H01F1/153
Amorphous metal strip and method for producing an amorphous metal strip
A method for the production of a metal strip is provided. The method includes providing an amorphous metal strip having a first main surface and a second, opposing main surface. The first and/or the second main surface are treated with a wet-chemical etching process and/or a photochemical etching process.
Amorphous metal strip and method for producing an amorphous metal strip
A method for the production of a metal strip is provided. The method includes providing an amorphous metal strip having a first main surface and a second, opposing main surface. The first and/or the second main surface are treated with a wet-chemical etching process and/or a photochemical etching process.
FE-BASED NANOCRYSTALLINE ALLOY AND ELECTRONIC COMPONENT USING THE SAME
An Fe-based nanocrystalline alloy is represented by Composition Formula, (Fe.sub.(1-a)M.sup.1a).sub.100-b-c-d-e-gM.sup.2.sub.bB.sub.cP.sub.dCu.sub.eM.sup.3.sub.g, where M.sup.1 is at least one element selected from the group consisting of Co and Ni, M.sup.2 is at least one element selected from the group consisting of Nb, Mo, Zr, Ta, W, Hf, Ti, V, Cr, and Mn, M.sup.3 is at least two elements selected from the group consisting of C, Si, Al, Ga, and Ge but necessarily includes C, and 0≤a≤0.5, 1.5<b≤3, 10≤c≤13, 0<d≤4, 0<e≤1.5, and 8.5≤g≤12.
FE-BASED NANOCRYSTALLINE ALLOY AND ELECTRONIC COMPONENT USING THE SAME
An Fe-based nanocrystalline alloy is represented by Composition Formula, (Fe.sub.(1-a)M.sup.1a).sub.100-b-c-d-e-gM.sup.2.sub.bB.sub.cP.sub.dCu.sub.eM.sup.3.sub.g, where M.sup.1 is at least one element selected from the group consisting of Co and Ni, M.sup.2 is at least one element selected from the group consisting of Nb, Mo, Zr, Ta, W, Hf, Ti, V, Cr, and Mn, M.sup.3 is at least two elements selected from the group consisting of C, Si, Al, Ga, and Ge but necessarily includes C, and 0≤a≤0.5, 1.5<b≤3, 10≤c≤13, 0<d≤4, 0<e≤1.5, and 8.5≤g≤12.
MIXTURE FOR FORMING A MULTILAYER INDUCTOR AND THE FABRICATION METHOD THEREOF
A mixture for making a multilayer inductor, wherein the mixture comprises a first magnetic powder, a second magnetic powder, and a glass material, wherein each of the first magnetic powder and the second magnetic powder comprises an amorphous or nanocrystalline magnetic powder, wherein a softening point temperature of the glass material is in a range of 300°˜430° C.
MIXTURE FOR FORMING A MULTILAYER INDUCTOR AND THE FABRICATION METHOD THEREOF
A mixture for making a multilayer inductor, wherein the mixture comprises a first magnetic powder, a second magnetic powder, and a glass material, wherein each of the first magnetic powder and the second magnetic powder comprises an amorphous or nanocrystalline magnetic powder, wherein a softening point temperature of the glass material is in a range of 300°˜430° C.
Fe-Ni Nanocomposite Alloys
A nanocomposite comprising crystalline grains in an amorphous matrix, the crystalline grains comprising an iron (Fe)-nickel (Ni) compound and being separated from one another by the amorphous matrix; and one or more barriers between the crystalline grains and the amorphous matrix, the barriers being configured to inhibit growth of the crystalline grains during forming of the crystalline grains, a barrier of the one or more barriers being between a crystalline grain and the amorphous matrix; wherein the amorphous matrix comprises an increased resistivity relative to a resistivity of the crystalline grains; and wherein the amorphous matrix is configured to reduce losses of the crystalline grains caused by a change in a magnetic field applied to the crystalline grains relative to losses of the crystalline grains that occur without the amorphous matrix.
SOFT MAGNETIC ALLOY AND MAGNETIC COMPONENT
A soft magnetic alloy comprising an internal area having a soft magnetic type alloy composition including Fe and Co, a Co concentrated area existing closer to a surface side than the internal area and having a higher Co concentration than in the internal area, a SB concentrated area existing closer to the surface side than the Co concentrated area and having a higher concentration of at least one element selected from Si and B than in the internal area, and a Fe concentrated area including Fe existing closer to the surface side than the SB concentrated area; wherein a crystalized area ratio of the SB concentrated area represented by S.sub.SB.sup.cry/S.sub.SB and a crystalized area ratio of the Fe concentrated area represented by S.sub.Fe.sup.cry/S.sub.Fe, satisfy a relation of (S.sub.SB.sup.cry/S.sub.SB)<(S.sub.Fe.sup.cry/S.sub.Fe).
Iron alloy particle and method for producing iron alloy particle
The iron alloy particle is a particle including an iron alloy. The particle includes multiple mixed-phase particles, each including nanocrystals of 10 nm or more and 100 nm or less (i.e., from 10 nm to 100 nm) in crystallite size and an amorphous phase; and a grain boundary layer between the mixed-phase particles. Also, the iron alloy has a composition containing Fe, Si, P, B, C, and Cu.
Fe-based soft magnetic alloy and method for manufacturing the same
The present disclosure relates to an iron (Fe)-based amorphous soft magnetic alloy and a method for manufacturing the soft magnetic alloy. According to the present disclosure, there is provided an Fe-based soft magnetic alloy including C and S meeting 1≥a+b≥6, wherein a is an atomic % content of C and b is an atomic % content of S, B meeting 4.5≥x≥13.0, wherein x is an atomic % content of B, Cu meeting 0.2≥y≥1.5, wherein y is an atomic % content of Cu, Al meeting 0.5≥z≥2, wherein z is an atomic % content of Al, and a remaining atomic % content of Fe and other inevitable impurities, wherein the Fe-based soft magnetic alloy includes a micro-structure, and wherein the micro-structure includes a crystalline phase with a mean crystalline grain size ranging from 15 nm to 50 nm in an amorphous base.