component of the material layer, to form fluid-filled droplets within a partially polymerized matrix, deforming the material layer to form anisotropic fluid-filled droplets, and further polymerizing the partially polymerized matrix to form an anisotropic voided polymer, including anisotropic voids in a polymer matrix. The anisotropic voids may include anisotropic nanovoids. Example methods may further include depositing electrodes on the anisotropic voided polymer so that at least a portion of the anisotropic voided polymer is located between the electrodes. Examples may include forming electroactive elements including an anisotropic nanovoided polymer, and devices (such as sensors and/or actuators) including electroactive elements.

Multiple layers between electrodes including nanovoided polymer

In some examples, a device includes a multilayer structure, a first electrode, and a second electrode, where the multilayer structure is located at least in part between the first electrode and the second electrode, and the multilayer structure includes a nanovoided polymer layer, and a solid layer. The solid layer may include a non-nanovoided layer. The nanovoided polymer layer may be an electroactive layer. The device may further include a control circuit configured to apply an electrical potential between the first electrode and the second electrode, which may induce a mechanical deformation of the multilayer.

Method for processing a lithium tantalate crystal substrate

A method for processing a lithium tantalate crystal substrate includes providing a lithium tantalate crystal substrate, roughening the lithium tantalate crystal substrate, providing a catalytic agent, bringing the lithium tantalate crystal substrate and the catalytic agent into contact with each other after the lithium tantalate crystal substrate is roughened, and subjecting the lithium tantalate crystal substrate to a reduction treatment. The reduction treatment is conducted at a temperature not higher than a Curie temperature of the lithium tantalate crystal substrate. The catalytic agent is selected from the group consisting of metal powder, metal gas, and metal carbonate powder.

Methods and mechanisms for maintaining an electro-active polymer in a pre-stretch state and uses thereof
11291121 · 2022-03-29 · ·

In some embodiments, the present invention is directed to an actuator which includes at least the following: a pre-stretched electro-active polymer film being pre-stretched in a single or biaxial planar directions; at least one first semi-stiff conductor attached to a first surface of the pre-stretched electro-active polymer film, wherein the first surface is parallel to the single or biaxial planar stretch directions; at least one second semi-stiff conductor attached to a second surface of the pre-stretched electro-active polymer film, wherein the second surface is opposite to the first surface; where the semi-stiff conductors are configured to: fix the pre-stretched electro-active polymer film in a pre-stretched state and allow the pre-stretched electro-active polymer film to expand; a pair of mechanical connectors coupled to each end of an active region of the pre-stretched electro-active polymer film.

Microelectronic assemblies having substrate-integrated perovskite layers

Disclosed herein are microelectronic assemblies with integrated perovskite layers, and related devices and methods. For example, in some embodiments, a microelectronic assembly may include an organic package substrate portion having a surface with a conductive layer, and a perovskite conductive layer on the conductive layer. In some embodiments, a microelectronic assembly may include an organic package substrate portion having a surface with a conductive layer, a perovskite conductive layer having a first crystalline structure on the conductive layer, and a perovskite dielectric layer having a second crystalline structure on the perovskite conductive layer. In some embodiments, the first and second crystalline structures have a same orientation.