B32B21/02
Transparent resin film, decorative board, and method for producing decorative board
The present invention provides a transparent resin film that is capable of imparting excellent design properties to a decorative board and is excellent in adhesion to a picture layer, a decorative board including the transparent resin film, and a method for producing the decorative board. Provided is a transparent resin film for protecting a picture layer provided on one side of a substrate, the transparent resin film having a pattern of protrusions and depressions on a picture layer side, the pattern of protrusions and depressions having a maximum height roughness Rz defined in JIS B 0601 (2001) within a range of 15 μm or larger and 70 μm or smaller.
Method to produce a veneer element and a veneer element
A method to produce a veneer element, including defects and dense portions. The method includes providing a substrate, providing a sub-layer, including a binder and coloured filler particles, applying the sub-layer on a first surface of the substrate, applying a veneer layer on the sub-layer, and applying pressure, preferably heat and pressure, to the veneer layer and/or the substrate, thereby forming a veneer element wherein, after pressing, the sub-layer is visible through a defect of the veneer element such as crack, cavity, hole and/or knot of the veneer layer. Also, a veneer element.
Method to produce a veneer element and a veneer element
A method to produce a veneer element, including defects and dense portions. The method includes providing a substrate, providing a sub-layer, including a binder and coloured filler particles, applying the sub-layer on a first surface of the substrate, applying a veneer layer on the sub-layer, and applying pressure, preferably heat and pressure, to the veneer layer and/or the substrate, thereby forming a veneer element wherein, after pressing, the sub-layer is visible through a defect of the veneer element such as crack, cavity, hole and/or knot of the veneer layer. Also, a veneer element.
METHOD FOR THE PRODUCTION OF A POLYVINYL CHLORIDE-FREE TOP LAYER, POLYVINYL CHLORIDE-FREE TOP LAYER AND DECKING ELEMENT
The present invention relates to a method for producing a polyvinyl chloride-free top layer (1) for a decking element (3), the method comprising the method steps indicated below: A) Providing a base layer (4) comprising and/or consisting of plastic; B) Printing a décor (6) on a top (5) of the base layer (4) facing a usable side (7); C) Bonding, preferably laminating, a, preferably transparent, wearing surface (8) to the printed base layer (4) to form a, preferably solid, layer composite (9); D) Embossing the layer composite (9) at least in some areas, preferably over the entire surface, with a structure (10) at least substantially synchronous with the décor (6), the structure (10) being embossed in such a way that it is visible both on the top (11) facing the usable side (7) and at least in some areas on the bottom (12) of the layer composite (9) facing away from the usable side (7); E) Application of a surface sealing layer (17), preferably a lacquer layer, to the top (11) of the layer composite (9) facing the usable side (7); F) optionally: curing of the surface sealing layer (17), preferably the lacquer layer.
METHOD FOR THE PRODUCTION OF A POLYVINYL CHLORIDE-FREE TOP LAYER, POLYVINYL CHLORIDE-FREE TOP LAYER AND DECKING ELEMENT
The present invention relates to a method for producing a polyvinyl chloride-free top layer (1) for a decking element (3), the method comprising the method steps indicated below: A) Providing a base layer (4) comprising and/or consisting of plastic; B) Printing a décor (6) on a top (5) of the base layer (4) facing a usable side (7); C) Bonding, preferably laminating, a, preferably transparent, wearing surface (8) to the printed base layer (4) to form a, preferably solid, layer composite (9); D) Embossing the layer composite (9) at least in some areas, preferably over the entire surface, with a structure (10) at least substantially synchronous with the décor (6), the structure (10) being embossed in such a way that it is visible both on the top (11) facing the usable side (7) and at least in some areas on the bottom (12) of the layer composite (9) facing away from the usable side (7); E) Application of a surface sealing layer (17), preferably a lacquer layer, to the top (11) of the layer composite (9) facing the usable side (7); F) optionally: curing of the surface sealing layer (17), preferably the lacquer layer.
Method for the production of panels from a board, press plate, method for the production of a board and board
Disclosed is a method for producing panels from a board which includes dissecting the board along predefined lines. The board includes a core material board and is laminated with a laminate material layer. The board is dissected along an impressed region running linear over the complete surface of the laminate material layer. Also disclosed are a press plate, a method for the production of a board having an impressed region, and a board for producing the panels.
Method for the production of panels from a board, press plate, method for the production of a board and board
Disclosed is a method for producing panels from a board which includes dissecting the board along predefined lines. The board includes a core material board and is laminated with a laminate material layer. The board is dissected along an impressed region running linear over the complete surface of the laminate material layer. Also disclosed are a press plate, a method for the production of a board having an impressed region, and a board for producing the panels.
Vibration absorption device and method for acoustic insulation
A vibration absorption device for acoustic insulation for a building structure comprises an absorbent cushion and a vibration isolation cushion. The building structure is selected from a ceiling structure, a floor structure and a partitioning structure separating two adjacent building compartments or a building compartment and the external environment. The absorbent cushion comprises sound absorbing material and the vibration isolation cushion comprising vibration isolation material. The vibration isolation cushion overlies and is laminated to the absorbent cushion. The vibration isolation cushion is rigid relative to the absorbent cushion. The absorbent cushion is supple relative to the vibration isolation cushion. The vibration absorption device is mountable to the building structure, to isolate vibrations and to provide acoustic insulation between the two separated and adjacent building compartments.
Method to produce a coating layer, a building panel and a coated foil
The present disclosure relates to a method to produce a coating layer, including applying a coating composition on a surface of a carrier, curing the coating composition to a coating layer, and subsequently applying pressure to the coating layer. The disclosure further relates to a method to produce a building panel, and such a building panel, and to a method to produce a coated foil, and such a coated foil.
FLOOR PANEL
A floor panel has a rectangular and oblong shape, and includes a substrate and a top layer provided on the substrate and forming a decorative side of the floor panel. The top layer is composed of a print provided on a carrier sheet and a transparent thermoplastic layer situated above the print. The substrate has a thickness from 2 to 10 millimeter and forms at least half of the thickness of the floor panel. The substrate is a polyurethane-based substrate and the transparent thermoplastic layer is polyurethane-based. The floor panel has a length of more than 1.1 meters and has a plurality of reinforcing layers situated outside the center line of the substrate. A reinforcing layer may be provided in combination with the substrate and the top layer.