Patent classifications
H01J37/347
Systems and methods for uniform target erosion magnetic assemblies
In an embodiment, a system includes: a chamber; and a magnetic assembly contained within the chamber. The magnetic assembly comprises: an inner magnetic portion comprising first magnets; and an outer magnetic portion comprising second magnets. At least two adjacent magnets, of either the first magnets or the second magnets, have different vertical displacements, and the magnetic assembly is configured to rotate around an axis to generate an electromagnetic field that moves ions toward a target region within the chamber.
System and method to control PVD deposition uniformity
A physical vapor deposition chamber comprising a rotating substrate support having a rotational axis, a first cathode having a radial center positioned off-center from a rotational axis of the substrate support is disclosed. A process controller comprising one or more process configurations selected from one or more of a first configuration to determine a rotation speed (v) for a substrate support to complete a whole number of rotations (n) around the rotational axis of the substrate support in a process window time (t) to form a layer of a first material on a substrate, or a second configuration to rotate the substrate support at the rotation speed (v).
Measuring method and semiconductor structure forming method
A measuring method is provided. A probe and a first sensor are disposed over a jig including a bar protruding from the jig. The probe is moved until a first surface of the probe is laterally aligned with a second surface of the bar facing the jig. A first distance between the second surface of the bar and the first sensor is obtained by the first sensor. The probe and the first sensor are disposed over a magnetron. Magnetic field intensities at different elevations above the magnetron are measured by the probe. A method for forming a semiconductor structure is also provided.
Anti-stiction process for MEMS device
A method for treating a micro electro-mechanical system (MEMS) component is disclosed. In one example, the method includes the steps of providing a first wafer, treating the first wafer to form cavities and at least an oxide layer on a top surface of the first wafer using a first chemical vapor deposition (CVD) process, providing a second wafer, bonding the second wafer on a top surface of the at least one oxide layer, treating the second wafer to form a first plurality of structures, depositing a layer of Self-Assembling Monolayer (SAM) to a surface of the MEMS component using a second CVD process.
Sputtering System with a Plurality of Cathode Assemblies
A magnetron sputtering system includes a substrate mounted within a vacuum chamber. A plurality of cathode assemblies includes a first set of cathode assemblies and a second set of cathode assemblies, and is configured for reactive sputtering. Each cathode assembly includes a target comprising sputterable material and has an at least partially exposed planar sputtering surface. A target support is configured to support the target in the vacuum chamber and rotate the target relative to the vacuum chamber about a target axis. A magnetic field source includes a magnet array. A cathode assemblies controller assembly is operative to actuate the first set of cathode assemblies without actuating the second set of cathode assemblies, and to actuate the second set of cathode assemblies without actuating the first set of cathode assemblies.
FILM FORMING METHOD, FILM FORMING APPARATUS, AND PROGRAM
There is provided a film forming method performed in a film forming apparatus having cathode units capable of installing a plurality of targets. The method comprises performing a film formation process using a first target between the first target and a second target that are disposed at the cathode units and are made of the same material, based on a recipe of the first target, receiving from a user, after a value for managing a lifespan of the first target has reached a predetermined threshold, selection of the second target to be used for the film forming process, and performing the film forming process using the selected second target based on a recipe in which setting of target-related control items of the recipe of the first target is converted for the selected second target.
OXYGEN CONTROLLED PVD ALN BUFFER FOR GAN-BASED OPTOELECTRONIC AND ELECTRONIC DEVICES
Oxygen controlled PVD AlN buffers for GaN-based optoelectronic and electronic devices is described. Methods of forming a PVD AlN buffer for GaN-based optoelectronic and electronic devices in an oxygen controlled manner are also described. In an example, a method of forming an aluminum nitride (AlN) buffer layer for GaN-based optoelectronic or electronic devices involves reactive sputtering an AlN layer above a substrate, the reactive sputtering involving reacting an aluminum-containing target housed in a physical vapor deposition (PVD) chamber with a nitrogen-containing gas or a plasma based on a nitrogen-containing gas. The method further involves incorporating oxygen into the AlN layer.
SPUTTERING APPARATUS INCLUDING GAS DISTRIBUTION SYSTEM
Some embodiments provide a magnetron sputtering apparatus including a vacuum chamber within which a controlled environment may be established, a target comprising one or more sputterable materials, wherein the target includes a racetrack-shaped sputtering zone that extends longitudinally along a longitudinal axis and comprises a straightaway area sandwiched between a first turnaround area and a second turnaround area, a gas distribution system that supplies a first gas mixture to the first turnaround area and/or the second turnaround area and supplies a second gas mixture to the straightaway area, wherein the first gas mixture reduces a sputtering rate relative to the second gas mixture. In some cases, the first gas mixture includes inert gas having a first atomic weight and the second gas mixture includes inert gas having a second atomic weight, wherein the second atomic weight is heavier than the first atomic weight.
Oxygen controlled PVD AlN buffer for GaN-based optoelectronic and electronic devices
Oxygen controlled PVD AlN buffers for GaN-based optoelectronic and electronic devices is described. Methods of forming a PVD AlN buffer for GaN-based optoelectronic and electronic devices in an oxygen controlled manner are also described. In an example, a method of forming an aluminum nitride (AlN) buffer layer for GaN-based optoelectronic or electronic devices involves reactive sputtering an AlN layer above a substrate, the reactive sputtering involving reacting an aluminum-containing target housed in a physical vapor deposition (PVD) chamber with a nitrogen-containing gas or a plasma based on a nitrogen-containing gas. The method further involves incorporating oxygen into the AlN layer.
MACHINE FOR THE DEPOSITION OF MATERIAL BY THE CATHODIC SPUTTERING TECHNIQUE
A machine for the deposition of material on a substrate by the cathodic sputtering technique is provided, of the type provided with a cathode assembly having a tubular support extending substantially along a first axis (A), and a plurality of magnetic elements constrained to the tubular support and spaced from one another along the first axis (A), and wherein each of the magnetic elements has at least one second axis (M) of magnetic orientation, linking the respective magnetic poles (N; S) and has an outer side jutting from the tubular support and an inner side constrained to the tubular support, wherein the second axis (M) linking the poles of each magnetic element is transverse to the first axis (A) of the tubular support and the polarity (S; N) of the outer sides of two consecutive magnetic elements along the first axis (A) on the tubular support is alternating.