H01M8/021

Solid oxide fuel cell and electrochemical cell

A solid oxide fuel cell including unit cells, including: a pair of interconnectors for electrically connecting the unit cells; a membrane-electrode assembly including an electrolyte membrane and a pair of electrode layers disposed with the electrolyte membrane therebetween; a pair of current collectors disposed between the electrode layers and the interconnectors so as to be in contact with the pair of electrode layers and the pair of interconnectors, respectively, and electrically connecting the pair of electrode layers and the pair of interconnectors; and elastic bodies biasing at least one current collector of the pair of current collectors toward a corresponding electrode layer and made of austenitic stainless steel.

ANODE SPLITTER PLATE AND METHODS FOR MAKING THE SAME

Various embodiments of a reactant feed and return assembly, such as an anode splitter plate (ASP), are provided for facilitating reactant feed and exhaust flow in a solid oxide fuel cell (SOFC) stack system. Embodiments include a reactant feed and return assembly including at least a first portion formed of a chromium-based alloy, such as a chromium-iron alloy, having a similar coefficient of thermal expansion as other SOFC components and may therefore reduce internal stress in an SOFC stack. Methods for making an a reactant feed and return assembly comprising a chromium-based alloy are also provided.

METAL SEPARATOR FOR FUEL CELL

A metal separator for a fuel cell is disposed on each side of a membrane electrode assembly. The metal separator includes a base material containing Fe as a primary component and 10 mass % or more of Cr. The base material further contains at least any one of 0.1 to 15 mass % of Ta, 0.1 to 15 mass % of V, and 4 to 10 mass % of Sn.

METAL SEPARATOR FOR FUEL CELL

A metal separator for a fuel cell is disposed on each side of a membrane electrode assembly. The metal separator includes a base material containing Fe as a primary component and 10 mass % or more of Cr. The base material further contains at least any one of 0.1 to 15 mass % of Ta, 0.1 to 15 mass % of V, and 4 to 10 mass % of Sn.

PROTON EXCHANGE MEMBRANE FUEL CELL WITH STEPPED CHANNEL BIPOLAR PLATE

A fuel cell assembly includes a pair of corrugated bipolar plates. Each of the plates is defined by peak portions and sidewalls connecting the peak portions. The plates are fitted and nested within each other such that the sidewalls are in direct contact. Some of the sidewalls include a stepped shoulder portion such that each of the some of the sidewalls and the peak portions adjacent thereto form a stair-step profile and define a flow channel having a depth greater than a width.

Fuel cell

A fuel cell includes a main body which is formed by stacking a cathode layer, an electrolyte layer, and an anode layer, in which the surface of one of the cathode and anode layers serves as a first main surface, and the surface of the other layer serves as a second main surface; a first current collector in contact with the first main surface; and a second current collector in contact with the second main surface. As viewed in a thickness direction, at least a portion of the boundary of a second region of the second current collector corresponding to the second main surface is located within a first region of the first current collector corresponding to the first main surface, and the remaining portion is located within the first region or on the boundary of the first region.

Fuel cell

A fuel cell includes a main body which is formed by stacking a cathode layer, an electrolyte layer, and an anode layer, in which the surface of one of the cathode and anode layers serves as a first main surface, and the surface of the other layer serves as a second main surface; a first current collector in contact with the first main surface; and a second current collector in contact with the second main surface. As viewed in a thickness direction, at least a portion of the boundary of a second region of the second current collector corresponding to the second main surface is located within a first region of the first current collector corresponding to the first main surface, and the remaining portion is located within the first region or on the boundary of the first region.

Stainless steel for separation plate of polymer electrolyte membrane fuel cell having improved hydrophilic property and corrosion resistance, and manufacturing method therefor
11398631 · 2022-07-26 · ·

Provided are stainless steel for a separator of a polymer electrolyte membrane fuel cell, which exhibits enhanced hydrophilicity and enhanced corrosion resistance, and a method of manufacturing the same. In the stainless steel for a separator of a polymer electrolyte membrane fuel cell, which exhibits enhanced hydrophilicity and enhanced corrosion resistance, according to an embodiment of the present invention, a ratio of Cr hydroxide/Cr oxide included in a passivation film of the stainless steel ranges from 0.5 to 1.7, and the passivation film has a contact angle (θ) of 70° or less. Thus, not only corrosion resistance may be enhanced by removing a non-conductive film formed on a surface of the stainless steel and forming a new conductive film thereon, but hydrophilicity may also be secured without additional surface treatment such as a separate coating or the like, and thus manufacturing costs may be reduced and productivity may be increased.

Stainless steel for separation plate of polymer electrolyte membrane fuel cell having improved hydrophilic property and corrosion resistance, and manufacturing method therefor
11398631 · 2022-07-26 · ·

Provided are stainless steel for a separator of a polymer electrolyte membrane fuel cell, which exhibits enhanced hydrophilicity and enhanced corrosion resistance, and a method of manufacturing the same. In the stainless steel for a separator of a polymer electrolyte membrane fuel cell, which exhibits enhanced hydrophilicity and enhanced corrosion resistance, according to an embodiment of the present invention, a ratio of Cr hydroxide/Cr oxide included in a passivation film of the stainless steel ranges from 0.5 to 1.7, and the passivation film has a contact angle (θ) of 70° or less. Thus, not only corrosion resistance may be enhanced by removing a non-conductive film formed on a surface of the stainless steel and forming a new conductive film thereon, but hydrophilicity may also be secured without additional surface treatment such as a separate coating or the like, and thus manufacturing costs may be reduced and productivity may be increased.

COMPRESSION APPARATUS

A compression apparatus includes a stack of electrochemical cells each including an anode, a cathode, and an electrolyte membrane interposed therebetween, a pair of insulating plates disposed at respective ends of the stack in a stacking direction, a pair of end plates disposed on outside surfaces of the respective insulating plates, and a voltage applicator that applies a voltage between the anode and the cathode. The end plate having the cathode gas channel includes a first region that includes an outer peripheral surface of the cathode gas channel and is composed of a first steel material and a second region other than the first region which is composed of a second steel material. The first steel material has higher hydrogen embrittlement resistance than the second steel material, and the second steel material has higher stiffness than the first steel material.