B23K35/02

FLUX-CORED WIRE AND METHOD FOR PRODUCING WELDED JOINT
20220395937 · 2022-12-15 · ·

A flux-cored wire of the present disclosure has a steel sheath and a flux filled at an inside of the steel sheath, has a total amount of moisture by ratio with respect to a total wire mass of 300 ppm or less, has flux containing fluorides, and has an amount of the fluorides by ratio with respect to the total wire mass of, by total of values converted to F, 0.11 mass % or more and 2.50 mass % or less. If using the flux-cored wire of the present disclosure for welding, a stable weld shape can be obtained and, further, the amount of diffusible hydrogen of the weld metal can be reduced. For this reason, the flux-cored wire of the present disclosure can be suitably used for welding high strength steel such as ferrite steel.

HIGH RELIABILITY LEAD-FREE SOLDER PASTES WITH MIXED SOLDER ALLOY POWDERS
20220395936 · 2022-12-15 ·

Some implementations of the disclosure describe a solder paste consisting essentially of: 10 wt % to 90 wt % of a first solder alloy powder, the first solder alloy powder consisting of a Sn—Sb alloy, a Sn—Ag—Cu—Sb alloy, a Sn—Ag—Cu—Sb—In alloy, a Sn—Ag—Cu—Sb—Bi alloy, or Sn—Ag—Cu—Sb—Bi—In alloy; 10 wt % to 90 wt % of a second solder alloy powder, the second solder alloy powder consisting of an Sn—Ag—Cu alloy or Sn—Ag—Cu—Bi alloy, and the second solder alloy powder having a lower solidus temperature than the first solder alloy powder; and flux.

Electrode for a welding torch or a cutting torch

The invention relates to an electrode (16) for a welding torch (17) or a cutting torch, comprising a main body (1) and a tip (3) arranged on an end surface (2) of the main body (1). The main body (1) is designed as a hollow body that is open on at least one side. On a side opposite one of the tips (3), the main body has an opening (4) for introducing a cooling medium into an interior space (7) of the main body (1), and at least two regions (5, 6) in the interior space (7), the two inner diameters of which are different from one another, and a transition region (8) located between the two regions (5, 6) having an inner diameter that decreases in the direction of the tip (3).

Electrode for a welding torch or a cutting torch

The invention relates to an electrode (16) for a welding torch (17) or a cutting torch, comprising a main body (1) and a tip (3) arranged on an end surface (2) of the main body (1). The main body (1) is designed as a hollow body that is open on at least one side. On a side opposite one of the tips (3), the main body has an opening (4) for introducing a cooling medium into an interior space (7) of the main body (1), and at least two regions (5, 6) in the interior space (7), the two inner diameters of which are different from one another, and a transition region (8) located between the two regions (5, 6) having an inner diameter that decreases in the direction of the tip (3).

Method for welding a welded part to a component and use of a welded part

A method for welding a welded part to a component is carried out as arc ignition welding by use of direct current, having a bias current phase in which an arc is formed between the negatively polarized welded part and the component, and a subsequent main current phase for melting material to the joint. The welded part: a) is a galvanized sphere made of C10C having a roundness G500, wherein the size of any zinc inclusions under the surface of the sphere equals 10 micrometers at maximum, orb) is formed by welding a galvanized sphere made of C10C having a roundness G500, wherein the size of any zinc inclusions under the surface of the sphere equals 10 micrometers at maximum, to a connection element.

Laminated molding and method of manufacturing laminated molding

An additively manufactured object formed by depositing weld bead layers, each of the weld bead layers being obtained by melting and solidifying a filler metal made of a mild steel, the additively manufactured object includes a plurality of the weld bead layers having a ferrite phase with an average grain diameter of 11 μm or less in a part except for a surface oxide film.

Welding element and welding method for connecting a weld element to a workpiece
11517973 · 2022-12-06 · ·

A welding element is operable for being connected to a workpiece using a welding method. The welding element comprises: a head and a shaft like anchor portion. The head includes a welding surface, a stop surface that is remote from the welding surface, and a plurality of pointed projections evenly and uniformly distributed over the entire welding surface. The shaft-like anchor portion extends along a longitudinal axis between a first end region and a second end region, with the first end region connected to the stop surface.

Hot-rolled steel sheet with excellent low-temperature toughness, steel pipe, and manufacturing method therefor
11519060 · 2022-12-06 · ·

A preferable aspect of the present invention provides a hot-rolled steel sheet with excellent low-temperature toughness, a steel pipe using the same, and a manufacturing method therefor, wherein the hot-rolled steel sheet contains, by weight, 0.35-0.65% C, 0.01-0.4% Si, 13-26% Mn, 0.01-0.3% Ti, 0.01% or less B, 4% or less Al, 1-6% Cr, 0.05% or less P, 0.02% or less S, 0.01% or less N, 0.01-2% Cu, 0.001-0.015% Nb, and the balance Fe and other unavoidable impurities, the alloy elements satisfying the following relational formulas—[Relational formula 1] 70<[10*(C/12)+(Mn/55)+(Al/27)]*100<95 and [Relational formula 2] 4<100*(Cr/52+100*(Nb/93))<9; wherein a microstructure comprises, by area fraction, 97% or more (including 100%) of austenite and 3% or less (including 0%) of a carbide, the crystal grain size of the austenite being 18-30 μm or less; and wherein the size of the carbide is 0.5 μm or less.

Welding device and welding method

A welding system includes a welding torch that welds a workpiece by using a wire, a suction device that sucks shielding gas, and a sucked shielding gas supply path for allowing the sucked shielding gas to flow, wherein the welding torch includes a contact chip that guides the wire, a shielding gas supply nozzle that supplies the shielding gas to a weld zone, and a suction nozzle that surrounds a periphery of the wire protruding from the contact chip, and is opened toward a tip of the wire to suck the shielding gas.

Bonded structure and bonding material

There is provided a bonding material which forms a bonding portion between two objects, which material contains (1) first metal particles comprising a first metal and having a median particle diameter in the range of 20 nm to 1 μm, and (2) second metal particles comprising, as a second metal, at least one alloy of Sn and at least one selected from Bi, In and Zn and having a melting point of not higher than 200° C.