Patent classifications
H01L21/76825
Semiconductor structure and method for manufacturing the same
A semiconductor structure includes a first dielectric layer, a first metal feature in the first dielectric layer, at least one etch stop layer on the first dielectric layer, a second dielectric layer on the at least one etch stop layer. The semiconductor structure further includes a first barrier sublayer on a sidewall of the second dielectric layer and the at least one etch stop layer, a second barrier sublayer on the first barrier sublayer and the first metal feature, and a second metal feature on the second barrier sublayer.
SEMICONDUCTOR DEVICE AND METHOD FOR FORMING THE SAME
A semiconductor device includes a first dielectric layer disposed over a substrate and a conductive feature, a doped dielectric layer disposed over the first dielectric layer, a first metal portion disposed in the first dielectric layer and in contact with the conductive feature, and a doped metal portion disposed over the first metal portion. The first metal portion and the doped metal portion include a same noble metal material. The doped dielectric layer and the doped metal portion include same dopants. The dopants are bonded to the noble metal material.
Interlayer dielectric layer
The present disclosure describes a method for forming a silicon-based, carbon-rich, low-k ILD layer with a carbon concentration between about 15 atomic % and about 20 atomic %. For example, the method includes depositing a dielectric layer, over a substrate, with a dielectric material having a dielectric constant below 3.9 and a carbon atomic concentration between about 15% and about 20%; exposing the dielectric layer to a thermal process configured to outgas the dielectric material; etching the dielectric layer to form openings; and filling the openings with a conductive material to form conductive structures.
Structure manufacturing method and manufacturing device, and light irradiation device
There is provided a structure manufacturing method, including: preparing a wafer at least whose surface comprises Group III nitride crystal in a state of being immersed in an etching solution containing peroxodisulfate ions; and irradiating the surface of the wafer with light through the etching solution; wherein the group III nitride crystal has a composition in which a wavelength corresponding to a band gap is 310 nm or more, and during irradiation of the light, the surface of the wafer is irradiated with a first light having a wavelength of 200 nm or more and less than 310 nm under a first irradiation condition, and is irradiated with a second light having a wavelength of 310 nm or more and less than a wavelength corresponding to the band gap under a second irradiation condition controlled independently of the first irradiation condition.
Transistor Contacts and Methods of Forming the Same
In an embodiment, a device includes: a gate structure on a channel region of a substrate; a gate mask on the gate structure, the gate mask including a first dielectric material and an impurity, a concentration of the impurity in the gate mask decreasing in a direction extending from an upper region of the gate mask to a lower region of the gate mask; a gate spacer on sidewalls of the gate mask and the gate structure, the gate spacer including the first dielectric material and the impurity, a concentration of the impurity in the gate spacer decreasing in a direction extending from an upper region of the gate spacer to a lower region of the gate spacer; and a source/drain region adjoining the gate spacer and the channel region.
Etch profile control of via opening
A method comprises forming a source/drain contact over a source/drain region; forming an etch stop layer over the source/drain contact and an interlayer dielectric (ILD) layer over the etch stop layer; performing a first etching process to form a via opening extending through the ILD layer and a recess in the etch stop layer; oxidizing a sidewall of the recess in the etch stop layer; after oxidizing the sidewall of the recess in the etch stop layer, performing a second etching process to extend the via opening down to the source/drain contact; and after performing the second etching process, forming a source/drain via in the via opening.
Techniques for improved low dielectric constant film processing
A method may include providing a substrate having, on a first surface of the substrate, a low dielectric constant layer characterized by a layer thickness. The method may include heating the substrate to a substrate temperature in a range of 200° C. to 550° C.; and directing an ion implant treatment to the low dielectric constant layer, while the substrate temperature is in the range of 200° C. to 550° C. As such, the ion implant treatment may include implanting a low weight ion species, at an ion energy generating an implant depth equal to 40% to 175% of the layer thickness.
Integrated capacitor with sidewall having reduced roughness
An integrated capacitor on a semiconductor surface on a substrate includes a capacitor dielectric layer including at least one silicon compound material layer on a bottom plate. The capacitor dielectric layer includes a pitted sloped dielectric sidewall. Each of the pits is at least partially filled by one of a plurality of noncontiguous dielectric portions. A conformal dielectric layer may be formed over the noncontiguous dielectric portions. A top metal layer provides a top plate of the capacitor.
Integrated capacitor with sidewall having reduced roughness
An integrated capacitor on a semiconductor surface on a substrate includes a capacitor dielectric layer including at least one silicon compound material layer on a bottom plate. The capacitor dielectric layer includes a pitted sloped dielectric sidewall. Each of the pits is at least partially filled by one of a plurality of noncontiguous dielectric portions. A conformal dielectric layer may be formed over the noncontiguous dielectric portions. A top metal layer provides a top plate of the capacitor.
SEMICONDUCTOR DEVICE INCLUDING A POROUS DIELECTRIC LAYER, AND METHOD OF FORMING THE SEMICONDUCTOR DEVICE
A semiconductor device includes a porous dielectric layer including a recessed portion, a conductive layer formed in the recessed portion, and a cap layer formed on the porous dielectric layer and on the conductive layer in the recessed portion, an upper surface of the porous dielectric layer being exposed through a gap in the cap layer.