H01L21/02581
LIGHT EMITTING DEVICE AND METHOD OF MANUFACTURING THE SAME
A light emitting device, includes a selective growth mask layer 44; a first light reflection layer 41 thinner than the selective growth mask layer 44; a laminated structure including a first compound semiconductor layer 21, an active layer 23, and a second compound semiconductor layer 22, the first compound semiconductor layer 21 being formed on the first light reflection layer 41; and a second electrode 32 formed on the second compound semiconductor layer 22, and a second light reflection layer 42, in which the second light reflection layer 42 is opposed to the first light reflection layer 41, and the second light reflection layer is not formed on an upper side of the selective growth mask layer 44.
GAN CRYSTAL AND GAN SUBSTRATE
Provided are: a GaN crystal used in a substrate for a nitride semiconductor device having a horizontal device structure, such as a GaN-HEMT; and a GaN substrate used for the production of a nitride semiconductor device having a horizontal device structure, such as a GaN-HEMT. The GaN crystal and the GaN substrate each include a surface having an inclination of 10° or less from a (0001) crystal plane and an area of 5 cm.sup.2 or more, and have an Mn concentration of 1.0 × 10.sup.16 atoms/cm.sup.3 or higher but lower than 1.0 × 10.sup.19 atoms/cm.sup.3 and a total donor impurity concentration of lower than 5.0 × 10.sup.16 atoms/cm.sup.3.
Composition And Method For Making Picocrystalline Artificial Borane Atoms
Materials containing picocrystalline quantum dots that form artificial atoms are disclosed. The picocrystalline quantum dots (in the form of born icosahedra with a nearly-symmetrical nuclear configuration) can replace corner silicon atoms in a structure that demonstrates both short range and long-range order as determined by x-ray diffraction of actual samples. A novel class of boron-rich compositions that self-assemble from boron, silicon, hydrogen and, optionally, oxygen is also disclosed. The preferred stoichiometric range for the compositions is (B.sub.12H.sub.w).sub.xSi.sub.yO.sub.z with 3≤w≤5, 2≤x≤4, 2≤y≤5 and 0≤z≤3. By varying oxygen content and the presence or absence of a significant impurity such as gold, unique electrical devices can be constructed that improve upon and are compatible with current semiconductor technology.
Doped Diamond SemiConductor and Method of Manufacture Using Laser Abalation
A doped diamond semiconductor and method of production using a laser is disclosed herein. As disclosed, a dopant and/or a diamond or sapphire seed material may be added to a graphite based ablative layer positioned below a confinement layer, the ablative layer also being graphite based and positioned above a backing layer, to promote formation of diamond particles having desirable semiconductor properties via the action of a laser beam upon the ablative layer. Dopants may be incorporated into the process to activate the reaction sought to produce a material useful in production of a doped semiconductor or a doped conductor suitable for the purpose of modulating the electrical, thermal or quantum properties of the material produced. As disclosed, the diamond particles formed by either the machine or method of confined pulsed laser deposition disclosed may be arranged as semiconductors, electrical components, thermal components, quantum components and/or integrated circuits.
Oxide semiconductor thin-film and thin-film transistor consisted thereof
The present application discloses an oxide semiconductor thin-film and a thin-film transistor consisted thereof. The oxide semiconductor thin-film is fabricated by doping a certain amount of rare-earth oxide (RO) as light stabilizer to metal oxide (MO) semiconductor. The thin-film transistor comprising a gate electrode, a channel layer consisted by the oxide semiconductor thin-film, a source and drain electrode; the thin-film transistor employing etch-stop structure, a back-channel etch structure or a top-gate self-alignment structure.
GROUP IIIA NITRIDE GROWTH SYSTEM AND METHOD
A system and method for growing a gallium nitride (GaN) structure that includes providing a template; and growing at least a first GaN layer on the template using a first sputtering process, wherein the first sputtering process includes: controlling a temperature of a sputtering target, and modulating between a gallium-rich condition and a gallium-lean condition, wherein the gallium-rich condition includes a gallium-to-nitrogen ratio having a first value that is greater than 1, and wherein the gallium-lean condition includes the gallium-to-nitrogen ratio having a second value that is less than the first value. Some embodiments include a load lock configured to load a substrate wafer into the system and remove the GaN structure from the system; and a plurality of deposition chambers, wherein the plurality of deposition chambers includes a GaN-deposition chamber configured to grow at least the first GaN layer on a template that includes the substrate wafer.
EPITAXIAL STRUCTURE OF SEMICONDUCTOR DEVICE AND METHOD OF MANUFACTURING THE SAME
Embodiments of the present disclosure provide an epitaxial structure of a semiconductor device and a method of manufacturing the same. The epitaxial structure includes a substrate, and an epitaxial layer located on a side of the substrate, the epitaxial layer including a nucleation layer located on a side of the substrate and a buffer layer located on a side of the nucleation layer away from the substrate, wherein a thickness of the buffer layer is inversely proportional to a thickness of the nucleation layer.
VANADIUM OXIDE FILM AND PROCESS FOR PRODUCING SAME
Provided is a vanadium oxide film which shows substantially no hysteresis of resistivity changes due to temperature rising/falling, has a low resistivity at room temperature, has a large absolute value of the temperature coefficient of resistance, and shows semiconductor-like resistance changes in a wide temperature range. In the vanadium oxide film, a portion of the vanadium has been replaced by aluminum and copper, and the amount of substance of aluminum is 10 mol % based on the sum total of the amount of substance of vanadium, the amount of substance of aluminum, and the amount of substance of copper. This vanadium oxide film has a low resistivity, has a large absolute value of the temperature coefficient of resistance, and shows substantially no hysteresis of resistivity changes due to temperature rising/falling. This vanadium oxide film is produced by applying a mixture solution containing a vanadium organic compound, an aluminum organic compound, and a copper organic compound to a substrate, calcining the substrate at a temperature lower than the temperature at which the substrate decomposes, and irradiating the surface of the substrate onto which the mixture solution has been applied with ultraviolet light.
SEMICONDUCTOR ELEMENT AND CRYSTALLINE LAMINATE STRUCTURE
A semiconductor element includes a high-resistivity substrate that includes a β-Ga.sub.2O.sub.3-based single crystal including an acceptor impurity, a buffer layer on the high-resistivity substrate, the buffer layer including a β-Ga.sub.2O.sub.3-based single crystal, and a channel layer on the buffer layer, the channel layer including a β-Ga.sub.2O.sub.3-based single crystal including a donor impurity. A crystalline laminate structure includes a high-resistivity substrate that includes a β-Ga.sub.2O.sub.3-based single crystal including an acceptor impurity, a buffer layer on the high-resistivity substrate, the buffer layer including a β-Ga.sub.2O.sub.3-based single crystal, and a donor impurity-containing layer on the buffer layer, the donor impurity-containing layer including a β-Ga.sub.2O.sub.3-based single crystal including a donor impurity.
MULTILAYER STRUCTURE, METHOD FOR MANUFACTURING SAME, SEMICONDUCTOR DEVICE, AND CRYSTALLINE FILM
A multilayer structure with excellent crystallinity and a semiconductor device of the multilayer structure with good mobility are provided. A multilayer structure includes: a corundum structured crystal substrate; and a crystalline film containing a corundum structured crystalline oxide as a major component, the film formed directly on the substrate or with another layer therebetween, wherein the crystal substrate has an off angle from 0.2° to 12.0°, and the crystalline oxide contains one or more metals selected from indium, aluminum, and gallium.