B01D2325/22

Porous hollow fiber membrane

The present invention provides a porous hollow fiber membrane that has both high strength and high pure water permeability, and that exhibits excellent thermal deformation resistance. The present invention is related to a porous hollow fiber membrane containing a fluororesin-based polymer, and a manufacturing method of the membrane comprises a drawing step and a relaxing step. The porous hollow fiber membrane is characterized in that: the molecular chain of the polymer is oriented in the longitudinal direction of the hollow fiber membrane; and at the same time internal distortion of oriented non-crystalline chains, which is disadvantageous in terms of entropy, is alleviated.

POLYMER COMPOSITE FILM, PREPARATION METHOD THEREFOR, AND LITHIUM-ION BATTERY
20190326577 · 2019-10-24 · ·

A polymer composite membrane, a method for fabricating same, and a lithium-ion battery including same are provided. The polymer composite membrane includes a porous base membrane and a heat-resistant layer covering at least one side surface of the porous base membrane, the heat-resistant layer includes a plurality of heat-resistant sub-layers sequentially stacked, and pore-blocking temperatures of the heat-resistant sub-layers are sequentially increased from inside to outside; each of the heat-resistant sub-layers includes at least one of a first heat-resistant polymer material and a second heat-resistant polymer material, and each of the heat-resistant sub-layers is separately configured as a fiber network structure; the melting point of the first heat-resistant polymer material is not less than 200 C.; and the melting point of the second heat-resistant polymer material is not less than 100 C.

Carbon-containing membrane for water and gas separation

The invention relates to a multilayer metallic or ceramic membrane device, comprising a macroporous carrier layer including pores having a pore diameter of more than 50 nm, and at least one mesoporous intermediate layer disposed thereon, including pores having a pore diameter of 2 nm to 50 nm. The membrane device according to the invention furthermore comprises at least one microporous cover layer disposed on the mesoporous intermediate layer, including pores having an average pore diameter of 0.3 nm to 1.5 nm, comprising graphite oxide or few-layer graphene oxide or graphite or few-layer graphene. In an advantageous embodiment, the cover layer comprises between 5 and 1000 layers of graphene oxide. In an advantageous embodiment, the cover layer can comprise between 5 and 1000 layers of partially reduced graphene oxide or graphene as a result of the at least partial reduction of the graphene oxide. The multilayer, chemically and mechanically stable and temperature-resistant membrane device according to the invention, comprising the functional cover layer thereof including microporous graphene oxide or graphene, is advantageously suitable for use in water separation or purification, or for gas separation.

FLUORINATED FILTER MEMBRANE, FILTERS, AND METHODS
20190282961 · 2019-09-19 ·

Described are filtration membranes that include a porous fluoropolymer membrane and thermally stable ionic groups; filters and filter components that include these filtration membranes; methods of making the filtration membranes, filters, and filter components; and method of using a filtration membrane, filter component, or filter to remove unwanted material from fluid.

NANOPOROUS ULTRA-HIGH MOLECULAR WEIGHT POLYETHYLENE MEMBRANE
20190267594 · 2019-08-29 ·

Methods are provided for producing a biaxially oriented nanoporous UHMWPE membrane. The method can include combining a petroleum jelly, an ultra-high-molecular-weight polyethylene (UHMWPE), and an antioxidant, forming a suspension, feeding the suspension into an extruder to produce a gel filament, pressing the gel filament to form a gel film, subjecting the gel film to an annealing temperature, and extracting the petroleum jelly from the gel film.

HEAT STABILIZED MEMBRANE
20240158589 · 2024-05-16 ·

A dry-process porous membrane having an oxygen induction time (OIT) greater than 3 minutes, greater than 5 minutes, greater than 10 minutes, greater than 15 minutes, greater than 20 minutes, or greater than 25 minutes where OIT is measured at 215? C. and 100% O.sub.2. The dry-process porous membrane may be a microporous polyolefin membrane.

MICROPOROUS MEMBRANE LITHIUM ION SECONDARY BATTERY AND METHOD OF PRODUCING THE MICROPOROUS MEMBRANE
20190252664 · 2019-08-15 ·

A method suppresses membrane thickness variation and air resistance variation after a compression at 60 C. or 80 C. Stretching is performed at least twice in at least different axial directions before the extraction of the solvent, and at the same time, at least one of (i) and (ii) is satisfied. (i) The step (c) is a first stretching step of stretching the sheet-shaped product at least once in a sheet transport direction (MD direction) and at least once in a sheet width direction (TD direction) individually, and the MD stretching magnification and the TD stretching magnification in the step (c) satisfy (TD stretching magnification MD stretching magnification2). (ii) The stretching temperature (T1) of a first axial stretching performed firstly in the step (c) and the maximal stretching temperature (T2) of a second stretching performed after the first axial stretching satisfy (T1T20).

ION EXCHANGE MEMBRANE, METHOD FOR PRODUCING ION EXCHANGE MEMBRANE, AND ELECTROLYZER

[Problem to be solved] To provide an ion exchange membrane, a method for producing an ion exchange membrane, and an electrolyzer that enable a reduction in electrolytic voltage when subjected to electrolysis.

[Solution] An ion exchange membrane including:

a membrane main body including a fluorine-containing polymer having an ion exchange group; and

a coating layer arranged on at least one face of the membrane main body;

wherein the coating layer includes inorganic particles and a binder,

a mass ratio of the binder to the total mass of the inorganic particles and the binder in the coating layer is more than 0.3 and 0.9 or less, and

a surface roughness of the coating layer is 1.20 m or more.

MICROPOROUS MEMBRANE, LITHIUM ION SECONDARY BATTERY AND METHOD OF PRODUCING THE MICROPOROUS MEMBRANE
20190198836 · 2019-06-27 ·

A microporous membrane has average membrane thickness of 15 m or less, and relative impedance A after a heat compression treatment under a pressure of 4.0 MPa at 80 C. for 10 minutes of 140% or less, the relative impedance A being obtained by the equation below: Relative impedance A=(impedance measured at 80 C. after the heat compression treatment)/(impedance measured at room temperature prior to the heat compression treatment)100.

METHOD FOR PREPARATION OF HOLLOW FIBER MEMBRANE DEVICES AND THE USE THEREOF

The invention is directed to preparation of hollow fiber membrane devices that exhibit improved durability and mechanical strength in air separation operations such as generation of nitrogen enriched air on board aircraft. In particular the invention provides for preparation of hollow fiber membrane modules with terminal tubesheets of superior mechanical properties and improved long term durability in air separation operations.