B05D2203/35

Analytic substrate coating apparatus and method
11307121 · 2022-04-19 ·

An apparatus and method for producing a coated analytic substrate using a compact and portable automated instrument located in the laboratory setting at the point of use which can consistently produce one or a plurality of coated analytic substrates “on demand” for using the analytic substrate immediately after coating, preferably without a step of rinsing the coated analytic substrate before use. The apparatus preferably uses applicator cartridges having a reservoir containing the coating compositions used to form the coatings. Preferably the cartridges are removable and interchangeable to facilitate the production of individual analytic substrates having different coatings or different coating patterns. These coated analytic substrates have superior specimen adhesion characteristics due to the improved quality of the coatings applied by the coating apparatus and due to the quickness with which the coated analytic substrates can be used in the lab after production.

Liquid composition, metallic luster film, and article

A liquid composition includes a thiophene polymer; and at least one polymerization component selected from the group including a monomer and an oligomer.

APPARATUS AND METHOD FOR REMOVING BUBBLES IN FLEXIBLE SUBSTRATE
20210362184 · 2021-11-25 ·

The present disclosure provides an apparatus for removing bubbles in a flexible substrate. The flexible substrate includes a baseplate and a polyimide layer coated on the baseplate. The apparatus includes a chamber including a top wall, a sidewall, and a bottom wall, wherein the top wall, the sidewall, and the bottom wall define an accommodation space; a heating plate disposed in the accommodation space; and a cooling conduit embedded in at least one of the top wall and the sidewall of the chamber.

Optical coating method, apparatus and product

This disclosure is directed to an improved process for making glass articles having optical coating and easy-to clean coating thereon, an apparatus for the process and a product made using the process. In particular, the disclosure is directed to a process in which the application of the optical coating and the easy-to-clean coating can be sequentially applied using a single apparatus. Using the combination of the coating apparatus and the substrate carrier described herein results in a glass article having both optical and easy-to-clean coating that have improved scratch resistance durability and optical performance, and in addition the resulting articles are “shadow free.”

EASY TO CLEAN COATING

The present invention relates to a process for preparing a thin film on a substrate in which a first precursor composition (FPC) and a second precursor composition (SPC) are combined, a thin layer of the combined first precursor composition (FPC) and second precursor composition (SPC) is formed on a substrate and the thin layer is cured, an article comprising said thin layer, a composition comprising said first precursor composition (FPC) and said second precursor composition (SPC), a kit-of-parts comprising said first precursor composition (FPC) and said second precursor composition (SPC) in two vessels and the use of said composition or kit-of-parts for preparing a thin film on a substrate and for preparing an optical or electrical coating.

FLUOROPOLYETHER GROUP-INCLUDING COMPOUND

A fluoropolyether group-containing compound of formula (1) or (2):

##STR00001##

wherein R.sup.F1, R.sup.X1, R.sup.X2 and R.sup.Si are as defined herein.

Antiglare film-coated substrate, method for its production, and article

To provide a production method capable of producing an antiglare film-coated substrate having excellent antiglare performance in a short time, an antiglare film-coated substrate having excellent antiglare performance, and an article provided with the substrate. A method for producing an antiglare film-coated substrate 1 comprising a substrate 3 and an antiglare film 5 formed on the substrate 3, characterized by comprising a step of preparing a coating composition comprising at least one of a silica precursor (A) and particles (C), and a liquid medium (B), wherein the liquid medium (B) contains a liquid medium (B1) having a boiling point of at most 150° C. in an amount of at least 86 mass % based on the total amount of the liquid medium (B), a step of electrically charging and spraying the coating composition by using an electrostatic coating apparatus having an electrostatic coating gun having a rotary atomizing head, to apply it on the substrate 3 to form a coating film, and a step of firing the coating film to form an antiglare film 5.

Silane compound containing perfluoro(poly)ether group

A perfluoro(poly)ether group containing silane compound of formula (1a) or (1b):
(Rf-PFPE).sub.β-X—(CR.sup.a.sub.kR.sup.b.sub.lR.sup.c.sub.m).sub.α  (1a)
(R.sup.c.sub.mR.sup.b.sub.lR.sup.a.sub.kC).sub.α—X-PFPE-X—(CR.sup.a.sub.kR.sup.b.sub.lR.sup.c.sub.m).sub.α  (1b)
wherein the symbols are as defined herein.

Superhydrophobic and dust mitigating coatings

A method is provided to form a dust mitigation coating that also mitigates or repels water, ice, and other liquids. Techniques to coat the surfaces of equipment and items with these dust, liquid, and ice mitigation coatings, minimize or eliminate mission problems caused by dust, liquid, or ice accumulation, particularly in outer space or on another planetary body or moon. Further, the dust mitigation coatings exhibit a Lotus-like effect, making the coated surfaces ultra-hydrophobic. The present invention is also directed to techniques for improving the functioning of terrestrial-based equipment and systems where dust, liquid, or ice accumulation is a problem, such as in hospitals and other health contexts, to prevent contamination.

IMPROVED METHOD FOR PLASMA IMMOBILIZATION OF A BIOMOLECULE TO A SUBSTRATE VIA A LINKING MOLECULE
20220001419 · 2022-01-06 ·

A two-step method is provided for the immobilization of a biomolecule through a linking molecule on a sample surface of a substrate by generating and maintaining a non-thermal atmospheric pressure plasma at a temperature between room temperature and 60° C. The preferred plasma temperature is room temperature. The method comprises of a first step and second step, which are sequentially carried out. In the first step of the method, the linking molecule is deposited onto the sample surface through exposing the sample surface to a first plasma jet and the linking molecule, generating a linking layer onto the sample surface. In a second sequential step of the method, the biomolecule is deposited onto the linking layer through exposing the linking layer to a second plasma jet and the biomolecule.