H01L21/02466

Optimized heteroepitaxial growth of semiconductors

A method of performing heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and a second precursor gas, to form a heteroepitaxial growth of one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN on the substrate; wherein the substrate comprises one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN; wherein the carrier gas is Hz, wherein the first precursor is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the second precursor is one of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide), H.sub.2S (hydrogen sulfide), and NH.sub.3 (ammonia). The process may be an HVPE (hydride vapor phase epitaxy) process.

Transdermal microneedle continuous monitoring system

Transdermal microneedles continuous monitoring system is provided. The continuous system monitoring includes a substrate, a microneedle unit, a signal processing unit and a power supply unit. The microneedle unit at least comprises a first microneedle set used as a working electrode and a second microneedle set used as a reference electrode, the first and second microneedle sets arranging on the substrate. Each microneedle set comprises at least a microneedle. The first microneedle set comprises at least a sheet having a through hole on which a barbule forms at the edge. One of the sheets provides the through hole from which the barbules at the edge of the other sheets go through, and the barbules are disposed separately.

OPTIMIZED THICK HETEROEPITAXIAL GROWTH OF SEMICONDUCTORS WITH IN-SITU SUBSTRATE PRETREATMENT
20230137113 · 2023-05-04 ·

A method of performing HVPE heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and ternary-forming gasses (V/VI group precursor), to form a heteroepitaxial growth of a binary, ternary, and/or quaternary compound on the substrate; wherein the carrier gas is H.sub.2, wherein the first precursor gas is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the ternary-forming gasses comprise at least two or more of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide, or antimony tri-hydride, or stibine), H.sub.2S (hydrogen sulfide), NH.sub.3 (ammonia), and HF (hydrogen fluoride); flowing the carrier gas over the Group II/III element; exposing the substrate to the ternary-forming gasses in a predetermined ratio of first ternary-forming gas to second ternary-forming gas (1tf:2tf ratio); and changing the 1tf:2tf ratio over time.

Optimized Heteroepitaxial Growth of Semiconductors
20230095501 · 2023-03-30 ·

A method of performing HVPE heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and ternary-forming gasses (V/VI group precursor), to form a heteroepitaxial growth of a binary, ternary, and/or quaternary compound on the substrate; wherein the carrier gas is Hz, wherein the first precursor gas is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the ternary-forming gasses comprise at least two or more of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), HzTe (hydrogen telluride), SbH.sub.3 (hydrogen antimonide, or antimony tri-hydride, or stibine), H.sub.2S (hydrogen sulfide), NH.sub.3 (ammonia), and HF (hydrogen fluoride); flowing the carrier gas over the Group II/III element; exposing the substrate to the ternary-forming gasses in a predetermined ratio of first ternary-forming gas to second ternary-forming gas (1tf:2tf ratio); and changing the 1tf:2tf ratio over time.

Optimized Heteroepitaxial Growth of Semiconductors
20230038745 · 2023-02-09 ·

A method of performing heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and a second precursor gas, to form a heteroepitaxial growth of one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN on the substrate; wherein the substrate comprises one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN; wherein the carrier gas is Hz, wherein the first precursor is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the second precursor is one of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide), H.sub.2S (hydrogen sulfide), and NH.sub.3 (ammonia). The process may be an HVPE (hydride vapor phase epitaxy) process.

Optimized Heteroepitaxial Growth of Semiconductors
20230042689 · 2023-02-09 ·

A method of performing heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and a second precursor gas, to form a heteroepitaxial growth of one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN on the substrate; wherein the substrate comprises one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN; wherein the carrier gas is Hz, wherein the first precursor is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the second precursor is one of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), HzTe (hydrogen telluride), SbH.sub.3 (hydrogen antimonide), H.sub.2S (hydrogen sulfide), and NH.sub.3 (ammonia). The process may be an HVPE (hydride vapor phase epitaxy) process.

Optimized Heteroepitaxial Growth of Semiconductors
20230042736 · 2023-02-09 ·

A method of performing heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and a second precursor gas, to form a heteroepitaxial growth of one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN on the substrate; wherein the substrate comprises one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN; wherein the carrier gas is H.sub.2, wherein the first precursor is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the second precursor is one of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide), H.sub.2S (hydrogen sulfide), and NH.sub.3 (ammonia). The process may be an HVPE (hydride vapor phase epitaxy) process.

Optimized thick heteroepitaxial growth of semiconductors with in-situ substrate pretreatment

A method of performing heteroepitaxy comprises exposing a substrate to a carrier gas, a first precursor gas, a Group II/III element, and a second precursor gas, to form a heteroepitaxial growth of one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN on the substrate; wherein the substrate comprises one of GaAs, AlAs, InAs, GaP, InP, ZnSe, GaSe, CdSe, InSe, ZnTe, CdTe, GaTe, HgTe, GaSb, InSb, AlSb, CdS, GaN, and AlN; wherein the carrier gas is Hz, wherein the first precursor is HCl, the Group II/III element comprises at least one of Zn, Cd, Hg, Al, Ga, and In; and wherein the second precursor is one of AsH.sub.3 (arsine), PH.sub.3 (phosphine), H.sub.2Se (hydrogen selenide), H.sub.2Te (hydrogen telluride), SbH.sub.3 (hydrogen antimonide), H.sub.2S (hydrogen sulfide), and NH.sub.3 (ammonia). The process may be an HVPE (hydride vapor phase epitaxy) process.

A METHOD OF CONTROLLED N-DOPING OF GROUP III-V MATERIALS GROWN ON (111) SI
20220259758 · 2022-08-18 · ·

The present invention is related to a method of providing n-doped group III-V materials grown on (111) Si, and especially to a method comprising steps of growth of group III-V materials interleaved with steps of no growth, wherein both growth steps and no growth steps are subject to a constant uninterrupted arsenic flux concentration.

Nanowire with reduced defects

A nanowire structure includes a substrate, a patterned mask layer on the substrate, and a nanowire. The patterned mask layer is on the substrate and includes an opening through which the substrate is exposed. The nanowire is on the substrate in the opening of the patterned mask layer. The nanowire includes a buffer layer on the substrate, a defect filtering layer on the buffer layer, and an active layer on the defect filtering layer. The defect filtering layer is a strained layer. By providing the defect filtering layer between the buffer layer and the active layer of the nanowire, defects present in the buffer layer can be prevented from propagating into the active layer. Accordingly, defects in the active layer of the nanowire are reduced, thereby improving the performance of the nanowire structure.