Y10T428/2495
Thermal barrier coating
A coated substrate has a substrate and a coating system having one or more ceramic layers. At least a first layer of one of the one or more ceramic layers is a columnar layer having as-deposited columns and intercolumn gaps. The intercolumn gaps have a mean width at least one of: at least 4.0 micrometers; and at least 1.5% of a thickness of said first layer.
Protective cover, protective cover package comprising same, and electronic device comprising protective cover
Various embodiments described herein disclose a protective cover of an electronic device, a protective cover package including the protective cover, and an electronic device to which the protective cover is applied. The protective cover includes a first protective layer including a flat region and a curved region and having a specified transparency, the curved region being disposed at an edge of the flat region and having a specified curvature, a second protective layer disposed below the first protective layer, the second protective layer being thicker than the first protective layer by a specified thickness or more, a bonding layer for bonding the first protective layer and the second protective layer, and an adhesive layer disposed below the second protective layer, wherein the first protective layer is thicker than the second protective layer. Various embodiments are possible.
Surface-treated steel sheet for cell container
A surface-treated steel sheet for a battery container includes a steel sheet, an iron-nickel diffusion layer formed on the steel sheet, and a nickel layer formed on the iron-nickel diffusion layer and constituting the outermost layer. When the Fe intensity and the Ni intensity are continuously measured from the surface of the surface-treated steel sheet for a battery container along the depth direction with a high frequency glow discharge optical emission spectrometric analyzer, the thickness of the iron-nickel diffusion layer being the difference (D2−D1) between the depth (D1) at which the Fe intensity exhibits a first predetermined value and the depth (D2) at which the Ni intensity exhibits a second predetermined value is 0.04 to 0.31 μm; and the total amount of the nickel contained in the iron-nickel diffusion layer and the nickel contained in the nickel layer is 10.8 to 26.7 g/m2.
Stabilized metal monolayer structure
A stabilized elementary metal structure is disclosed. The stabilized elementary metal structure may include an elementary metal having at least one layer and having a two-dimensional layer structure, and an organic molecular layer provided on at least one of a top surface and a bottom surface of the elementary metal.
Panel and Method for Producing a Panel
The invention relates to a panel and a method for producing a panel. The panel is in particular a floor, wall or ceiling panel, and comprises at least one core layer, the core layer comprising an upper core surface and a lower core surface and at least one pair of opposite side edges; wherein the core layer comprises magnesium oxide cement; wherein the core has a density which is substantially homogenous over its entire volume, and wherein at least one decorative top layer is attached to an upper core surface of the core layer.
Cobalt chemistry for smooth topology
An electroplated cobalt deposit and a method of electrodepositing cobalt on a surface to produce a level deposit across the surface of the substrate. The cobalt electrolyte contains (1) a source of cobalt ions; (2) boric acid; (3) a pH adjuster; and (4) an organic additive, which contains a suppressor. The electroplated cobalt deposit exhibits a level surface such that the thickness difference across substantially the entire surface of the substrate of less than about 200 nm.
Hybrid side rail assemblies and mattresses including the same
A side rail assembly and a mattress assembly including the side rail assembly about at least a portion of a perimeter of the mattress assembly. The side rail assembly includes a laminate structure including one or more foam layers and one or more fiber layers in a stacked arrangement. The fiber layer can be a non-woven layer.
Composite coating and fabrication method thereof
The present disclosure provides a composite coating and a method for fabricating the composite coating. The composite coating comprises a polymer layer, a metal interlayer and an amorphous metal coating. The polymer layer is formed on a substrate and acts as a diffusion barrier layer, which is thick and dense enough to prevent the corrosive substances from penetrating into the substrate. The metal interlayer is formed between the polymer layer and the amorphous metal coating for improving the adhesion of the amorphous metal coating to the substrate.
ALUMINIUM AND MAGNESIUM COATED PART ASSEMBLY
A part assembly (100), comprising: an aluminium part (101); a magnesium part (102), the magnesium part (102) coated in a first coating (104); a bond (103), the bond (103) securing the aluminium part (101) to the coated magnesium part (114); wherein the aluminium part (101), the coated magnesium part (114) and the bond (103) are subjected to an electrophoresis coating process to coat the aluminium part (101) in a second coating (105). By subjecting the aluminium part (101), the coated magnesium part (114) and the bond (103) to an electrophoresis coating process to coat the aluminium part (101) in a second coating (105) this may provide a simpler manufacturing process.
Surface-treated steel plate for cell container
A surface-treated steel sheet for a battery container, including a steel sheet, an iron-nickel diffusion layer formed on the steel sheet, and a nickel layer formed on the iron-nickel diffusion layer (and constituting the outermost layer, wherein when the Fe intensity and the Ni intensity are continuously measured from the surface of the surface-treated steel sheet for a battery container along the depth direction with a high frequency glow discharge optical emission spectrometric analyzer, the thickness of the iron-nickel diffusion layer being the difference between the depth at which the Fe intensity exhibits a first predetermined value and the depth at which the Ni intensity exhibits a second predetermined value is 0.04 to 0.31 μm; and the total amount of the nickel contained in the iron-nickel diffusion layer and the nickel contained in the nickel layer is 4.4 g/m.sup.2 or more and less than 10.8 g/m.sup.2.