H01L21/02532

SOURCE/DRAIN CONTACTS FOR NON-PLANAR TRANSISTORS

The present description relates to the field of fabricating microelectronic devices having non-planar transistors. Embodiments of the present description relate to the formation of source/drain contacts within non-planar transistors, wherein a titanium-containing contact interface may be used in the formation of the source/drain contact with a discreet titanium silicide formed between the titanium-containing interface and a silicon-containing source/drain structure.

VERTICALLY INTEGRATED SEMICONDUCTOR DEVICE
20230238285 · 2023-07-27 ·

Embodiments of present invention provide a semiconductor device. The semiconductor device includes a silicon (Si) substrate containing a set of short channel field-effect-transistors (FETs); a germanium (Ge) layer on top of the Si substrate containing a set of long channel p-type FETs (PFETs); and an oxide semiconductor layer on top of the Ge layer containing a set of long channel n-type FETs (NFETs), wherein the set of short channel FETs, long channel PFETs, and long channel NFETs are interconnected through a set of far-back-end-of-line (FBEOL) layers.

METHOD FOR MANUFACTURING EPITAXIAL WAFER AND EPITAXIAL WAFER

A method for manufacturing an epitaxial wafer by forming a single crystal silicon layer on a wafer containing a group IV element including silicon, the method including the steps of: removing a natural oxide film on a surface of the wafer containing the group IV element including silicon in an atmosphere containing hydrogen; forming an oxygen atomic layer by oxidizing the wafer after removing the natural oxide film; and forming a single crystal silicon by epitaxial growth on the surface of the wafer after forming the oxygen atomic layer, where a planar density of oxygen in the oxygen atomic layer is set to 4×10.sup.14 atoms/cm.sup.2 or less. A method for manufacturing an epitaxial wafer having an epitaxial layer of good-quality single crystal silicon while also allowing the introduction of an oxygen atomic layer in an epitaxial layer stably and simply.

POLYCRYSTALLINE FILM, METHOD FOR FORMING POLYCRYSTALLINE FILM, LASER CRYSTALLIZATION DEVICE AND SEMICONDUCTOR DEVICE

The present invention provides a microstructure in which evenly distributed crystal grains line up in parallel lines extending along the surface of the film, and a no-lateral-growth region left at each of locations exposed to both ends of a grain interface, which serves as a partition between the neighboring two crystal grains. According to the present invention, there are also provided: a method for forming a polycrystalline film, such as a thin polycrystalline silicon film, a thin aluminum film, and a thin copper film, which is flat and even, in surface, electrically uniform and stable, and mechanically stable; a laser crystallization device for use in manufacture of polycrystalline films, and a semiconductor device using the polycrystalline film and having good electrical property and increased breakdown voltage.

Adjusting the Profile of Source/Drain Regions to Reduce Leakage

A method includes forming a protruding semiconductor stack including a plurality of sacrificial layers and a plurality of nanostructures, with the plurality of sacrificial layers and the plurality of nanostructures being laid out alternatingly. The method further includes forming a dummy gate structure on the protruding semiconductor stack, etching the protruding semiconductor stack to form a source/drain recess, and forming a source/drain region in the source/drain recess. The formation of the source/drain region includes growing first epitaxial layers. The first epitaxial layers are grown on sidewalls of the plurality of nanostructures, and a cross-section of each of the first epitaxial layers has a quadrilateral shape. The first epitaxial layers have a first dopant concentration. The formation of the source/drain region further includes growing a second epitaxial layer on the first epitaxial layers. The second epitaxial layer has a second dopant concentration higher than the first dopant concentration.

FIELD EFFECT TRANSISTORS COMPRISING A MATRIX OF GATE-ALL-AROUND CHANNELS
20230027293 · 2023-01-26 ·

Provided is a semiconductor structure with shared gated devices. The semiconductor structure comprises a substrate and a bottom dielectric isolation (BDI) layer on top of the substrate. The structure further comprises a pFET region that includes a p-doped Source-Drain epitaxy material and a first nanowire matrix above the BDI layer. The structure further comprises an nFET region that includes a n-doped Source-Drain epitaxy material and a second nanowire matrix above the BDI layer. The structure further comprises a conductive gate material on top of a portion of the first nanowire matrix and the second nanowire matrix. The structure further comprises a vertical dielectric pillar separating the pFET region and the nFET region. The vertical dielectric pillar extends downward through the BDI layer into the substrate. The vertical dielectric pillar further extends upward through the conductive gate material to a dielectric located above the gate region.

FILM DEPOSITION METHOD AND ELEMENT INCLUDING FILM DEPOSITED BY THE FILM DEPOSITION METHOD

A film deposition method may include preparing a non-planar substrate including a first surface, a second surface, and an inclined surface between the first surface and the second surface; depositing a film having a thickness deviation on the first surface, the second surface, and the inclined surface; and etching the film deposited on the first surface, the second surface, and the inclined surface. A height of the second surface may be different than a height of the first surface.

Semiconductor Device and Method of Forming Same
20230028653 · 2023-01-26 ·

A method includes depositing a first semiconductor layer and a second semiconductor layer over a substrate; patterning the first semiconductor layer, the second semiconductor layer, and the substrate to form a first nanostructure, a second nanostructure, and a semiconductor fin; forming a recess in the first nanostructure and the second nanostructure, the recess exposing the semiconductor fin; epitaxially growing a first layer in the recess, a first portion of the first layer being disposed along a first sidewall of the first nanostructure, a second portion of the first layer being disposed along the semiconductor fin, the first portion of the first layer comprising two sidewalls extending toward a middle of the recess, the first portion of the first layer further comprising a first surface most distal from the first sidewall and directly interposed between the two sidewalls, the first portion being physically separated from the second portion; and epitaxially growing a second layer over the first portion of the first layer and over the second portion of the first layer, the second layer physically connecting the first portion of the first layer to the second portion of the first layer.

METHODS OF FORMATION OF A SIGE/SI SUPERLATTICE

A method and apparatus for forming a super-lattice structure on a substrate is described herein. The super-lattice structure includes a plurality of silicon-germanium layers and a plurality of silicon layers disposed in a stacked pattern. The methods described herein produce a super-lattice structure with transition width of less than about 1.4 nm between each of the silicon-germanium layers and an adjacent silicon layer. The methods described herein include flowing one or a combination of a silicon containing gas, a germanium containing gas, and a halogenated species.

METHOD OF MANUFACTURING A SEMICONDUCTOR DEVICE AND A SEMICONDUCTOR DEVICE
20230023936 · 2023-01-26 ·

In a method of manufacturing a semiconductor device, a first fin structure, a second fin structure, a first wall fin structure and a second wall fin structure are formed over a substrate. The first and second fin structures are disposed between the first and second wall fin structures, and lower portions of the first and second fin structures and the first and second wall fin structures are embedded in the isolation insulating layer and upper portions thereof are exposed from the isolation insulating layer. A sidewall spacer layer is formed on sidewalls of the first and second fin structures. Source/drain regions of the first and second fin structures are recessed. An epitaxial source/drain structure is formed over the recessed first and second fin structures. A width W1 of the first and second fin structures is smaller than a thickness W2 of the sidewall spacer layer.