Y10T428/24926
ARTICLES WITH A LOW-ELASTIC MODULUS LAYER AND RETAINED STRENGTH
One or more aspects of the disclosure pertain to an article including a film disposed on a glass substrate, which may be strengthened, where the interface between the film and the glass substrate is modified, such that the article has an improved average flexural strength, and the film retains key functional properties for its application. Some key functional properties of the film include optical, electrical and/or mechanical properties. The bridging of a crack from one of the film or the glass substrate into the other of the film or the glass substrate can be suppressed by inserting a nanoporous crack mitigating layer between the glass substrate and the film.
GLASS ARTICLES WITH LOW-FRICTION COATINGS
Coated pharmaceutical packages may comprise a glass body formed from a borosilicate glass composition having a Type 1 chemical durability according to USP 660, the glass body having an interior surface and an exterior surface and a wall extending therebetween. A low-friction thermally stable coating having a thickness of ≤1 μm may be positioned on at least a portion of the exterior surface. The low-friction coating may comprise a silane. The portion of the exterior surface of the coated pharmaceutical package may have a coefficient of friction that is at least 20% less than an uncoated pharmaceutical package formed from the same borosilicate glass composition.
Laminated glazing
A laminated glazing including a first glass sheet and a second glass sheet laminated via at least one thermoplastic interlayer, and an optical sensor arranged on the inner face of the laminated glazing. The thermoplastic interlayer includes a zone that is opaque to visible wavelengths and that extends at least in the zone surrounding the optical sensor.
Glass articles with low-friction coatings
Coated pharmaceutical packages are disclosed. The coated pharmaceutical packages may include a glass body comprising a first surface and a second surface opposite the first surface. The glass body may be a glass container formed from a borosilicate glass composition and the first surface is an exterior surface of the glass container. A low-friction coating may be positioned on at least a portion of the first surface of the glass body. In embodiments, the low-friction coating may be a fluoropolymer.
Glass articles with low-friction coatings
Coated glass pharmaceutical packages are disclosed. According to embodiments, a coated glass pharmaceutical package may include a glass container formed from one of a borosilicate glass composition that meets Type 1 criteria according to USP <660> or an alkali aluminosilicate glass having a Class HGA 1 hydrolytic resistance when tested according to the ISO 720-1985 testing standard. A low-friction coating may be bonded to the exterior surface of the glass container. The low-friction coating may include a polymer. The exterior surface of the glass container with the low-friction coating may have a coefficient of friction of less than or equal to 0.7. The coated glass pharmaceutical package may be thermally stable after depyrogenation in air at a temperature of at least about 260° C. for 30 minutes.
ARTICLES WITH PATTERNED COATINGS
Embodiments of a article including include a substrate and a patterned coating are provided. In one or more embodiments, when a strain is applied to the article, the article exhibits a failure strain of 0.5% or greater. Patterned coating may include a particulate coating or may include a discontinuous coating. The patterned coating of some embodiments may cover about 20% to about 75% of the surface area of the substrate. Methods for forming such articles are also provided.
Methods for forming ceramic matrix composite structures
Methods of forming ceramic matrix composite structures include joining at least two lamina together to form a flexible ceramic matrix composite structure. Ceramic matrix composite structures include at least one region of reduced inter-laminar bonding at a selected location between lamina thereof. Thermal protection systems include at least one seal comprising a ceramic matrix composite material and have at least one region of reduced inter-laminar bonding at a selected location between lamina used to form the seal. Methods of forming thermal protection systems include providing one or more such seals between adjacent panels of a thermal protection system.
Polymer coatings
The present disclosure relates to polymer coatings covalently attached to the surface of a substrate and the preparation of the polymer coatings, such as poly(N-(5-azidoacetamidylpentyl)acrylamide-co-acrylamide) (PAZAM), in the formation and manipulation of substrates, such as molecular arrays and flow cells. The present disclosure also relates to methods of preparing a substrate surface by using beads coated with a covalently attached polymer, such as PAZAM, and the method of determining a nucleotide sequence of a polynucleotide attached to a substrate surface described herein.
Method for producing a structured coating on a substrate, coated substrate, and semi-finished product having a coated substrate
The invention relates to a method for producing a structured coating on a substrate, wherein the method comprises the following steps: providing a substrate having a surface to be coated and producing a structured coating on the surface of the substrate to be coated by depositing at least one evaporation coating material, namely aluminium oxide, silicon dioxide, silicon nitride, or titanium dioxide, on the surface of the substrate to be coated by means of thermal evaporation of the at least one evaporation coating material and using additive structuring. The invention further relates to a coated substrate and a semi-finished product having a coated substrate.
Articles having retained strength
One or more aspects of the disclosure pertain to an article including a film disposed on a glass substrate, which may be strengthened, where the interface between the film and the glass substrate is modified, such that the article retains its average flexural strength, and the film retains key functional properties for its application. Some key functional properties of the film include optical, electrical and/or mechanical properties. The bridging of a crack from one of the film or the glass substrate into the other of the film or the glass substrate can be prevented by inserting a crack mitigating layer between the glass substrate and the film.