H01F1/33

COIL COMPONENT MAGNETIC BASE

A coil component includes a magnetic portion that includes metal particles and a resin material, a coil conductor embedded in the magnetic portion and having a core portion, and outer electrodes electrically connected to the coil conductor. The magnetic portion includes a magnetic outer coating and a magnetic base having a protrusion portion. The coil conductor is disposed on the magnetic base such that the protrusion portion is located in the core portion. The magnetic outer coating is disposed so as to cover the coil conductor, and the bottom surface of the magnetic base includes a recessed portion in an area opposite to the protrusion portion.

COIL COMPONENT MAGNETIC BASE

A coil component includes a magnetic portion that includes metal particles and a resin material, a coil conductor embedded in the magnetic portion and having a core portion, and outer electrodes electrically connected to the coil conductor. The magnetic portion includes a magnetic outer coating and a magnetic base having a protrusion portion. The coil conductor is disposed on the magnetic base such that the protrusion portion is located in the core portion. The magnetic outer coating is disposed so as to cover the coil conductor, and the bottom surface of the magnetic base includes a recessed portion in an area opposite to the protrusion portion.

SILICON OXIDE-COATED IRON POWDER, METHOD FOR PRODUCING THE SAME, MOLDED BODY FOR INDUCTOR USING THE SAME, AND INDUCTOR
20210050132 · 2021-02-18 ·

A silicon oxide-coated iron powder has a small particle diameter, can achieve high in a high frequency band, and has high insulating property. In a method for producing the powder, a silicon alkoxide is added to a slurry containing iron powder having an average particle diameter of 0.25 m or more and 0.80 m or less and an average axial ratio of 1.5 or less dispersed in a mixed solvent of water and an organic material containing water in an amount of 1% by mass or more and 40% by mass or less. Then, a hydrolysis catalyst for the silicon alkoxide is added to perform silicon oxide coating, the method resulting in a silicon oxide-coated iron powder having the high in a high frequency band and the high insulating property.

SILICON OXIDE-COATED SOFT MAGNETIC POWDER AND METHOD FOR PRODUCING SAME
20210060642 · 2021-03-04 ·

A silicon oxide-coated soft magnetic powder has excellent insulating property and provides a high powder compact density. In making the powder, silicon alkoxide is added to a slurry containing soft magnetic powder containing iron in an amount of 20% by mass or more dispersed in a mixed solvent of water and an organic solvent containing water in an amount of 1% by mass or more and 40% by mass or less. A hydrolysis catalyst for the silicon alkoxide is then added to perform silicon oxide coating. The coated magnetic powder has a coverage factor R of 70% or more defined by R=Si100/(Si+M) (wherein Si and M represent molar fractions of Si and elements constituting the soft magnetic powder obtained by an XPS measurement), a powder compact density of 4.0 g/cm.sup.3 or more, and high at high frequency and high insulating property.

COIL COMPONENT

A coil component includes a support substrate and a coil portion disposed on the support substrate, a body, in which the support substrate and the coil portion are embedded, having one surface and the other surface, one side surface and the other side surface, and one end surface and the other end surface, a first lead-out portion and a second lead-out portion, respectively extending from the coil portion to be exposed from the one side surface and the other side surface, an insulating layer disposed on each of the one surface and the other surface, and an oxide insulating layer disposed on each of the one side surface and the other side surface and each of the one end surface and the other end surface. The insulating layer is provided with a plurality of slits spaced apart from each other to expose a surface of the body.

INDIRECT ADDITIVE MANUFACTURING PROCESS FOR FABRICATING BONDED SOFT MAGNETS

A bonded soft magnet object comprising bonded soft magnetic particles of an iron-containing alloy having a soft magnet characteristic, wherein the bonded soft magnetic particles have a particle size of at least 200 nm and up to 100 microns. Also described herein is a method for producing the bonded soft magnet by indirect additive manufacturing (IAM), such as by: (i) producing a soft magnet preform by bonding soft magnetic particles with an organic binder, wherein the magnetic particles have an iron-containing alloy composition with a soft magnet characteristic, and wherein the particles of the soft magnet material have a particle size of at least 200 nm and up to 100 microns; (ii) subjecting the preform to an elevated temperature sufficient to remove the organic binder to produce a binder-free preform; and (iii) sintering the binder-free preform at a further elevated temperature to produce the bonded soft magnet.

INDIRECT ADDITIVE MANUFACTURING PROCESS FOR FABRICATING BONDED SOFT MAGNETS

A bonded soft magnet object comprising bonded soft magnetic particles of an iron-containing alloy having a soft magnet characteristic, wherein the bonded soft magnetic particles have a particle size of at least 200 nm and up to 100 microns. Also described herein is a method for producing the bonded soft magnet by indirect additive manufacturing (IAM), such as by: (i) producing a soft magnet preform by bonding soft magnetic particles with an organic binder, wherein the magnetic particles have an iron-containing alloy composition with a soft magnet characteristic, and wherein the particles of the soft magnet material have a particle size of at least 200 nm and up to 100 microns; (ii) subjecting the preform to an elevated temperature sufficient to remove the organic binder to produce a binder-free preform; and (iii) sintering the binder-free preform at a further elevated temperature to produce the bonded soft magnet.

COIL COMPONENT AND METHOD FOR MANUFACTURING SAME
20210065974 · 2021-03-04 ·

A magnetic body of the coil component is constituted by soft magnetic metal grains joined together via a glass phase, wherein the soft magnetic metal grains contain Fe in their metal part and also have, on their surface, an amorphous insulation layer containing Si and O, and wherein the percentage by mass of Si relative to all elements in the insulation layer is higher than that in the glass phase. The coil component can offer improved dielectric breakdown voltage.

COIL DEVICE

A coil device includes: a drum core having first and second flange portions and a winding core portion therebetween; a coil wound around the core portion; a plate core connected to first and second flange portions first and second flange surfaces at a first direction side; a first electrode terminal on the first flange portion, one coil end portion electrically connected on the first electrode terminal; and a second electrode terminal on the second flange portion, the other coil end portion electrically connected on the second electrode terminal. The plate core has a first and second projecting portions respectively protruding toward the first and second flange surfaces and having first and second flat surfaces facing the first and second flange surfaces. The drum core and the plate core are connected by abutting and bonding the first and second flange surfaces against the first and second flat surfaces.

SOFT MAGNETIC METAL POWDER AND ELECTRONIC COMPONENT

Provided is a soft magnetic metal powder including a plurality of soft magnetic metal particles. Each of the soft magnetic metal particles includes a metal particle and an oxidized part covering the metal particle. The metal particle includes at least Fe. The oxidized part includes an oxide of at least one kind of element selected from the group consisting of Fe, Si, and B, and at least one kind of element of Ca and Mg. A concentration of Ca or Mg in the metal particle and the oxidized part is maximum in the oxidized part. An average value of a maximum value of the concentration of Ca or Mg in the oxidized part is 0.2 atom % or more.