Patent classifications
H01L21/76882
Forming Liners to Facilitate The Formation of Copper-Containing Vias in Advanced Technology Nodes
A semiconductor device includes a source/drain component of a transistor. A source/drain contact is disposed over the source/drain component. A source/drain via is disposed over the source/drain contact. The source/drain via contains copper. A first liner at least partially surrounds the source/drain via. A second liner at least partially surrounds the first liner. The first liner and the second liner are disposed between the source/drain contact and the source/drain via. The first liner and the second liner have different material compositions.
Bottom-up formation of contact plugs
A method includes etching a dielectric layer to form a trench in the dielectric layer, depositing a metal layer extending into the trench, performing a nitridation process on the metal layer to convert a portion of the metal layer into a metal nitride layer, performing an oxidation process on the metal nitride layer to form a metal oxynitride layer, removing the metal oxynitride layer, and filling a metallic material into the trench using a bottom-up deposition process to form a contact plug.
Semiconductor device and method for forming the same
A semiconductor device includes a first dielectric layer disposed over a substrate and a conductive feature, a doped dielectric layer disposed over the first dielectric layer, a first metal portion disposed in the first dielectric layer and in contact with the conductive feature, and a doped metal portion disposed over the first metal portion. The first metal portion and the doped metal portion include a same noble metal material. The doped dielectric layer and the doped metal portion include same dopants. The dopants are bonded to the noble metal material.
BICONVEX LOW RESISTANCE METAL WIRE
At least one opening having a biconvex shape is formed into a dielectric material layer. A void-free metallization region (interconnect metallic region and/or metallic contact region) is provided to each of the openings. The void-free metallization region has the biconvex shape and exhibits a low wire resistance.
Cobalt first layer advanced metallization for interconnects
A method for fabricating an advanced metal conductor structure is described. A pattern in a dielectric layer is provided. The pattern includes a set of features in the dielectric for a set of metal conductor structures. An adhesion promoting layer is created over the patterned dielectric. A ruthenium layer is deposited over the adhesion promoting layer. Using a physical vapor deposition process, a cobalt layer is deposited over the ruthenium layer. A thermal anneal is performed which reflows the cobalt layer to fill the set of features to form a set of metal conductor structures. In another aspect of the invention, an integrated circuit device is formed using the method.
Semiconductor Device and Method of Fabricating the Same
A semiconductor device and a method of fabricating the same are provided. The semiconductor device includes a first interlayer insulating layer including a first trench, on a substrate a first liner layer formed along a side wall and a bottom surface of the first trench and including noble metal, the noble metal belonging to one of a fifth period and a sixth period of a periodic chart that follows numbering of International Union of Pure and Applied Chemistry (IUPAC) and belonging to one of eighth to tenth groups of the periodic chart, and a first metal wire filling the first trench on the first liner layer, a top surface of the first metal wire having a convex shape toward a bottom suffice of the first trench.
SEAM-HEALING METHOD UPON SUPRA-ATMOSPHERIC PROCESS IN DIFFUSION PROMOTING AMBIENT
Aspects of the disclosure include methods of treating a substrate to remove one or more of voids, seams, and grain boundaries from interconnects formed on the substrate. The method includes heating the substrate in an environment pressurized at supra-atmospheric pressure. In one example, the substrate may be heated in a hydrogen-containing atmosphere.
Method for electrochemically depositing metal on a reactive metal film
In accordance with one embodiment of the present disclosure, a method for depositing metal on a reactive metal film on a workpiece includes electrochemically depositing a metallization layer on a seed layer formed on a workpiece using a plating electrolyte having at least one plating metal ion, a pH range of about 6 to about 11 and applying a cathodic potential in the range of about −1 V to about −6 V. The workpiece includes a barrier layer disposed between the seed layer and a dielectric surface of the workpiece, the barrier layer including a first metal having a standard electrode potential more negative than 0 V and the seed layer including a second metal having a standard electrode potential more positive than 0 V.
Reflow enhancement layer for metallization structures
A reflow enhancement layer is formed in an opening prior to forming and reflowing a contact metal or metal alloy. The reflow enhancement layer facilitates the movement (i.e., flow) of the contact metal or metal alloy during a reflow anneal process such that a void-free metallization structure of the contact metal or metal alloy is provided.
ADVANCED THROUGH SUBSTRATE VIA METALLIZATION IN THREE DIMENSIONAL SEMICONDUCTOR INTEGRATION
A method providing a high aspect ratio through substrate via in a substrate is described. The through substrate via has vertical sidewalls and a horizontal bottom. The substrate has a horizontal field area surrounding the through substrate via. A metallic barrier layer is deposited on the sidewalls of the through substrate via. A nitridation process converts a surface portion of the metallic barrier layer to a nitride surface layer. The nitride surface layer enhances the nucleation of subsequent depositions. A first metal layer is deposited to fill a portion of the through substrate via and cover the horizontal field area. A thermal anneal step to reflow a portion of the first metal layer on the horizontal field area into the through substrate via. A second metal layer is deposited over the first metal layer to fill a remaining portion of the through substrate via. Another aspect of the invention is a device created by the method.