B01J3/062

Polycrystalline compacts, earth-boring tools including such compacts, and methods of fabricating polycrystalline compacts

A polycrystalline compact includes diamond, cubic boron nitride, and at least one hard material, which may be aluminum nitride, gallium nitride, silicon nitride, titanium nitride, silicon carbide, titanium carbide, titanium boride, titanium diboride, and/or aluminum boride. The diamond, the cubic boron nitride, and the hard material are intermixed and interbonded to form a polycrystalline material. An earth-boring tool includes a bit body and a polycrystalline diamond compact secured to the bit body. Methods of fabricating polycrystalline compacts include forming a mixture comprising diamond, non-cubic boron nitride, and a metal or semimetal; encapsulating the mixture in a container; and subjecting the encapsulated mixture to high-pressure and high-temperature conditions to form a polycrystalline material.

Method for producing carbon particles by detonation

A production method of a carbon particle by a detonation method includes a step of disposing an explosive substance in a periphery of a raw material substance, and a step of subjecting the explosive substance to a detonation. The explosive substance is a liquid at normal temperature and normal pressure. The raw material substance contains an aromatic compound having 3 or more nitro groups.

Methods of fabricating a polycrystalline diamond compact

Embodiments relate to polycrystalline diamond compacts (PDCs) and methods of manufacturing such PDCs in which an at least partially leached polycrystalline diamond (PCD) table is infiltrated with a low viscosity cobalt-based alloy infiltrant. In an embodiment, a method includes forming a PCD table in the presence of a metal-solvent catalyst in a first high-pressure/high-temperature (HPHT) process. The method includes at least partially leaching the PCD table to remove at least a portion of the metal-solvent catalyst therefrom to form an at least partially leached PCD table. The method includes subjecting the at least partially leached PCD table and a substrate to a second HPHT process effective to at least partially infiltrate the at least partially leached PCD table with a cobalt-based alloy infiltrant having a composition at or near a eutectic composition of the cobalt-based alloy infiltrant.

Aqueous leaching solutions and methods of leaching at least one interstitial constituent from a polycrystalline diamond body using the same

In an embodiment, a method of fabricating a leached polycrystalline diamond (PCD) body is disclosed. The PCD body includes bonded diamond grains defining interstitial regions at least a portion of which include at least one interstitial constituent disposed therein. The method includes leaching the PCD body with a leaching agent to remove at least a portion of the at least one interstitial constituent therefrom. The leaching agent includes a mixture having hydrofluoric acid in a first concentration of about 10 weight % to about 50 weight %, nitric acid in a second concentration of about 5 weight % to about 25 weight %, and water in a third concentration of about 25 weight % to about 85 weight %. Further embodiments relate to different leaching methods and different leaching agent compositions.

Support structure for a body of polycrystalline diamond material during leaching

A support structure (40) for a PCD element (10) comprises a support (42) into which a PCD element (10) is locatable and a sealing element (48) for location in the support structure (40) and configured to protect a non-leached portion of a PCD element (10) during a leaching process. The support (42) is formed from or coated with a polyketone based plastics material.

Methods of fabricating polycrystalline diamond by functionalizing diamond nanoparticles, green bodies including functionalized diamond nanoparticles, and methods of forming polycrystalline diamond cutting elements

Method of fabricating polycrystalline diamond include functionalizing surfaces of diamond nanoparticles with fluorine, combining the functionalized diamond nanoparticles with a polymer to form a mixture, and subjecting the mixture to high pressure and high temperature (HPHT) conditions to form inter-granular bonds between the diamond nanoparticles. A green body includes a plurality of diamond nanoparticles functionalized with fluorine, and a polymer material interspersed with the plurality of diamond nanoparticles. A method of forming cutting element includes functionalizing surfaces of diamond nanoparticles with fluorine, and combining the functionalized diamond nanoparticles with a polymer to form a mixture. The mixture is formed over a body, and the mixture and the body are subjected to HPHT conditions to form inter-granular bonds between the diamond nanoparticles and secure the bonded diamond nanoparticles to the body.

Multi-heater method for growing high quality diamond

Disclosed herein is an apparatus and method for growing a diamond. The apparatus for growing a diamond comprises: a reaction cell that is configured to grow the diamond therein; a main heater including a main heating surface that is arranged along a first inner surface of the reaction cell; and a sub-heater including a sub-heating surface that is arranged along a second inner surface of the reaction cell, the second inner surface being non-parallel with the first inner surface.

Dense packing particle size distribution for PDC cutters
10166654 · 2019-01-01 · ·

A superabrasive compact and a method of making the superabrasive compact are disclosed. A method of making a superabrasive compact comprises steps of providing a plurality of superabrasive particles having a particle size distribution with a first ratio (d50)/(d50 principle particles) ranging from about 0.86 to about 0.92; providing a support to the plurality of superabrasive particles; and subjecting the support and the plurality of superabrasive particles to conditions of an elevated temperature and pressure suitable for producing the polycrystalline superabrasive compact.

Post processing method for cannabis oil
12059671 · 2024-08-13 · ·

A cannabis oil formulation comprises a level of terpene concentration of at least 4.88% by weight, detectable levels of tetrahydrocannabinol (THC) and at least two other cannabinoids, and a level of tetrahydrocannabinolic acid (THCA) concentration that is not detectable.

Polycrystalline diamond compacts including a polycrystalline diamond table having a modified region exhibiting porosity

Polycrystalline diamond compacts (PDCs) and methods of manufacturing such PDCs. In an embodiment, the PDC includes a polycrystalline diamond (PCD) table having at least a portion of a metal-solvent catalyst removed therefrom. Removing at least a portion of a metal-solvent catalyst from the PCD table may increase the porosity of the PCD table relative to a PCD table that has not been treated to remove the metal-solvent catalyst. Likewise, removing at least a portion of a metal-solvent catalyst from the PCD table may decrease the specific magnetic saturation and increase the coercivity of the PCD table relative to a PCD table that has not been treated to remove the metal-solvent catalyst.