Y10T428/249924

Electrostatic-assisted fiber spinning method and production of highly aligned and packed hollow fiber assembly and membrane

The invention provides a highly aligned and closely packed hollow fiber assembly, wherein the assemblies of fibrous membrane has a width-to-fiber diameter ratio (W/d) larger than 10 and the orientation of the fibers is no larger than +/10. Also provided is an electrospinning process for the preparation of the fiber assembly of the invention and its applications.

Fibrous structures and methods for making same

Fibrous structures that exhibit a pore volume distribution such that at least 25% and/or at least 43% of the total pore volume present in the fibrous structures exists in pores of radii of from 91 m to 140 m, and to methods for making such fibrous structures are provided.

SYSTEMS AND METHODS FOR GROWTH OF NANOSTRUCTURES ON SUBSTRATES, INCLUDING SUBSTRATES COMPRISING FIBERS

Systems and methods for the formation of nanostructures, including carbon-based nanostructures, are generally described. In certain embodiments, substrate configurations and associated methods are described.

Composite non-woven fibrous webs having continuous particulate phase and methods of making and using the same

The disclosure relates to composite nonwoven fibrous web including an embedded phase having a population of particulates forming a substantially continuous three-dimensional network, and a matrix phase comprising a population of fibers forming a three-dimensional network around the particulates. The disclosure also relates to methods of making a composite nonwoven fibrous web including forming an embedded phase having a population of particulates in a substantially continuous three-dimensional network, and forming a matrix phase comprising a population of fibers forming a three-dimensional network around the particulates. Articles made from a composite nonwoven fibrous web prepared according to the methods as described above are also disclosed. In exemplary embodiments, the articles may include gas filtration articles, liquid filtration articles, sound absorption articles, surface cleaning articles, cellular growth support articles, drug delivery articles, personal hygiene articles, and wound dressing articles.

Conductive flooring material and a production method therefor
09677286 · 2017-06-13 · ·

The present invention relates to a conductive flooring material containing a conductive deformation-preventing layer containing conductive fibers comprising glass fibers and carbon fibers, and to a production method therefor. The present invention can provide a conductive material which is useful not only in the form of tiles but also in the form of long sheets because the conductive fibers comprise glass fiber and carbon fiber impart not only outstanding electrical conductivity but also stable deformation-preventing properties.

Chemical oxygen generator

A chemical oxygen generator with enhanced structural integrity. In some embodiments, the chemical core of the chemical oxygen generator is reinforced with one or more reinforcing structures that are integral with the core. In some embodiments, as the core burns, the one or more reinforcing structures become fused with the core.

Method of making polyimide fiber assembly
09617669 · 2017-04-11 · ·

A polyimide fiber assembly of the present invention includes polyimide fibers having curved shapes with an average fiber diameter falling within a range of greater than 1 m to not greater than 100 m, the polyimide fiber assembly having a bulk density falling within a range of not less than 1 kg/m.sup.3 to not greater than 30 kg/m.sup.3. This makes it possible to realize a polyimide fiber assembly that is both excellent in thermal insulation performance and sound absorbency and light in weight. The polyimide fiber assembly of the present invention can be obtained by a production method comprising the steps of: (i) discharging a polymeric resin solution obtained by dissolving polyamic acid or polyimide in an organic solvent; and (ii) using external force to cause the polymeric resin solution thus discharged to fly in a direction of the external force, the external force being external force of gas from a direction intersecting with a discharge direction in which the polymeric resin solution is discharged, and then forming a polymeric resin into fibers by spinning while vaporizing the organic solvent contained in the polymeric resin solution.

METHOD AND APPARATUS FOR TREATING BONE FRACTURES, AND/OR FOR FORTIFYING AND/OR AUGMENTING BONE, INCLUDING THE PROVISION AND USE OF COMPOSITE IMPLANTS

A composite implant comprising an injectable matrix material which is flowable and settable, and at least one reinforcing element for integration with the injectable matrix material, the at least one reinforcing element adding sufficient strength to the injectable matrix material such that when the composite implant is disposed in a cavity in a bone, the composite implant supports the bone.

A method for treating a bone, the method comprising: selecting at least one reinforcing element to be combined with an injectable matrix material so as to together form a composite implant capable of supporting the bone; positioning the at least one reinforcing element in a cavity in the bone; flowing the injectable matrix material into the cavity in the bone so that the injectable matrix material interfaces with the at least one reinforcing element; and transforming the injectable matrix material from a flowable state to a non-flowable state so as to establish a static structure for the composite implant, such that the composite implant supports the adjacent bone.

ULTRA-LOW REFLECTANCE BROADBAND OMNI-DIRECTIONAL ANTI-REFLECTION COATING

An anti-reflection coating has an average total reflectance of less than 10%, for example less than 5.9% such as from 4.9% to 5.9%, over a spectrum of wavelengths of 400-1100 nm and a range of angles of incidence of 0-90 degrees with respect to a surface normal of the anti-reflection coating. An anti-reflection coating has a total reflectance of less than 10%, for example less than 6% such as less than 4%, over an entire spectrum of wavelengths of 400-1600 nm and an entire range of angles of incidence of 0-70 degrees with respect to a surface normal of the anti-reflection coating.

Composite structures having improved heat aging and interlayer bond strength

Disclosed herein are composite structures having improved heat aging and interlayer adhesion properties, processes for making them, and end use articles. The composite structures comprise a second component overmolded onto a first component and wherein the surface of the first and optionally of second component comprise a copper based heat stabilizer thereby providing superior bond strength between components compared to polyhydric alcohol based heat stabilizers.