H01L21/28537
Schottky barrier diode with reduced leakage current and method of forming the same
A method of manufacturing a Schottky barrier diode includes: forming a first well region over a substrate; forming a first dielectric layer over the first well region; patterning the first dielectric layer by reducing a first thickness of the first dielectric layer; removing the first dielectric layer to expose a surface of the first well region; and forming a conductive layer over the first well region to obtain a Schottky barrier interface. A Schottky barrier diode manufactured based on the above method is also provided.
METHODS OF FORMING DOPED SILICIDE POWER DEVICES
Exemplary methods of forming a semiconductor structure may include forming a layer of metal on a semiconductor substrate. The layer of metal may extend along a first surface of the semiconductor substrate. The semiconductor substrate may be or include silicon. The methods may include performing an anneal to produce a metal silicide. The methods may include implanting ions in the metal silicide to increase a barrier height over 0.65 V.
Method for manufacturing a grid
A grid is manufactured with a combination of ion implant and epitaxy growth. The grid structure is made in a SiC semiconductor material with the steps of a) providing a substrate comprising a doped semiconductor SiC material, said substrate comprising a first layer (n1), b) by epitaxial growth adding at least one doped semiconductor SiC material to form separated second regions (p2) on the first layer (n1), if necessary with aid of removing parts of the added semiconductor material to form separated second regions (p2) on the first layer (n1), and c) by ion implantation at least once at a stage selected from the group consisting of directly after step a), and directly after step b); implanting ions in the first layer (n1) to form first regions (p1). It is possible to manufacture a grid with rounded corners as well as an upper part with a high doping level. It is possible to manufacture a component with efficient voltage blocking, high current conduction, low total resistance, high surge current capability, and fast switching.
Methods for LDMOS and other MOS transistors with hybrid contact
A lateral DMOS transistor structure includes a substrate of a first dopant polarity, a body region of the first dopant polarity, a source region, a drift region of a second dopant polarity, a drain region, a channel region, a gate structure over the channel region, a hybrid contact implant, of the second dopant polarity, in the source region, and a respective metal contact on or within each of the source region, gate structure, and drain region. The hybrid contact implant and the metal contact together form a hybrid contact defining first, second, and third electrical junctions. The first junction is a Schottky junction formed vertically between the source metal contact and the body. The second junction is an ohmic junction formed laterally between the source metal contact and the hybrid contact implant. The third junction is a rectifying PN junction between the hybrid contact implant and the channel region.
Methods of forming microelectronic devices
A microelectronic device comprises a stack structure, cell pillar structures, an active body structure, digit line structures, and control logic devices. The stack structure comprises vertically neighboring tiers, each of the vertically neighboring tiers comprising a conductive structure and an insulative structure vertically neighboring the conductive structure. The cell pillar structures vertically extend through the stack structure and each comprise a channel material and an outer material stack horizontally interposed between the channel material and the stack structure. The active body structure vertically overlies the stack structure and is in contact with the channel material of the cell pillar structures. The active body structure comprises a metal material having a work function greater than or equal to about 4.7 electronvolts. The digit line structures vertically underlie the stack structure and are coupled to the cell pillar structures. Memory devices, electronic systems, and methods of forming a microelectronic device are also described.
Junction barrier Schottky diode device and method for fabricating the same
A method for fabricating a junction barrier Schottky diode device is disclosed. The junction barrier Schottky device includes an N-type semiconductor layer, a plurality of first P-type doped areas, a plurality of second P-type doped areas, and a conductive metal layer. The first P-type doped areas and the second P-type doped are formed in the N-type semiconductor layer. The second P-type doped areas are self-alignedly formed above the first P-type doped areas. The spacing between every neighboring two of the second P-type doped areas is larger than the spacing between every neighboring two of the first P-type doped areas. The conductive metal layer, formed on the N-type semiconductor layer, covers the first P-type doped areas and the second P-type doped areas.
Method for reducing Schottky barrier height and semiconductor device with reduced Schottky barrier height
A method for controlling Schottky barrier height in a semiconductor device includes forming an alloy layer including at least a first element and a second element on a first surface of a semiconductor substrate. The semiconductor substrate is a first element-based semiconductor substrate, and the first element and the second element are Group IV elements. A first thermal anneal of the alloy layer and the first element-based substrate is performed. The first thermal anneal causes the second element in the alloy layer to migrate towards a surface of the alloy layer. A Schottky contact layer is formed on the alloy layer after the first thermal anneal.
Vertical Trench Device Configurations for Radiation-Environment Applications
Semiconductor devices and associated fabrication methods are disclosed. In one disclosed approach a process for forming a semiconductor device is provided. The process includes: implanting a first region of semiconductor material using a first channeled implant with a first conductivity type; and implanting, after the first channeled implant, a second region of semiconductor material using a second channeled implant with a second conductivity type. The first channeled implant disrupts a crystal structure of the first region of semiconductor material and does not disrupt a crystal structure of the second region of semiconductor material.
METHOD FOR REDUCING SCHOTTKY BARRIER HEIGHT AND SEMICONDUCTOR DEVICE WITH REDUCED SCHOTTKY BARRIER HEIGHT
A method for controlling Schottky barrier height in a semiconductor device includes forming an alloy layer including at least a first element and a second element on a first surface of a semiconductor substrate. The semiconductor substrate is a first element-based semiconductor substrate, and the first element and the second element are Group IV elements. A first thermal anneal of the alloy layer and the first element-based substrate is performed. The first thermal anneal causes the second element in the alloy layer to migrate towards a surface of the alloy layer. A Schottky contact layer is formed on the alloy layer after the first thermal anneal.
JUNCTION BARRIER SCHOTTKY DIODE DEVICE AND METHOD FOR FABRICATING THE SAME
A method for fabricating a junction barrier Schottky diode device is disclosed. The junction barrier Schottky device includes an N-type semiconductor layer, a plurality of first P-type doped areas, a plurality of second P-type doped areas, and a conductive metal layer. The first P-type doped areas and the second P-type doped are formed in the N-type semiconductor layer. The second P-type doped areas are self-alignedly formed above the first P-type doped areas. The spacing between every neighboring two of the second P-type doped areas is larger than the spacing between every neighboring two of the first P-type doped areas. The conductive metal layer, formed on the N-type semiconductor layer, covers the first P-type doped areas and the second P-type doped areas.