B23K1/06

WIRE BONDING APPARATUS
20180151532 · 2018-05-31 ·

To provide a wire bonding apparatus, which is insusceptible to a bonding state at a second bonding point due to a wire cut error or the like, or to members such as a capillary and a wire, and is capable of automatically protruding the wire from a leading end of the capillary, provided is a wire bonding apparatus including: a capillary (6) having a through hole through which a wire (40) is to be inserted; a holding unit, which is provided above the capillary (6), and is configured to hold the wire (40) inserted through the capillary (6); and a vibrating unit configured to vertically vibrate the capillary (6). Under a state in which the holding unit holds the wire (40), the vibrating unit vertically vibrates the capillary (6) so that the wire (40) is protruded from the leading end of the capillary.

WIRE BONDING APPARATUS
20180151532 · 2018-05-31 ·

To provide a wire bonding apparatus, which is insusceptible to a bonding state at a second bonding point due to a wire cut error or the like, or to members such as a capillary and a wire, and is capable of automatically protruding the wire from a leading end of the capillary, provided is a wire bonding apparatus including: a capillary (6) having a through hole through which a wire (40) is to be inserted; a holding unit, which is provided above the capillary (6), and is configured to hold the wire (40) inserted through the capillary (6); and a vibrating unit configured to vertically vibrate the capillary (6). Under a state in which the holding unit holds the wire (40), the vibrating unit vertically vibrates the capillary (6) so that the wire (40) is protruded from the leading end of the capillary.

Method for ultrasonic welding with particles trapping

The present invention relates to a method of connecting two components by ultrasonic welding for producing a power semiconductor module, said method comprising the steps of: a) Aligning the components to be welded to form a welding interface; b) Aligning a welding tool to the aligned components; c) Removably arranging a trapping material at least partly encompassing the welding interface, whereby the trapping material is a foam; and d) Connecting the components by activating the welding tool. The method like described above provides an easy and cost-saving measure in order to prevent particle contamination when performing a welding process such as particularly an ultrasonic welding process sue to scattered particles.

Method for ultrasonic welding with particles trapping

The present invention relates to a method of connecting two components by ultrasonic welding for producing a power semiconductor module, said method comprising the steps of: a) Aligning the components to be welded to form a welding interface; b) Aligning a welding tool to the aligned components; c) Removably arranging a trapping material at least partly encompassing the welding interface, whereby the trapping material is a foam; and d) Connecting the components by activating the welding tool. The method like described above provides an easy and cost-saving measure in order to prevent particle contamination when performing a welding process such as particularly an ultrasonic welding process sue to scattered particles.

WIRE BONDING APPARATUS AND WIRE BONDING METHOD
20180090464 · 2018-03-29 · ·

In order to easily and accurately measure an offset for wire bonding and improve precision of wire bonding, a wiring bonding apparatus includes a first imaging unit, a bonding tool, a moving mechanism, a reference member, a second imaging unit arranged on the opposite side to the bonding tool and the first imaging unit with respect to a reference surface, and a control unit. The first imaging unit detects a position of an optical axis of the first image capture unit with respect to a position of the reference member, the second imaging unit detects the position of the reference member when moving the bonding tool above the reference member according to pre-stored offset values, and detects a position of a ball-shaped tip section of a wire, and the control unit measures a change in offset between the bonding tool and the first imaging unit based on each detection result.

WIRE BONDING APPARATUS AND WIRE BONDING METHOD
20180090464 · 2018-03-29 · ·

In order to easily and accurately measure an offset for wire bonding and improve precision of wire bonding, a wiring bonding apparatus includes a first imaging unit, a bonding tool, a moving mechanism, a reference member, a second imaging unit arranged on the opposite side to the bonding tool and the first imaging unit with respect to a reference surface, and a control unit. The first imaging unit detects a position of an optical axis of the first image capture unit with respect to a position of the reference member, the second imaging unit detects the position of the reference member when moving the bonding tool above the reference member according to pre-stored offset values, and detects a position of a ball-shaped tip section of a wire, and the control unit measures a change in offset between the bonding tool and the first imaging unit based on each detection result.

METHOD OF JOINING A SURFACE-MOUNT COMPONENT TO A SUBSTRATE WITH SOLDER THAT HAS BEEN TEMPORARILY SECURED
20180082975 · 2018-03-22 ·

A method of joining a surface-mount component to a substrate includes placing a piece of solder on top of the substrate and temporarily bonding the piece of solder to the substrate with at least one temporary bond. The method also includes placing a surface-mount component on top of the substrate with a bottom face of the surface-mount component facing the substrate. The surface-mount component has at least one lateral side. The method further includes positioning the surface-mount component with the at least one lateral side proximate the piece of solder, heating the substrate and the piece of solder to a joining temperature for a time sufficient for the solder to flow into an area between the bottom face of the surface-mount component and the substrate, and cooling the substrate and solder.

METHOD OF JOINING A SURFACE-MOUNT COMPONENT TO A SUBSTRATE WITH SOLDER THAT HAS BEEN TEMPORARILY SECURED
20180082975 · 2018-03-22 ·

A method of joining a surface-mount component to a substrate includes placing a piece of solder on top of the substrate and temporarily bonding the piece of solder to the substrate with at least one temporary bond. The method also includes placing a surface-mount component on top of the substrate with a bottom face of the surface-mount component facing the substrate. The surface-mount component has at least one lateral side. The method further includes positioning the surface-mount component with the at least one lateral side proximate the piece of solder, heating the substrate and the piece of solder to a joining temperature for a time sufficient for the solder to flow into an area between the bottom face of the surface-mount component and the substrate, and cooling the substrate and solder.

Method of Tight Crack Braze Repair Using Acoustics
20180056459 · 2018-03-01 ·

A method for braze repair of tight cracks in a superalloy component is provided. The method includes directing energy, e.g., from an acoustic energy source, towards surfaces of the tight crack to break up one or more contaminants, corrosion products, or oxides at the surface. The directed energy may cause opposed walls of the tight crack to vibrate to break up the oxides, and to generate a modest heat for allowing infiltration of the tight crack with a braze material. The braze material is then melted at a melt temperature of the braze material but below the melt temperature of the component. The braze material is then solidified to repair the tight crack.

Method of Tight Crack Braze Repair Using Acoustics
20180056459 · 2018-03-01 ·

A method for braze repair of tight cracks in a superalloy component is provided. The method includes directing energy, e.g., from an acoustic energy source, towards surfaces of the tight crack to break up one or more contaminants, corrosion products, or oxides at the surface. The directed energy may cause opposed walls of the tight crack to vibrate to break up the oxides, and to generate a modest heat for allowing infiltration of the tight crack with a braze material. The braze material is then melted at a melt temperature of the braze material but below the melt temperature of the component. The braze material is then solidified to repair the tight crack.