B23K2101/001

Method of fabricating an airfoil preform, an airfoil, and a nozzle sector, by selective melting on a bed of powder
11511342 · 2022-11-29 · ·

A method of fabricating an airfoil preform for a turbine engine by selective melting on a bed of powder, the preform including an airfoil and a removable support secured to the airfoil, the airfoil being fabricated layer by layer from a first edge to a second edge of the airfoil, the method including fabricating the removable support and the airfoil, the removable support being for securing to a fabrication platform and to a portion of a face of the airfoil situated near the first edge and facing the fabrication platform. The face of the airfoil facing the fabrication platform includes a flat extending away from the face, the flat being present over a portion of the face that is situated outside the first edge, the support being secured to the flat or both to the flat and to the portion of the face that is situated outside the first edge.

Method for modular additive manufacturing of a component and a component

A method for the additive manufacturing of a component having the following steps: additively building up multiple sub-sections for the component using a powder bed-based method, arranging the sub-sections to form a composite and additively completing the component, wherein material is deposited, by a deposition welding method, along a peripheral direction around the composite of the sub-sections in such a way that the sub-sections are integrally bonded to each other.

Cupped contour for gas turbine engine blade assembly

A gas turbine engine assembly according to an example of the present disclosure includes, among other things, an endwall having a first material composition, an airfoil extending in a radial direction from the endwall, and a cupped contour of a second material composition that is formed on the endwall to define a cooling chamber, the first material composition different than the second material composition. A method of forming an endwall is also disclosed.

Manufacturing method for hard-to-weld materials

A method of manufacturing a hard-to-weld material by a beam-assisted additive manufacturing process is presented. The method includes depositing a first layer for the material onto the substrate, the first layer including a major fraction of a base material for the component and a minor fraction of a solder, depositing a second layer of the base material for the component and a thermal treatment of the layer arrangement. The thermal treatment includes a first thermal cycle at a first temperature above 1200° C. for a duration of more than 3 hours, a subsequent second thermal cycle at a second temperature above 1000° C. for more than 2 hours, and a subsequent third thermal cycle and a third temperature above 700° C. for more than 12 hours. A manufactured component is also presented.

Method for joining a modular hot gas component using welding and high-temperature soldering, and joined component

A method for joining a modular hot gas component by welding and high-temperature soldering. In order to optimally join high-temperature components, a first component is plugged into pins of a second component, a soldering material is placed between the two components, and the pins of the second component are welded to the first component.

METHOD AND SYSTEM FOR DRILLING CERAMIC

A method of machining includes mounting a component in a drilling machine. The component has a target region where the hole is to be drilled. The component and a jet head are situated relative to each other in a drilling arrangement in which the target region is at a first position that is vertically equal to or vertically above a second position at which the jet head is located. A liquid stream is jetted from the jet head and contains either abrasive particles or a laser beam. The stream impinges the target region, and the abrasive particles or the laser beam cause removal of material from the component to form the hole. The liquid stream rebounds off of the component as back-splash. The drilling arrangement causes gravitational draining of the back-splash from the target region to reduce interference between the back-splash and the liquid stream.

Linear friction-joining device and linear friction-joining method

The present disclosure provides a linear friction joining device which includes: a pressing device for pressing a second member onto a first member in a pressing direction; a vibrator for relatively vibrating the first member and the second member; a controller which is configured to bring the second member into contact with the first member by a position control, which depends on a measurement result of position sensors, to change the position control to a load control, which depends on a measurement result of load sensors, and to increase a pressing load toward a joining load; and a joining load reaching time adjuster which is configured to adjust a length of a joining load reaching time which is between the time when the position control is changed to the load control and the time when the pressing load reaches the joining load.

WELD-BRAZING TECHNIQUES
20230050740 · 2023-02-16 ·

A method includes positioning a braze material along a defect of a component of a turbine system, positioning a cover over the braze material, and focusing a heat source on the cover to melt the braze material along the defect.

Manufacture of cooling holes for ceramic matrix composite components

Systems and methods for machining openings of a component are provided. In one exemplary aspect, a laser system includes features for machining an opening into a component, such as a cooling hole for a CMC component of a gas turbine engine. The component can be oriented in a first position and lasered while oriented in the first position to form a portion of the opening. The component is then oriented to a second position and lasered while oriented in the second position to form another portion of the opening. The component is alternated between the first and second positions until the predetermined geometry of the opening is formed. The component is oriented in the first and second positions such that the laser beam can machine the component without clipping areas that are not desired to be machined.

Method for manufacturing a propeller blade and a propeller blade
11572154 · 2023-02-07 · ·

The present invention involves a method for manufacturing a blade (1) for a propeller, which blade (1) has a leading edge (2) and a trailing edge, the method comprising the steps of: forming a conduit in the blade (1), making a plurality of holes (7) through which the conduit (6) communicates with the exterior of the blade (1), and providing a blade blank having an edge part receiving surface (4) extending along at least a major part of the leading edge (2) of the blade (1) to be manufactured, wherein forming a conduit (6) comprises building up an edge part (3) onto the edge part receiving surface (4) by a wire-based additive manufacturing process, wherein the additive manufacturing process is adapted to form the conduit (6) at least partly delimited by the edge part (3) and extending along the leading edge (2) of the blade (1) to be manufactured.