Patent classifications
B32B2307/50
OVERLAY APPLICATOR TRAY AND METHOD OF USING THE SAME
An overlay applicator tray including a cradle including a device slot. The device slot is configured to securely hold an electronic device in the cradle. The overlay applicator tray also can include an overlay applicator. The overlay applicator can include an overlay layer and an adhesive release liner. The overlay layer can include a top side and a bottom side. The bottom side is configured to be adhered to a screen of the electronic device. The adhesive release liner is removably attached to the bottom side of the overlay layer. The overlay applicator tray additionally can include an alignment piece coupling the cradle to the overlay applicator. The alignment piece aligns the overlay layer of the overlay applicator with the screen as the overlay layer is applied to the screen when the electronic device is securely held in the device slot. The overlay applicator tray further can include a first pull tab on the adhesive release liner. The first pull tab is configured to be pulled to remove the adhesive release liner from the bottom side of the overlay layer and expose an adhesive of the overlay layer. Other embodiments are described.
Flexible display apparatus
A flexible display apparatus includes a first functional layer, a second functional layer above the first functional layer, a third functional layer above the second functional layer, a first adhesive layer between the first functional layer and the second functional layer, and having a first recovery rate, and a second adhesive layer between the second functional layer and the third functional layer, and having a second recovery rate that is lower than the first recovery rate.
Laminated metal sheet for metal container lid and method for manufacturing the same
A laminated metal sheet for a metal container lid includes a polyester resin layer formed on a metal sheet. The polyester resin layer is composed of an A and a B layer, wherein the melting point of the A layer is lower than the melting point of the B layer by 20° C. or more, the A layer includes a molten layer where the value of the ratio of a peak intensity I.sub.0° to a peak intensity I.sub.90° is 1.5 or less, the B layer includes an orientation layer where the value of the ratio of the peak intensity I.sub.0° to the peak intensity I.sub.90° is 3.0 or more, the thickness of the A layer is within the range from 5 μm or more to less than 30 μm, and the thickness of the B layer is within the range from 0.5 μm or more to less than 6.0 μm.
Thermoplastic prepreg based foam product
A system for manufacturing a thermoplastic prepreg product includes a belt or conveyor, a prepreg applicator that positions a thermoplastic prepreg atop the belt or conveyor, a foam applicator that applies a foam mixture atop the thermoplastic prepreg, a heating mechanism that heats the thermoplastic prepreg and the foam mixture to cause the foam mixture to react atop the thermoplastic prepreg, and a laminator that is configured to press the thermoplastic prepreg and foam mixture to control a thickness of the resulting thermoplastic prepreg product. The thermoplastic prepreg includes a fabric, mat, or web of fibers and a thermoplastic material that is impregnated within the fabric, mat, or web of fibers. The thermoplastic material is formed from in situ polymerization of monomers and oligomers. The foam mixture includes an isocyanate, a polyol blend, and a blowing agent.
SYSTEMS AND METHODS FOR GRADIENT SEAL FLEXIBLE FILMS
A film includes an outer layer and a sealant layer attached to the outer layer. The sealant layer includes a first layer having a first viscosity and a second layer having a second viscosity. The first layer is attached to the outer layer and the second layer is attached to the first layer. The first viscosity is greater than the second viscosity.
Stretchable films, methods of manufacturing the same and display devices including the same
A display device including a flexible base substrate; a pixel circuit and a light emitting structure sequentially disposed on the flexible base substrate; and a stretchable film attached on a bottom of the flexible base substrate. The stretchable film includes a first region and a second region, which are divided according to curvatures of an object, and at least one of different patterns and different disposed structures are arranged in each of the first region and the second region.
Gas barrier laminate
This gas barrier laminate comprises a base layer; a gas barrier layer laminated on one surface (A) of the base layer, directly or with another layer sandwiched therebetween; a protective film (α) laminated directly on the gas barrier layer; and a protective film (β) laminated on a surface (B) opposite to the surface (A) of the base layer, directly or with another layer sandwiched therebetween, wherein the gas barrier layer contains a specific inorganic compound, and an adhesion at the time of peeling the protective film (α) and an adhesion at the time of peeling the protective film (β) under specific conditions are both less than or equal to specific values. By means of this invention, there is provided a gas barrier laminate having a base layer, a gas barrier layer, and protective films, in which each of the protective films can be peeled off without adversely affecting the external appearance of an exposed surface, and even after the protective film is peeled off, the original water vapor-blocking properties are maintained in the remaining laminate.
Multilayer cling film and box
A plastic film for cling film application packed in a box, and a box including such a film, are described. The cling film includes a polyolefin such as low-density polyethylene (LDPE), linear low-density polyethylene (LLDPE), metallocene LLDPE, polyolefin plastomer, ethylene vinyl acetate (EVA), ethylene methyl acrylate (EMA), ethylene butyl acrylate (EBA), polypropylene (PP), cyclic olefin copolymer, or combinations thereof; and a polymer with a Young's modulus higher than 500 MPa selected from ethylene vinyl alcohol (EVOH), polyamide, polyester, cyclic olefin copolymer, polypropylene and polylactide (PLA), or combinations thereof. The film includes an inner layer and an outer layer, wherein the outer layer is free of polypropylene. The film is packed in a box which does not include any cutting unit. The film is configured to be manually cut by a user without using any cutting unit.
Composite film
The present disclosure relates to a multilayer composite that may include a first porous layer, and a first barrier layer overlying the first porous layer. The first barrier layer may include a polyaramid material, a polyimide material, or any combination thereof. The multilayer composite may have a flame resistance rating of at least about 180° C. and a 50% strain compression rating of not greater than about 600 kPa.
METHOD OF MANUFACTURING A LIGHTWEIGHT, STRUCTURALLY REINFORCED OBJECT OF THERMOPLASTIC MATERIAL
Lightweight, structurally reinforced thermoplastic objects comprising at least one reinforcement zone are manufactured by providing a heatable rigid forming chamber with a chamber volume. At a temperature below the thermoplastic softening temperature, the chamber is loaded with a plurality of thermoplastic lofting bodies and a plurality of thermoplastic reinforcement bodies wherein the lofting bodies are heat-loftable bodies comprising a thermoplastic matrix containing an elastically compressed assembly of reinforcement fibers embedded therein, lofty non-woven bodies comprising an elastically compressible assembly of reinforcement fibers and thermoplastic fibers. Upon closing the chamber, lofting bodies of lofty non-wovens are elastically compressed, producing an internal pressure. After heating the chamber above softening temperature, reinforcement bodies and lofting bodies are ow thermoplastically formable, and lofting bodies configured as heat-loftable bodies produce a second internal pressure. After a predetermined processing time, the chamber is cooled yielding a structurally reinforced object.