B29C48/03

USE OF MODIFIED CELLULOSIC THERMOPLASTIC TO PRODUCE CLEAR CAULK CARTRIDGE
20210170438 · 2021-06-10 · ·

A caulk cartridge for use with high organic solvent caulk is disclosed. The cartridge includes a cartridge body formed as an open-ended elongate cylindrical tube having a first end, a second end, and an inner surface, a nozzle affixed to the first end of the cartridge body, and a plunger engaging with the inner surface of the cartridge body and forming a seal at the second end and slidable along a longitudinal axis of the cartridge body from the second end toward the first end. The cartridge body is manufactured from a cellulosic thermoplastic with a high organic solvent barrier.

USE OF MODIFIED CELLULOSIC THERMOPLASTIC TO PRODUCE CLEAR CAULK CARTRIDGE
20210170438 · 2021-06-10 · ·

A caulk cartridge for use with high organic solvent caulk is disclosed. The cartridge includes a cartridge body formed as an open-ended elongate cylindrical tube having a first end, a second end, and an inner surface, a nozzle affixed to the first end of the cartridge body, and a plunger engaging with the inner surface of the cartridge body and forming a seal at the second end and slidable along a longitudinal axis of the cartridge body from the second end toward the first end. The cartridge body is manufactured from a cellulosic thermoplastic with a high organic solvent barrier.

EXTRUDER SCREW HAVING PATHS WITHIN THE SCREW, EXTRUDER, AND EXTRUSION METHOD

An extruder screw includes a screw main body, conveyance portions, barrier portions, and paths. The raw materials, the conveyance of which is limited by the barrier portions, flow in from the entrance. The raw materials flowing in from the entrance flow through the paths in an opposite direction to a conveyance direction of the conveyance portions. The exit is opened in the outer circumferential surface of the screw main body at a position on an upstream side in the conveyance direction in the conveyance portions in which the entrance is opened.

Vented twin-screw kneading extrusion apparatus and extrusion method

According to the present invention, devolatilization of a synthetic resin formed from a polymer or synthetic rubber can be improved and the synthetic resin can be foamed at a low temperature by injecting a devolatilization agent through a devolatilization agent injection nozzle provided in a downstream end segment cylinder of a cylinder assembly. In a vented twin-screw kneading extrusion apparatus and extrusion method according to the present invention, a devolatilization agent, which is injected through a downstream end devolatilization agent injection nozzle provided on a downstream end segment cylinder constituted by a segment cylinder positioned on a downstream end of a cylinder assembly, is dispersed in molten resin in the downstream end segment cylinder and kneaded by a downstream end kneading portion such that the molten resin is foamed by the devolatilization agent and then extruded.

PIPE WITH AN OUTER WRAP

This disclosure relates generally to corrugated pipe, and more particularly to corrugated pipe with an outer wrap. In one embodiment, a pipe includes an axially extended bore defined by a corrugated outer wall having axially adjacent, outwardly-extending corrugation crests, separated by corrugation valleys. The pipe also includes an outer wrap applied to the outer wall. The outer wrap may include fibers and plastic. The outer wrap may span the corrugation crests producing a smooth outer surface.

Method of fabricating a miniature device having an acoustic diaphragm
11019444 · 2021-05-25 · ·

A method of forming a device having a compliant member includes applying heat to a thermoplastic elastomer to maintain the thermoplastic elastomer in a softened state. The thermoplastic elastomer is extruded in the softened state as a film of thermoplastic elastomer. One or more of a bobbin and a housing, each having and end, is positioned such that the end extends at least partially into the film of thermoplastic elastomer. The positioning occurs when the thermoplastic elastomer is in the softened state and/or the bobbin and/or housing is at a temperature that is greater than a temperature of the film of thermoplastic elastomer. The film is cooled so that the bobbin and/or housing are secured to the film and so that the thermoplastic elastomer is in a state that exhibits rubber-like properties.

Method of fabricating a miniature device having an acoustic diaphragm
11019444 · 2021-05-25 · ·

A method of forming a device having a compliant member includes applying heat to a thermoplastic elastomer to maintain the thermoplastic elastomer in a softened state. The thermoplastic elastomer is extruded in the softened state as a film of thermoplastic elastomer. One or more of a bobbin and a housing, each having and end, is positioned such that the end extends at least partially into the film of thermoplastic elastomer. The positioning occurs when the thermoplastic elastomer is in the softened state and/or the bobbin and/or housing is at a temperature that is greater than a temperature of the film of thermoplastic elastomer. The film is cooled so that the bobbin and/or housing are secured to the film and so that the thermoplastic elastomer is in a state that exhibits rubber-like properties.

Extruder screw having paths within the screw, extruder, and extrusion method

An extruder screw includes a screw main body, conveyance portions, barrier portions, and paths. The raw materials, the conveyance of which is limited by the barrier portions, flow in from the entrance. The raw materials flowing in from the entrance flow through the paths in an opposite direction to a conveyance direction of the conveyance portions. The exit is opened in the outer circumferential surface of the screw main body at a position on an upstream side in the conveyance direction in the conveyance portions in which the entrance is opened.

Extruder screw having paths within the screw, extruder, and extrusion method

An extruder screw includes a screw main body, conveyance portions, barrier portions, and paths. The raw materials, the conveyance of which is limited by the barrier portions, flow in from the entrance. The raw materials flowing in from the entrance flow through the paths in an opposite direction to a conveyance direction of the conveyance portions. The exit is opened in the outer circumferential surface of the screw main body at a position on an upstream side in the conveyance direction in the conveyance portions in which the entrance is opened.

METHOD OF PRODUCING A COATED VEHICLE WINDSHIELD FOR A HEAD-UP DISPLAY (HUD)
20210107256 · 2021-04-15 ·

A method for determining pane thicknesses and a wedge angle of a coated windshield for a projection arrangement of a head-up display. A wedge angle and a combination of glass thicknesses are determined by means of which the glass ghost image and the layer ghost image are optimally reduced. The method proceeds from a starting thickness of the two glass panes of the windshield for which that wedge angle is determined, in an iterative process, that represents an optimal compromise between the minimization of the glass ghost image and the minimization of the layer ghost image. Then, the glass thicknesses are determined varied within a specified range for each combination of the optimal wedge angles. Thus, it is possible, iteratively, to identify that combination of glass thicknesses that results in the least occurrence of ghost images, in addition to the associated optimal wedge angle.