B23K20/22
Method of friction welding workpieces by adjusting a sweep length
A method of friction welding a first workpiece to a second workpiece, includes the first workpiece with a first faying surface having a first faying length, the second workpiece with a second faying surface having a second faying length, the second faying length greater than the first faying length; positioning the first workpiece adjacent the second workpiece; reciprocating the first workpiece and the second workpiece against one another, the first faying moves relative to the second faying by a sweep length, a temperature at the first and second faying surfaces increases to create a weld interface; each of the first and second workpieces are consumed into the weld interface, adjusting the sweep length the sweep length remains equal to a difference between the second and the first faying lengths; and stopping the reciprocating and allowing the first and second workpieces to cool to weld the first and second workpieces together.
Joining of dissimilar materials using impact welding
A system and method for joining dissimilar metals. In one embodiment, a method comprises providing a first metal plate, a second metal plate, and an intermediate body that is positioned between the first metal plate and the second metal plate. The first metal plate is then driven into the intermediate body, which causes at least a portion of the intermediate body to collide with the second metal plate. As a result, the material of the intermediate body joins the first metal plate to the second plate. In another embodiment, a method for joining dissimilar metals comprises providing a first metal that is not amenable to welding, a second metal that is joinable to the first metal, and an intermediate body that is not joinable to at least the first metal. The intermediate body may have at least one hole such that the first metal and the second metal are positioned over and on opposite sides of the hole(s). At least a portion of the second metal may then be driven into the hole(s) to be joined to first metal.
Joining of dissimilar materials using impact welding
A system and method for joining dissimilar metals. In one embodiment, a method comprises providing a first metal plate, a second metal plate, and an intermediate body that is positioned between the first metal plate and the second metal plate. The first metal plate is then driven into the intermediate body, which causes at least a portion of the intermediate body to collide with the second metal plate. As a result, the material of the intermediate body joins the first metal plate to the second plate. In another embodiment, a method for joining dissimilar metals comprises providing a first metal that is not amenable to welding, a second metal that is joinable to the first metal, and an intermediate body that is not joinable to at least the first metal. The intermediate body may have at least one hole such that the first metal and the second metal are positioned over and on opposite sides of the hole(s). At least a portion of the second metal may then be driven into the hole(s) to be joined to first metal.
PROCESSES AND TOOLING ASSOCIATED WITH DIFFUSION BONDING THE PERIPHERY OF A CAVITY-BACK AIRFOIL
A fixture assembly includes a first fixture portion, a second fixture portion that interfaces with the first fixture portion, and a sub-fixture movably mounted to the first fixture portion. A multiple of actuators selectively move the sub-fixture toward the second fixture portion. A method of manufacturing a fan blade includes deploying the sub-fixture from the first fixture portion to effectuate a peripheral diffusion bond to join the blade body and the cover of the fan blade.
METHODS OF FORMING AND STAMPING TAILOR FRICTION STIR WELDED BLANKS WITH ENHANCED EDGE STRETCH
A method of forming a stamped part includes forming a tailor welded blank by friction stir welding (FSW) a first blank to a second blank, removing a FSW start spot and a FSW stop spot from the tailor welded blank using a machining process such that a finished tailor welded blank is formed and stamping the finished tailor welded blank into the stamped part such that a weld formed by FSW the first blank to the second blank is plastically deformed. The first blank and the second blank can be aluminum alloy blanks and a predetermined amount of material is machined from the FSW start spot and the FSW stop spot, the predetermined amount of material being equal to or greater than a thickness of the first blank and the second blank.
METHOD OF JOINING HIGH ENTROPY ALLOY, APPARATUS FOR JOINING HIGH ENTROPY ALLOY, AND JOINED STRUCTURE OF HIGH ENTROPY ALLOY
A method of joining a high entropy alloy is provided. The method of joining a high entropy alloy includes the steps of: arranging specimens made of a high entropy alloy to be in contact with each other; and diffusion joining the specimens made of the high entropy alloy by simultaneously applying a compressive stress and a current to a joint of the specimens within a range in which the high entropy alloy does not melt.
METHOD OF JOINING HIGH ENTROPY ALLOY, APPARATUS FOR JOINING HIGH ENTROPY ALLOY, AND JOINED STRUCTURE OF HIGH ENTROPY ALLOY
A method of joining a high entropy alloy is provided. The method of joining a high entropy alloy includes the steps of: arranging specimens made of a high entropy alloy to be in contact with each other; and diffusion joining the specimens made of the high entropy alloy by simultaneously applying a compressive stress and a current to a joint of the specimens within a range in which the high entropy alloy does not melt.
Welding wire preheating systems and methods
Welding wire preheating systems and methods are disclosed. An example welding method includes: receiving a signal indicative of initiation of welding process; prior to initiating a welding arc based on the received signal, controlling voltage or current applied to a welding electrode to preheat the electrode to a temperature above an ambient temperature but below a melting point of the welding electrode; monitoring feedback voltage to determine a termination of preheating; and terminating preheating prior to initiating the welding arc in accordance with a welding protocol.
KINETICALLY LIMITED NANO-SCALE DIFFUSION BOND STRUCTURES AND METHODS
Bulk materials having a kinetically limited nano-scale diffusion bond is provided. The bulk materials having a kinetically limited nano-scale diffusion bond includes transparent material, absorbent opaque material and a diffusion bond. The transparent material has properties that allow an electromagnetic beam of a select wavelength to pass there through without more than minimal energy absorption. The absorbent opaque material has properties that significantly absorb energy from the electromagnetic beam. The diffusion bond is formed by the electromagnetic beam bonding the transparent material to the absorbent opaque material. Moreover, the diffusion bond has a thickness that is less than 1000 nm.
KINETICALLY LIMITED NANO-SCALE DIFFUSION BOND STRUCTURES AND METHODS
Bulk materials having a kinetically limited nano-scale diffusion bond is provided. The bulk materials having a kinetically limited nano-scale diffusion bond includes transparent material, absorbent opaque material and a diffusion bond. The transparent material has properties that allow an electromagnetic beam of a select wavelength to pass there through without more than minimal energy absorption. The absorbent opaque material has properties that significantly absorb energy from the electromagnetic beam. The diffusion bond is formed by the electromagnetic beam bonding the transparent material to the absorbent opaque material. Moreover, the diffusion bond has a thickness that is less than 1000 nm.