B29K2081/04

Method and insert for welding thermoplastic components

A method for welding thermoplastic components, in particular, thermoplastic fiber composite structural components for an aircraft or spacecraft, having the following steps. Arranging an insert, which has a conductor structure having a plurality of parallel electrical conductor elements, in a joining zone between a first thermoplastic component and a second thermoplastic component such that at least some portions of the parallel electrical conductor elements are located in the joining zone; locally melting the components in the region of the joining zone by supplying current to the conductor structure; disconnecting the connector elements; and removing the insert from the joining zone by pulling out the disconnected conductor elements. An insert for the resistance welding of thermoplastic components is also provided.

Method for manufacturing foam molded body and foam molded body
11648713 · 2023-05-16 · ·

A method for producing a foam-molded product by using a plasticizing cylinder, includes: plasticizing and melting the thermoplastic resin to provide the molten resin in a plasticization zone of the plasticizing cylinder; introducing a pressurized fluid containing the physical foaming agent at a fixed pressure into a starvation zone of the plasticizing cylinder to retain the starvation zone at the fixed pressure; allowing the molten resin to be in the starved state in the starvation zone; bringing the molten resin in contact with the pressurized fluid containing the physical foaming agent at the fixed pressure, in the starvation zone in a state in which the starvation zone is retained at the fixed pressure; and molding the molten resin having been brought in contact with the pressurized fluid containing the physical foaming agent into the foam-molded product.

Low-dielectric resin composition, low-dielectric resin/metal composite material and preparation method thereof, and electronic equipment

A resin composition comprises, based on 100% by weight of the resin composition: 45-70 wt % of a main resin, 20-45 wt % of a chopped glass fiber, 1-3 wt % of a toughening resin, 0.2-0.5 wt % of an unmodified glycidyl methacrylate, and 0-10 wt % of an auxiliaries. The main resin is selected from at least one of PBT resin and PPS resin. The chopped glass fiber has a dielectric constant of 4.0 to 4.4 at 1 MHz.

INJECTION MOLDED PARTS
20230143023 · 2023-05-11 ·

The invention relates to an injection molded part comprising a composition comprising: a. Polyarylene sulfide (PAS) in an amount of between 50 wt % and 90 wt %; b. Glass fibers in an amount of between 10 wt % and 50 wt %; wherein the composition has a sodium content of at most 3500 ppm as measured by Inductively coupled plasma atomic emission spectroscopy (ICP-AES) and wherein the composition has a iodine content of at most 100 ppm as measured by X-ray fluorescence (XRF) and wherein the weight percentage and ppm is with respect to the total weight of the composition. The invention further relates to a fuel cell comprising the injection molded part.

Method of joining two objects

A method for joining two objects by anchoring an insert portion provided on one of the objects in an opening provided on the other one of the objects. The anchorage is achieved by liquefaction of a thermoplastic material and interpenetration of the liquefied material and a penetrable material, the two materials being arranged on opposite surfaces of the insert portion and the wall of the opening. Before such liquefaction and interpenetration, an interference fit is established in which such opposite surfaces are pressed against each other, and, for the anchoring, mechanical vibration energy and possibly a shearing force are applied, wherein the shearing force puts a shear stress on the interference fit.

Method of joining two objects

A method for joining two objects by anchoring an insert portion provided on one of the objects in an opening provided on the other one of the objects. The anchorage is achieved by liquefaction of a thermoplastic material and interpenetration of the liquefied material and a penetrable material, the two materials being arranged on opposite surfaces of the insert portion and the wall of the opening. Before such liquefaction and interpenetration, an interference fit is established in which such opposite surfaces are pressed against each other, and, for the anchoring, mechanical vibration energy and possibly a shearing force are applied, wherein the shearing force puts a shear stress on the interference fit.

POLY(ARYLENE SULFIDE) AND PRODUCTION METHOD THEREFOR

A polyarylene sulfide in which when the cumulative integral value from the molecular weight of 100 to the molecular weight of 10,000 in a molecular weight distribution curve is 100, the cumulative integrated value at the molecular weight of 4000 is 48 to 53, and when the melt flow rate of the polyarylene sulfide is defined as MFR1, and when the melt flow rate obtained after mixing the polyarylene sulfide with an epoxy silane coupling agent at a weight ratio of 100:1 and heating the resulting mixture at 315.5° C. for 5 minutes is defined as MFR2, the rate of change represented by MFR2/MFR1 is not more than 0.085.

METHOD FOR MANUFACTURING FOAM MOLDED BODY AND FOAM MOLDED BODY
20230202080 · 2023-06-29 · ·

A method for producing a foam-molded product by using a plasticizing cylinder, includes: plasticizing and melting the thermoplastic resin to provide the molten resin in a plasticization zone of the plasticizing cylinder; introducing a pressurized fluid containing the physical foaming agent at a fixed pressure into a starvation zone of the plasticizing cylinder to retain the starvation zone at the fixed pressure; allowing the molten resin to be in the starved state in the starvation zone; bringing the molten resin in contact with the pressurized fluid containing the physical foaming agent at the fixed pressure, in the starvation zone in a state in which the starvation zone is retained at the fixed pressure; and molding the molten resin having been brought in contact with the pressurized fluid containing the physical foaming agent into the foam-molded product.

Cure-on-demand liquid sealant composition, process for the preparation thereof and uses thereof

The present invention is directed to a liquid sealant composition based on polysulphide, capable of curing on demand, and the process for preparing same, the liquid sealant composition including: (i) a polysulphide comprising an —SH end group, (ii) a crosslinking agent chosen from ethylenically unsaturated or acetylenically unsaturated compounds, the unsaturated ethylenic or unsaturated acetylenic functions of the crosslinking agent being chemically blocked with a blocking agent, and (iii) optionally, a catalyst. The present invention also relates to a process for coating a substrate with a composition according to the invention, and also to the cured sealant materials formed from this composition. Finally, the invention relates to the use of a liquid sealant composition according to the invention for the construction and/or the maintenance, and more particularly for the adhesive bonding and/or the protection, of vehicles and machines.

Method for welding parts made of thermoplastic material

A method for welding at least two parts including a thermoplastic material and having respective surfaces to be welded, including: inserting an insert between the surfaces to be welded of the two parts; generating heat via the insert; wherein the insert moves in relation to the parts to be welded in a welding direction. Also, an installation adapted for implementation of this method.